material

NaSi2N3

ID:

mp-8973

DOI:

10.17188/1312873


Tags: Sodium disilicon nitride

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Unknown
Formation Energy / Atom
-1.220 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.11 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
4.184 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cmc21 [36]
Hall
C 2c 2
Point Group
mm2
Crystal System
orthorhombic

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
WS2 (mp-224) <1 1 1> <0 0 1> 0.003 158.2
Mg (mp-153) <0 0 1> <0 0 1> 0.019 52.7
LiAlO2 (mp-3427) <1 1 0> <1 0 1> 0.021 141.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.032 52.7
WS2 (mp-224) <0 0 1> <0 0 1> 0.032 52.7
MoS2 (mp-1434) <1 1 0> <0 1 1> 0.046 118.6
GaN (mp-804) <0 0 1> <0 1 1> 0.048 178.0
ZrO2 (mp-2858) <1 1 -1> <0 1 0> 0.053 136.0
GdScO3 (mp-5690) <0 1 1> <0 1 0> 0.057 54.4
LaF3 (mp-905) <0 0 1> <0 0 1> 0.060 316.3
WS2 (mp-224) <1 1 0> <0 0 1> 0.061 158.2
C (mp-48) <0 0 1> <0 1 0> 0.066 190.4
LiF (mp-1138) <1 1 0> <0 1 0> 0.075 353.5
SiC (mp-11714) <1 1 0> <1 0 0> 0.077 327.6
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.114 105.4
GaTe (mp-542812) <1 0 0> <0 1 1> 0.121 178.0
LiTaO3 (mp-3666) <1 0 0> <0 1 0> 0.122 217.6
GaSe (mp-1943) <0 0 1> <1 0 0> 0.124 187.2
TbScO3 (mp-31119) <0 1 1> <0 1 0> 0.131 54.4
TiO2 (mp-390) <1 0 0> <1 0 0> 0.136 187.2
TeO2 (mp-2125) <0 1 0> <0 1 0> 0.151 136.0
SiO2 (mp-6930) <1 1 0> <0 1 0> 0.151 190.4
LiGaO2 (mp-5854) <1 0 1> <0 1 0> 0.163 136.0
TbScO3 (mp-31119) <0 0 1> <0 0 1> 0.167 158.2
CdWO4 (mp-19387) <0 1 0> <0 1 1> 0.170 237.3
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.186 52.7
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.204 158.2
LaF3 (mp-905) <1 1 0> <1 0 1> 0.208 282.0
Ni (mp-23) <1 1 1> <0 1 0> 0.212 299.2
CsI (mp-614603) <1 1 1> <0 0 1> 0.215 105.4
DyScO3 (mp-31120) <0 0 1> <0 0 1> 0.220 158.2
DyScO3 (mp-31120) <0 1 1> <0 1 0> 0.230 54.4
NdGaO3 (mp-3196) <1 0 1> <0 0 1> 0.245 52.7
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.252 158.2
CdS (mp-672) <1 1 1> <1 0 1> 0.263 211.5
GdScO3 (mp-5690) <1 0 1> <1 0 0> 0.268 280.8
TbScO3 (mp-31119) <1 0 1> <1 0 0> 0.277 280.8
InP (mp-20351) <1 1 1> <0 1 0> 0.278 244.8
SrTiO3 (mp-4651) <1 0 0> <0 1 1> 0.286 178.0
GdScO3 (mp-5690) <1 1 1> <1 1 0> 0.287 216.5
ZnO (mp-2133) <1 0 0> <0 1 1> 0.288 178.0
CdS (mp-672) <0 0 1> <0 0 1> 0.292 105.4
LaF3 (mp-905) <1 0 0> <1 0 1> 0.294 211.5
DyScO3 (mp-31120) <1 0 1> <1 0 0> 0.304 280.8
YAlO3 (mp-3792) <1 1 0> <1 0 1> 0.307 282.0
ZnO (mp-2133) <1 1 1> <0 1 0> 0.312 217.6
SiC (mp-7631) <0 0 1> <0 1 0> 0.325 108.8
SiC (mp-11714) <0 0 1> <0 1 0> 0.332 108.8
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.338 210.9
Si (mp-149) <1 1 0> <0 0 1> 0.342 210.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
332 121 87 0 0 0
121 429 67 0 0 0
87 67 365 0 0 0
0 0 0 89 0 0
0 0 0 0 130 0
0 0 0 0 0 92
Compliance Tensor Sij (10-12Pa-1)
3.5 -0.9 -0.7 0 0 0
-0.9 2.6 -0.3 0 0 0
-0.7 -0.3 2.9 0 0 0
0 0 0 11.2 0 0
0 0 0 0 7.7 0
0 0 0 0 0 10.8
Shear Modulus GV
119 GPa
Bulk Modulus KV
186 GPa
Shear Modulus GR
113 GPa
Bulk Modulus KR
184 GPa
Shear Modulus GVRH
116 GPa
Bulk Modulus KVRH
185 GPa
Elastic Anisotropy
0.28
Poisson's Ratio
0.24

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 0.05958 0.00000
0.00000 0.00000 0.00000 -0.15479 0.00000 0.00000
-0.00329 -0.28810 0.28240 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.28240 C/m2
Crystallographic Direction vmax
0.00000
0.00000
1.00000

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
36
U Values
--
Pseudopotentials
VASP PAW: N Na_pv Si
Final Energy/Atom
-7.2232 eV
Corrected Energy
-86.6790 eV
-86.6790 eV = -86.6790 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations

User Data

dtu

Authors:
name conditions value ref
band gap
type
indirect
method
Kohn-Sham
functional
GLLB-SC
5.06 eV
band gap
type
direct
method
Kohn-Sham
functional
GLLB-SC
5.09 eV
band gap
type
indirect
method
quasiparticle
functional
GLLB-SC
6.87 eV
band gap
type
direct
method
quasiparticle
functional
GLLB-SC
6.90 eV
derivative discontinuity
functional
GLLB-SC
1.81 eV

Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 72466

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)