Final Magnetic Moment14.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.444 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.097 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.52 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + SnP2O7 + SnO2 + Mn2P2O7 |
Band Gap0.013 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [146] |
HallR 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 264.3 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 198.2 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 198.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 66.1 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 198.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 198.2 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 264.3 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 264.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 264.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 66.1 |
Al (mp-134) | <1 1 1> | <0 0 1> | 198.2 |
MgO (mp-1265) | <1 0 0> | <0 0 1> | 330.4 |
PbS (mp-21276) | <1 1 0> | <0 0 1> | 264.3 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 66.1 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 330.4 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 198.2 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 66.1 |
MoSe2 (mp-1634) | <1 1 0> | <0 0 1> | 264.3 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 330.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 66.1 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 191.4 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 264.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 66.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 198.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 264.3 |
BN (mp-984) | <0 0 1> | <0 0 1> | 66.1 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 198.2 |
LiGaO2 (mp-5854) | <1 1 0> | <0 0 1> | 198.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 198.2 |
Ge3(BiO3)4 (mp-23560) | <1 1 1> | <0 0 1> | 198.2 |
C (mp-66) | <1 1 1> | <0 0 1> | 66.1 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 330.4 |
PbS (mp-21276) | <1 0 0> | <0 0 1> | 330.4 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 330.4 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 198.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 264.3 |
PbSe (mp-2201) | <1 1 0> | <0 0 1> | 264.3 |
Si (mp-149) | <1 1 0> | <0 0 1> | 330.4 |
Si (mp-149) | <1 1 1> | <0 0 1> | 198.2 |
Au (mp-81) | <1 1 1> | <0 0 1> | 264.3 |
CdSe (mp-2691) | <1 1 0> | <0 0 1> | 264.3 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 66.1 |
WSe2 (mp-1821) | <1 1 0> | <0 0 1> | 264.3 |
WSe2 (mp-1821) | <1 1 1> | <0 0 1> | 264.3 |
ZrO2 (mp-2858) | <0 1 1> | <0 0 1> | 198.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 66.1 |
CaCO3 (mp-3953) | <1 0 0> | <0 0 1> | 264.3 |
YAlO3 (mp-3792) | <1 0 0> | <0 0 1> | 330.4 |
YAlO3 (mp-3792) | <1 1 0> | <0 0 1> | 330.4 |
SiC (mp-8062) | <1 0 0> | <1 0 0> | 191.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
MnPO4 (mp-773411) | 0.3493 | 0.050 | 3 |
VPO4 (mp-861584) | 0.3959 | 0.076 | 3 |
MnCrO4 (mp-769911) | 0.4799 | 0.071 | 3 |
Ti5(PO5)4 (mp-559530) | 0.4698 | 0.000 | 3 |
Cr3AgO8 (mp-560237) | 0.4564 | 0.000 | 3 |
TiCu(PO4)2 (mp-756467) | 0.2746 | 0.053 | 4 |
Mn5Fe(PO4)6 (mp-772374) | 0.2862 | 0.040 | 4 |
TiMn5(PO4)6 (mp-772326) | 0.2585 | 0.037 | 4 |
Mn5V(PO4)6 (mp-773464) | 0.2791 | 0.038 | 4 |
Mn5Nb(PO4)6 (mp-772580) | 0.2462 | 0.043 | 4 |
Cr5O12 (mp-773920) | 0.7311 | 0.000 | 2 |
Mo4O11 (mp-565865) | 0.6942 | 0.005 | 2 |
V5O12 (mp-778252) | 0.7144 | 0.003 | 2 |
Cr3O8 (mp-557959) | 0.7473 | 0.048 | 2 |
VFe3Sb2(PO4)6 (mp-761422) | 0.1890 | 0.049 | 5 |
TiFe3Sn2(PO4)6 (mp-777557) | 0.2182 | 0.069 | 5 |
CrFe3Sn2(PO4)6 (mp-776666) | 0.2113 | 0.082 | 5 |
TiFe3Sb2(PO4)6 (mp-776046) | 0.2038 | 0.039 | 5 |
MnCr3Te2(PO4)6 (mp-765202) | 0.1984 | 0.089 | 5 |
Na2Li3Ti3Al(PO4)6 (mp-769078) | 0.3972 | 0.065 | 6 |
Zr12Si2Bi2P16PbO72 (mp-693759) | 0.3386 | 0.009 | 6 |
LiTi3MnCr(PO4)6 (mp-772224) | 0.2752 | 0.001 | 6 |
Li2Ti2MnCr2(PO4)6 (mp-777244) | 0.3842 | 0.015 | 6 |
Na2LiTi3Al(PO4)6 (mp-769074) | 0.3910 | 0.011 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eVV: 3.25 eV |
PseudopotentialsVASP PAW: Mn_pv V_pv Sn_d P O |
Final Energy/Atom-7.2287 eV |
Corrected Energy-283.8114 eV