Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingUnknown |
Formation Energy / Atom-1.184 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.68 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 215.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 215.5 |
AlN (mp-661) | <0 0 1> | <1 0 1> | 186.9 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 232.0 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 198.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 198.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 281.8 |
CeO2 (mp-20194) | <1 0 0> | <1 1 0> | 58.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 167.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 49.7 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 290.1 |
GaAs (mp-2534) | <1 1 0> | <1 1 1> | 181.0 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 198.9 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 267.9 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 66.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 116.0 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 181.0 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 248.7 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 198.9 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 261.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 265.3 |
Te2W (mp-22693) | <0 1 1> | <1 0 1> | 299.0 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 66.3 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 201.0 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 331.6 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 186.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 265.3 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 336.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 215.5 |
TePb (mp-19717) | <1 0 0> | <1 0 1> | 336.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 248.7 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 215.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 149.2 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 265.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 265.3 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 248.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 1> | 181.0 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 265.3 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 265.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 66.3 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 290.1 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 116.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 16.6 |
Bi2Te3 (mp-34202) | <1 0 0> | <0 0 1> | 132.6 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 290.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 1> | 181.0 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 215.5 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 49.7 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 281.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 0> | 290.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
SrHg2 (mp-11472) | 0.6908 | 0.003 | 2 |
ThZn2 (mp-7496) | 0.6833 | 0.000 | 2 |
CeO2 (mp-1018659) | 0.6199 | 0.443 | 2 |
ThCu2 (mp-1377) | 0.6828 | 0.000 | 2 |
BaHg2 (mp-11267) | 0.6612 | 0.000 | 2 |
YSiAu (mp-9025) | 0.1151 | 0.000 | 3 |
CeGeAu (mp-4219) | 0.0806 | 0.000 | 3 |
NdGeAu (mp-1018826) | 0.2337 | 0.000 | 3 |
GdCuGe (mp-13212) | 0.0903 | 0.000 | 3 |
LaAgGe (mp-20568) | 0.2539 | 0.000 | 3 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points30 |
U Values-- |
PseudopotentialsVASP PAW: As Pd Sm_3 |
Final Energy/Atom-6.0337 eV |
Corrected Energy-36.2025 eV
-36.2025 eV = -36.2025 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)