Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.780 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.09 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToDy2Co3Si5 + DySi |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 1 0> | 305.1 |
AlN (mp-661) | <0 0 1> | <0 1 0> | 224.8 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 321.2 |
AlN (mp-661) | <1 1 1> | <0 1 0> | 256.9 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 144.5 |
GaAs (mp-2534) | <1 1 0> | <1 0 1> | 91.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 80.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 1 0> | 289.0 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 80.3 |
AlN (mp-661) | <1 0 1> | <0 1 0> | 192.7 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 289.0 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 337.2 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 32.1 |
GaAs (mp-2534) | <1 1 1> | <0 1 0> | 289.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 91.9 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 323.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 160.6 |
ZnSe (mp-1190) | <1 1 0> | <1 0 1> | 91.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 16.1 |
GaN (mp-804) | <1 0 0> | <0 1 0> | 240.9 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 194.1 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 266.6 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 93.3 |
LiF (mp-1138) | <1 0 0> | <0 1 0> | 16.1 |
LiF (mp-1138) | <1 1 0> | <0 1 0> | 112.4 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 256.9 |
SiO2 (mp-6930) | <1 0 1> | <0 1 0> | 273.0 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 353.3 |
Te2W (mp-22693) | <0 0 1> | <0 1 0> | 240.9 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 266.6 |
Te2W (mp-22693) | <0 1 1> | <0 1 0> | 289.0 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 80.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 128.5 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 1> | 91.9 |
DyScO3 (mp-31120) | <1 1 0> | <0 1 0> | 64.2 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 80.3 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 337.2 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 32.1 |
ZnSe (mp-1190) | <1 1 1> | <0 1 0> | 289.0 |
Te2Mo (mp-602) | <0 0 1> | <0 1 0> | 176.6 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 144.5 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 194.1 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 240.9 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 1> | 67.2 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 1> | 275.6 |
CdS (mp-672) | <0 0 1> | <0 1 0> | 289.0 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 256.9 |
CdS (mp-672) | <1 1 1> | <0 1 0> | 208.8 |
LiF (mp-1138) | <1 1 1> | <0 1 0> | 144.5 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 0> | 240.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
177 | 68 | 58 | 0 | 0 | 0 |
68 | 182 | 96 | 0 | 0 | 0 |
58 | 96 | 211 | 0 | 0 | 0 |
0 | 0 | 0 | 72 | 0 | 0 |
0 | 0 | 0 | 0 | 49 | 0 |
0 | 0 | 0 | 0 | 0 | 66 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
6.7 | -2 | -1 | 0 | 0 | 0 |
-2 | 7.8 | -3 | 0 | 0 | 0 |
-1 | -3 | 6.4 | 0 | 0 | 0 |
0 | 0 | 0 | 14 | 0 | 0 |
0 | 0 | 0 | 0 | 20.2 | 0 |
0 | 0 | 0 | 0 | 0 | 15.1 |
Shear Modulus GV61 GPa |
Bulk Modulus KV113 GPa |
Shear Modulus GR59 GPa |
Bulk Modulus KR111 GPa |
Shear Modulus GVRH60 GPa |
Bulk Modulus KVRH112 GPa |
Elastic Anisotropy0.18 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoCoSi2 (mp-8743) | 0.0405 | 0.005 | 3 |
CeCoSi2 (mp-7095) | 0.1322 | 0.000 | 3 |
TmCoSi2 (mp-1025408) | 0.0835 | 0.014 | 3 |
ErCoSi2 (mp-3128) | 0.0772 | 0.000 | 3 |
TbCoSi2 (mp-4969) | 0.0377 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Dy_3 Co Si |
Final Energy/Atom-6.4209 eV |
Corrected Energy-51.0833 eV
Uncorrected energy = -51.3673 eV
Composition-based energy adjustment (0.071 eV/atom x 4.0 atoms) = 0.2840 eV
Corrected energy = -51.0833 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)