Final Magnetic Moment0.056 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.227 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.111 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiNi2P3O10 + LiNiPO4 |
Band Gap3.448 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21 [4] |
HallP 2yb |
Point Group2 |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 231.9 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 250.1 |
AlN (mp-661) | <1 0 1> | <0 1 1> | 286.2 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 324.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 285.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 278.3 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 231.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 185.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 231.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 231.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 324.7 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 250.1 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 204.9 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 231.9 |
DyScO3 (mp-31120) | <0 1 1> | <0 0 1> | 324.7 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 324.7 |
DyScO3 (mp-31120) | <1 1 1> | <0 0 1> | 139.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 324.7 |
CdS (mp-672) | <1 1 0> | <1 0 -1> | 102.4 |
CdS (mp-672) | <1 1 1> | <1 0 -1> | 102.4 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 185.5 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 285.6 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 285.6 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 109.3 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 231.9 |
YVO4 (mp-19133) | <0 0 1> | <1 0 -1> | 102.4 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 109.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 231.9 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 218.5 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 250.1 |
BN (mp-984) | <0 0 1> | <0 1 1> | 190.8 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 139.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 324.7 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 139.1 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 46.4 |
CdTe (mp-406) | <1 0 0> | <1 0 1> | 218.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 -1> | 204.9 |
TiO2 (mp-2657) | <1 0 1> | <0 1 0> | 250.1 |
C (mp-66) | <1 1 0> | <1 0 1> | 109.3 |
GdScO3 (mp-5690) | <1 1 1> | <0 0 1> | 139.1 |
KP(HO2)2 (mp-23959) | <0 1 0> | <0 0 1> | 231.9 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 0 1> | 109.3 |
LaF3 (mp-905) | <1 0 1> | <0 0 1> | 139.1 |
LaF3 (mp-905) | <1 1 0> | <0 0 1> | 92.8 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 185.5 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 185.5 |
InSb (mp-20012) | <1 0 0> | <1 0 1> | 218.5 |
BaTiO3 (mp-5986) | <1 0 0> | <0 0 1> | 278.3 |
NdGaO3 (mp-3196) | <1 0 1> | <0 0 1> | 324.7 |
Ga2O3 (mp-886) | <0 1 0> | <0 1 1> | 286.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Cu4(PO4)3 (mp-673151) | 0.6295 | 0.039 | 3 |
MgSiO3 (mp-642228) | 0.6755 | 0.224 | 3 |
MgSiO3 (mp-642210) | 0.6180 | 0.165 | 3 |
LiPO3 (mp-29195) | 0.5853 | 0.000 | 3 |
Na2Ge2O5 (mp-772769) | 0.6705 | 0.032 | 3 |
LiMn2(PO4)2 (mp-767083) | 0.5422 | 0.065 | 4 |
Li2Fe(Si2O5)2 (mp-772589) | 0.5648 | 0.053 | 4 |
LiCu(PO3)2 (mp-759874) | 0.5339 | 0.087 | 4 |
Li2Mn3(P2O7)2 (mp-762715) | 0.4453 | 0.063 | 4 |
LiNiP2O7 (mp-761590) | 0.5470 | 0.089 | 4 |
CrN2 (mp-1016069) | 0.7138 | 0.474 | 2 |
CrN2 (mp-1096899) | 0.6038 | 0.474 | 2 |
BaZn2As3HO11 (mp-758313) | 0.6830 | 0.007 | 5 |
Mg5Al4Fe(SiO4)6 (mp-743769) | 0.5788 | 0.280 | 5 |
Li2ZrFe(PO4)3 (mp-706279) | 0.7215 | 0.303 | 5 |
Li2CuP3(HO5)2 (mp-849277) | 0.7464 | 0.083 | 5 |
Li11Sc7Ti(PO4)12 (mp-695286) | 0.7267 | 0.637 | 5 |
KMg3AlSi3(O5F)2 (mp-684841) | 0.6854 | 0.223 | 6 |
NaCaMgAl(SiO3)4 (mp-720244) | 0.6944 | 0.317 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesNi: 6.2 eV |
PseudopotentialsVASP PAW: Li_sv Ni_pv P O |
Final Energy/Atom-6.3905 eV |
Corrected Energy-328.4458 eV
Uncorrected energy = -293.9638 eV
Composition-based energy adjustment (-0.687 eV/atom x 28.0 atoms) = -19.2360 eV
Composition-based energy adjustment (-2.541 eV/atom x 6.0 atoms) = -15.2460 eV
Corrected energy = -328.4458 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)