Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.089 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP62m [189] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 281.2 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 328.1 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 54.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 162.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 46.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 54.3 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 217.1 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 217.1 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 217.1 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 46.9 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 187.5 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 293.0 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 234.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 0> | 281.2 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 217.1 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 140.6 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 243.5 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 217.1 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 217.1 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 162.8 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 143.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 140.6 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 162.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 328.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 140.6 |
BN (mp-984) | <1 0 1> | <1 0 0> | 140.6 |
BN (mp-984) | <1 1 0> | <1 0 0> | 140.6 |
BN (mp-984) | <1 1 1> | <1 0 0> | 234.4 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 215.1 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 217.1 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 195.3 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 234.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 93.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 328.1 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 162.8 |
Bi2Se3 (mp-541837) | <0 0 1> | <1 1 0> | 243.5 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 162.4 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 234.4 |
InAs (mp-20305) | <1 0 0> | <1 1 1> | 195.3 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 162.8 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 325.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 54.3 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 162.8 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 271.3 |
Al (mp-134) | <1 0 0> | <0 0 1> | 162.8 |
Al (mp-134) | <1 1 0> | <0 0 1> | 271.3 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 234.4 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 286.8 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 217.1 |
TeO2 (mp-2125) | <0 0 1> | <1 1 0> | 162.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
90 | 38 | 21 | 0 | 0 | 0 |
38 | 90 | 21 | 0 | 0 | 0 |
21 | 21 | 93 | 0 | 0 | 0 |
0 | 0 | 0 | 28 | 0 | 0 |
0 | 0 | 0 | 0 | 28 | 0 |
0 | 0 | 0 | 0 | 0 | 26 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
13.9 | -5.5 | -1.8 | 0 | 0 | 0.0 |
-5.5 | 13.9 | -1.8 | 0 | 0 | 0.0 |
-1.8 | -1.8 | 11.5 | 0 | 0 | -0.0 |
0 | 0 | 0 | 36.1 | 0.0 | 0 |
0 | 0 | 0 | 0.0 | 36.1 | 0 |
0.0 | 0.0 | -0.0 | 0 | 0 | 38.8 |
Shear Modulus GV29 GPa |
Bulk Modulus KV48 GPa |
Shear Modulus GR28 GPa |
Bulk Modulus KR48 GPa |
Shear Modulus GVRH29 GPa |
Bulk Modulus KVRH48 GPa |
Elastic Anisotropy0.13 |
Poisson's Ratio0.25 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv As |
Final Energy/Atom-4.4215 eV |
Corrected Energy-53.0584 eV
-53.0584 eV = -53.0584 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)