Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-2.851 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.016 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLiAlO2 + LiCrO2 |
Band Gap3.777 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 144.2 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 72.1 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 144.2 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 301.3 |
GaAs (mp-2534) | <1 0 0> | <1 0 -1> | 100.9 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 142.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 240.3 |
AlN (mp-661) | <1 0 0> | <1 1 -1> | 111.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 215.2 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 213.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 -1> | 335.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 132.1 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 144.2 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 72.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 142.0 |
BaF2 (mp-1029) | <1 0 0> | <1 0 -1> | 151.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 129.1 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 240.3 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 168.2 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 142.0 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 149.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 43.0 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 144.2 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 213.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 172.2 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 -1> | 302.8 |
InAs (mp-20305) | <1 0 0> | <1 0 -1> | 151.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 129.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 -1> | 100.9 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 142.0 |
KCl (mp-23193) | <1 0 0> | <1 0 -1> | 252.3 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 -1> | 223.6 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 264.3 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 1> | 224.8 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 213.0 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 216.3 |
Te2W (mp-22693) | <1 1 0> | <0 1 0> | 216.3 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 258.3 |
YVO4 (mp-19133) | <1 0 0> | <1 1 -1> | 279.5 |
YVO4 (mp-19133) | <1 1 0> | <0 1 0> | 264.3 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 264.3 |
Te2Mo (mp-602) | <1 0 0> | <0 1 0> | 216.3 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 264.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 86.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 288.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 216.3 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 -1> | 252.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 86.1 |
BN (mp-984) | <0 0 1> | <1 0 0> | 44.0 |
BN (mp-984) | <1 0 1> | <0 1 0> | 120.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Li2MnO3 (mp-565799) | 0.1236 | 0.000 | 3 |
Li2TiO3 (mp-2931) | 0.1228 | 0.000 | 3 |
Na2CdO3 (mp-754782) | 0.1300 | 0.107 | 3 |
Na2US3 (mp-15886) | 0.1238 | 0.000 | 3 |
Li2MnO3 (mp-18988) | 0.1196 | 0.000 | 3 |
Li24Mn11CrO36 (mp-770668) | 0.1557 | 0.000 | 4 |
Li24Mn11CrO36 (mp-770492) | 0.1559 | 0.000 | 4 |
Li4TiCo3O8 (mp-770897) | 0.1356 | 0.063 | 4 |
Li3Al2FeO6 (mp-770727) | 0.0440 | 0.021 | 4 |
Li3Al2VO6 (mp-770102) | 0.1281 | 0.027 | 4 |
LiTe3 (mp-27466) | 0.2962 | 0.009 | 2 |
Bi2Te3 (mp-568390) | 0.3090 | 0.248 | 2 |
In2Se3 (mp-1068548) | 0.3270 | 0.530 | 2 |
In2Se3 (mp-20830) | 0.3356 | 0.530 | 2 |
Sb2Te3 (mp-1080789) | 0.3462 | 0.129 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.4402 | 0.139 | 5 |
Hg (mp-982872) | 0.5236 | 0.020 | 1 |
Sb (mp-632286) | 0.4445 | 0.059 | 1 |
Te (mp-570459) | 0.4829 | 0.044 | 1 |
Te (mp-10654) | 0.5741 | 0.047 | 1 |
Te (mp-105) | 0.4688 | 0.047 | 1 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesCr: 3.7 eV |
PseudopotentialsVASP PAW: Li_sv Al Cr_pv O |
Final Energy/Atom-6.7123 eV |
Corrected Energy-346.6744 eV
Uncorrected energy = -322.1904 eV
Composition-based energy adjustment (-0.687 eV/atom x 24.0 atoms) = -16.4880 eV
Composition-based energy adjustment (-1.999 eV/atom x 4.0 atoms) = -7.9960 eV
Corrected energy = -346.6744 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)