material

Ca2ZnN2

ID:

mp-8818

DOI:

10.17188/1312752


Tags: Dicalcium zinc nitride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.861 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.52 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.770 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 69049 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
NaCl (mp-22862) <1 0 0> <0 0 1> 0.000 64.8
PbS (mp-21276) <1 0 0> <0 0 1> 0.000 324.0
Al2O3 (mp-1143) <1 0 0> <1 0 1> 0.002 189.1
KTaO3 (mp-3614) <1 0 0> <0 0 1> 0.004 64.8
GaSe (mp-1943) <1 0 0> <0 0 1> 0.011 272.2
TiO2 (mp-390) <0 0 1> <0 0 1> 0.019 116.6
Al (mp-134) <1 0 0> <0 0 1> 0.021 64.8
YVO4 (mp-19133) <1 0 1> <0 0 1> 0.024 207.4
LaAlO3 (mp-2920) <1 0 0> <1 0 1> 0.027 141.8
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.027 51.8
TbScO3 (mp-31119) <1 0 0> <0 0 1> 0.027 324.0
Te2W (mp-22693) <1 1 1> <1 0 0> 0.029 227.3
LiGaO2 (mp-5854) <0 1 1> <1 1 0> 0.029 128.6
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.032 236.4
SiC (mp-8062) <1 1 0> <1 0 0> 0.032 136.4
Al (mp-134) <1 1 0> <0 0 1> 0.033 324.0
Cu (mp-30) <1 0 0> <0 0 1> 0.037 13.0
C (mp-66) <1 1 0> <0 0 1> 0.038 90.7
DyScO3 (mp-31120) <1 0 0> <0 0 1> 0.044 324.0
CdS (mp-672) <1 0 0> <1 1 0> 0.044 257.2
CaCO3 (mp-3953) <1 0 1> <0 0 1> 0.044 90.7
ZnO (mp-2133) <1 1 1> <0 0 1> 0.046 285.1
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.046 64.8
AlN (mp-661) <1 0 1> <0 0 1> 0.049 194.4
ZnSe (mp-1190) <1 1 0> <0 0 1> 0.054 324.0
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.054 181.8
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.054 181.8
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.056 272.2
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.059 64.8
Cu (mp-30) <1 1 1> <0 0 1> 0.065 246.3
WS2 (mp-224) <1 0 1> <0 0 1> 0.066 233.3
GaTe (mp-542812) <1 0 0> <0 0 1> 0.067 311.1
TiO2 (mp-2657) <1 1 0> <1 0 1> 0.072 236.4
NaCl (mp-22862) <1 1 0> <0 0 1> 0.075 324.0
GaAs (mp-2534) <1 1 0> <0 0 1> 0.076 324.0
SrTiO3 (mp-4651) <1 0 0> <0 0 1> 0.079 349.9
AlN (mp-661) <0 0 1> <1 0 0> 0.084 136.4
SiC (mp-7631) <1 0 1> <0 0 1> 0.085 337.0
Mg (mp-153) <1 0 1> <0 0 1> 0.088 285.1
LiGaO2 (mp-5854) <1 1 1> <1 0 1> 0.089 330.9
C (mp-66) <1 0 0> <0 0 1> 0.090 13.0
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.092 324.0
Ag (mp-124) <1 1 1> <0 0 1> 0.094 207.4
Ge(Bi3O5)4 (mp-23352) <1 1 1> <1 0 0> 0.094 181.8
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.095 236.4
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.096 194.4
BN (mp-984) <1 0 1> <0 0 1> 0.103 181.5
Te2W (mp-22693) <1 0 0> <1 1 0> 0.110 192.9
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.111 349.9
SiC (mp-11714) <1 0 0> <0 0 1> 0.113 155.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
148 28 41 0 0 0
28 148 41 0 0 0
41 41 218 0 0 0
0 0 0 29 0 0
0 0 0 0 29 0
0 0 0 0 0 51
Compliance Tensor Sij (10-12Pa-1)
7.3 -1 -1.2 0 0 0
-1 7.3 -1.2 0 0 0
-1.2 -1.2 5 0 0 0
0 0 0 34.6 0 0
0 0 0 0 34.6 0
0 0 0 0 0 19.6
Shear Modulus GV
49 GPa
Bulk Modulus KV
82 GPa
Shear Modulus GR
42 GPa
Bulk Modulus KR
78 GPa
Shear Modulus GVRH
45 GPa
Bulk Modulus KVRH
80 GPa
Elastic Anisotropy
0.86
Poisson's Ratio
0.26

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
5.60 0.00 0.00
0.00 5.60 -0.00
0.00 -0.00 7.87
Dielectric Tensor εij (total)
15.36 -0.01 0.00
-0.01 15.36 -0.00
0.00 -0.00 15.31
Polycrystalline dielectric constant εpoly
(electronic contribution)
6.35
Polycrystalline dielectric constant εpoly
(total)
15.35
Refractive Index n
2.52
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr2ZnN2 (mp-9306) 0.1871 0.000 3
Cs2HgO2 (mp-7232) 0.3515 0.000 3
K2HgO2 (mp-5860) 0.2422 0.000 3
Ca2CoN2 (mp-1029532) 0.2470 0.007 3
Rb2HgO2 (mp-5072) 0.2629 0.000 3
Li2V3NiO8 (mp-776203) 0.7281 0.073 4
Li2V3CoO8 (mp-777304) 0.7299 0.269 4
Li2V3CrO8 (mp-849964) 0.7103 0.070 4
Ba3ZnN2O (mp-545788) 0.7061 0.007 4
Li2V3FeO8 (mp-771747) 0.7290 0.114 4
Cr3N2 (mp-1014303) 0.7119 0.147 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Zn N
Final Energy/Atom
-5.0939 eV
Corrected Energy
-26.1913 eV
Uncorrected energy = -25.4693 eV Composition-based energy adjustment (-0.361 eV/atom x 2.0 atoms) = -0.7220 eV Corrected energy = -26.1913 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 69049
Submitted by
User remarks:
  • Dicalcium zinc nitride

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)