Final Magnetic Moment41.010 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFiM |
Formation Energy / Atom-1.642 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.101 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.96 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMnO2 + O2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinC2/m [12] |
Hall-C 2y |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 1> | <0 1 0> | 287.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 287.7 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 117.8 |
TePb (mp-19717) | <1 1 0> | <0 1 0> | 191.8 |
Ag (mp-124) | <1 1 1> | <1 0 0> | 117.8 |
Al (mp-134) | <1 1 1> | <0 1 0> | 287.7 |
CdTe (mp-406) | <1 1 0> | <0 1 0> | 191.8 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 95.9 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 151.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 287.7 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 95.9 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 95.9 |
Ag (mp-124) | <1 1 0> | <0 1 0> | 95.9 |
TeO2 (mp-2125) | <1 0 0> | <0 1 0> | 287.7 |
C (mp-66) | <1 1 0> | <0 1 0> | 287.7 |
InP (mp-20351) | <1 1 0> | <0 1 0> | 95.9 |
Ni (mp-23) | <1 1 0> | <0 1 0> | 191.8 |
InSb (mp-20012) | <1 1 0> | <0 1 0> | 191.8 |
BaTiO3 (mp-5986) | <1 1 1> | <0 1 0> | 287.7 |
MoSe2 (mp-1634) | <1 0 0> | <1 1 0> | 151.9 |
Ga2O3 (mp-886) | <0 1 0> | <0 1 0> | 287.7 |
Ga2O3 (mp-886) | <1 0 0> | <0 1 0> | 287.7 |
Ga2O3 (mp-886) | <1 1 0> | <0 1 0> | 287.7 |
WSe2 (mp-1821) | <1 0 0> | <1 1 0> | 151.9 |
Fe2O3 (mp-24972) | <1 0 0> | <0 1 0> | 287.7 |
Fe2O3 (mp-24972) | <1 0 1> | <0 1 0> | 287.7 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 135.8 |
MgAl2O4 (mp-3536) | <1 0 0> | <0 0 1> | 135.8 |
Ge (mp-32) | <1 1 0> | <0 1 0> | 95.9 |
LiAlO2 (mp-3427) | <0 0 1> | <0 0 1> | 135.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Mg(Mo3O8)2 (mvc-12777) | 0.5929 | 0.234 | 3 |
Zn(Mo3O8)2 (mvc-15081) | 0.6142 | 0.234 | 3 |
Ag15(BiI4)16 (mp-686149) | 0.6029 | 0.041 | 3 |
Ag13(BiI4)14 (mp-686119) | 0.6276 | 0.040 | 3 |
Fe3OF7 (mp-774191) | 0.7042 | 0.121 | 3 |
Mn15O32 (mp-777108) | 0.0859 | 0.097 | 2 |
Mo3O8 (mvc-14257) | 0.7042 | 0.326 | 2 |
Zr63S128 (mp-1024087) | 0.6973 | 0.029 | 2 |
Mo3O8 (mp-715479) | 0.7121 | 0.284 | 2 |
Cr3O8 (mvc-8154) | 0.6451 | 0.376 | 2 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Mn_pv O |
Final Energy/Atom-6.9203 eV |
Corrected Energy-372.9425 eV
-372.9425 eV = -325.2564 eV (uncorrected energy) - 25.2128 eV (MP Advanced Correction) - 22.4733 eV (MP Anion Correction)
|