material

KPdF3

ID:

mp-9061

DOI:

10.17188/1312942


Tags: Potassium trifluoropalladate

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.135 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.032 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.20 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
K2PdF6 + Pd
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Pm3m [221]
Hall
-P 4 2 3
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 73167 from Topological Materials Database
Topological Classification
SM*
Subclassification
ESFD
Crossing Type
Point
* Semimetal
Enforced Semimetal with Fermi point Degeneracy
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
YVO4 (mp-19133) <1 0 1> <1 0 0> 0.000 278.5
NaCl (mp-22862) <1 1 1> <1 1 1> 0.004 225.1
TePb (mp-19717) <1 1 1> <1 1 1> 0.009 225.1
Ni (mp-23) <1 1 0> <1 1 0> 0.013 52.5
C (mp-66) <1 0 0> <1 0 0> 0.015 167.1
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.015 148.6
Ge (mp-32) <1 0 0> <1 0 0> 0.017 167.1
Si (mp-149) <1 0 0> <1 0 0> 0.017 148.6
C (mp-48) <1 0 0> <1 1 0> 0.020 288.9
SiO2 (mp-6930) <1 0 1> <1 1 0> 0.023 105.0
TeO2 (mp-2125) <1 0 0> <1 1 0> 0.031 210.1
YAlO3 (mp-3792) <0 1 1> <1 1 1> 0.031 96.5
LiGaO2 (mp-5854) <1 0 1> <1 0 0> 0.033 222.8
LaAlO3 (mp-2920) <1 0 1> <1 1 1> 0.033 225.1
GdScO3 (mp-5690) <0 1 0> <1 0 0> 0.034 352.8
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.035 297.1
Bi2Te3 (mp-34202) <0 0 1> <1 1 1> 0.036 225.1
GaN (mp-804) <1 0 0> <1 1 0> 0.036 183.8
LiF (mp-1138) <1 1 0> <1 1 0> 0.039 210.1
Mg (mp-153) <1 0 0> <1 1 0> 0.040 183.8
LiAlO2 (mp-3427) <1 1 0> <1 1 0> 0.040 236.4
C (mp-48) <1 1 1> <1 0 0> 0.041 204.3
LiF (mp-1138) <1 0 0> <1 0 0> 0.042 148.6
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.043 352.8
GaAs (mp-2534) <1 0 0> <1 0 0> 0.047 167.1
Au (mp-81) <1 1 1> <1 0 0> 0.048 334.3
Al (mp-134) <1 1 0> <1 1 0> 0.051 210.1
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.053 78.8
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.053 352.8
GaN (mp-804) <1 1 0> <1 1 0> 0.054 236.4
Al (mp-134) <1 0 0> <1 0 0> 0.056 148.6
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.065 92.8
CdTe (mp-406) <1 1 1> <1 1 1> 0.073 225.1
SiC (mp-11714) <1 0 1> <1 0 0> 0.073 130.0
ZnSe (mp-1190) <1 0 0> <1 0 0> 0.074 167.1
TiO2 (mp-390) <1 0 0> <1 1 0> 0.074 183.8
CdWO4 (mp-19387) <1 0 0> <1 1 0> 0.075 157.6
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.076 241.4
WSe2 (mp-1821) <0 0 1> <1 0 0> 0.077 260.0
MoSe2 (mp-1634) <0 0 1> <1 0 0> 0.078 260.0
ZnSe (mp-1190) <1 1 1> <1 1 1> 0.078 225.1
InSb (mp-20012) <1 1 1> <1 1 1> 0.086 225.1
SiC (mp-7631) <1 0 0> <1 0 0> 0.087 92.8
ZrO2 (mp-2858) <0 1 1> <1 0 0> 0.088 278.5
WS2 (mp-224) <1 1 0> <1 0 0> 0.089 315.7
Ag (mp-124) <1 1 1> <1 0 0> 0.091 334.3
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.091 210.1
SiC (mp-7631) <1 1 0> <1 1 1> 0.096 160.8
GaSe (mp-1943) <0 0 1> <1 0 0> 0.096 241.4
CaCO3 (mp-3953) <1 0 0> <1 1 0> 0.096 262.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
120 42 42 0 0 0
42 120 42 0 0 0
42 42 120 0 0 0
0 0 0 13 0 0
0 0 0 0 13 0
0 0 0 0 0 13
Compliance Tensor Sij (10-12Pa-1)
10.2 -2.6 -2.6 0 0 0
-2.6 10.2 -2.6 0 0 0
-2.6 -2.6 10.2 0 0 0
0 0 0 76.5 0 0
0 0 0 0 76.5 0
0 0 0 0 0 76.5
Shear Modulus GV
23 GPa
Bulk Modulus KV
68 GPa
Shear Modulus GR
18 GPa
Bulk Modulus KR
68 GPa
Shear Modulus GVRH
21 GPa
Bulk Modulus KVRH
68 GPa
Elastic Anisotropy
1.58
Poisson's Ratio
0.36

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
CsPbCl3 (mp-23037) 0.0000 0.007 3
Lu3AlN (mp-1017627) 0.0000 0.000 3
Tb3AlC (mp-570822) 0.0000 0.000 3
Nd3AlC (mp-571330) 0.0000 0.026 3
RbMnF3 (mp-623245) 0.0000 0.000 3
Ba2VFeO6 (mp-1096778) 0.0000 2.635 4
Ba2ScSbO6 (mp-20709) 0.0000 2.196 4
Ba2YbSbO6 (mp-14223) 0.0000 1.747 4
Ba2YSbO6 (mp-14226) 0.0000 2.082 4
Ba2NbFeO6 (mp-1096853) 0.0000 2.952 4
Sr3Sb2 (mp-1013583) 0.0000 0.381 2
Ba3Bi2 (mp-1013736) 0.0000 0.388 2
Sr3P2 (mp-1013552) 0.0000 0.403 2
Sr3As2 (mp-1013559) 0.0000 0.367 2
Ba3As2 (mp-1013560) 0.0000 0.418 2
BaLaMgBiO6 (mp-41414) 0.0488 0.096 5
BaLaMgNbO6 (mp-39288) 0.0712 0.090 5
SrLaNbZnO6 (mp-41918) 0.0665 0.126 5
SrLaMnCoO6 (mp-40761) 0.0404 0.247 5
Sr6Ca2MnFe7O24 (mp-1075969) 0.0482 0.021 5
Na5Ca2Ce3Ti8Nb2O30 (mp-721094) 0.7380 0.065 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: K_sv Pd F
Final Energy/Atom
-4.2446 eV
Corrected Energy
-21.2228 eV
-21.2228 eV = -21.2228 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 73167
  • 6047
Submitted by
User remarks:
  • Potassium trifluoropalladate

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)