Final Magnetic Moment3.272 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-2.364 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.051 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.70 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToVO2 + V2O5 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/m [11] |
Hall-P 2yb |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
V3CoO8 (mp-776864) | 0.3661 | 0.248 | 3 |
MnV3O8 (mp-776217) | 0.3661 | 0.057 | 3 |
V3NiO8 (mp-776184) | 0.3824 | 0.052 | 3 |
V3FeO8 (mp-771199) | 0.3830 | 0.043 | 3 |
TiV3O8 (mp-849354) | 0.3964 | 0.029 | 3 |
Li2VOF4 (mp-780857) | 0.6943 | 0.000 | 4 |
LiV2(OF)3 (mp-779825) | 0.7207 | 0.100 | 4 |
LiV2(OF)3 (mp-779071) | 0.7197 | 0.117 | 4 |
Li2V4O5F8 (mp-764711) | 0.4328 | 0.073 | 4 |
V6O13 (mp-715617) | 0.3224 | 0.040 | 2 |
V6O13 (mp-714921) | 0.0296 | 0.064 | 2 |
V6O13 (mp-18896) | 0.1175 | 0.018 | 2 |
V6O13 (mp-19457) | 0.1359 | 0.028 | 2 |
V6O13 (mp-715560) | 0.1268 | 0.028 | 2 |
Na2LiLa3Ti6O18 (mp-676447) | 0.7109 | 0.025 | 5 |
Hg12SbBr(ClO3)2 (mp-642625) | 0.7293 | 0.032 | 5 |
Na11La7Th2Ti20O60 (mp-686371) | 0.7128 | 0.017 | 5 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesV: 3.25 eV |
PseudopotentialsVASP PAW: V_pv O |
Final Energy/Atom-7.6061 eV |
Corrected Energy-327.4766 eV
-327.4766 eV = -289.0330 eV (uncorrected energy) - 20.1840 eV (MP Advanced Correction) - 18.2595 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)