Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.837 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.60 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.607 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP62m [189] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <0 0 1> | 266.0 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 266.0 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 146.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 88.7 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 111.3 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 266.0 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 202.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 202.0 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 266.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 88.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 269.4 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 222.7 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 88.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 88.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 266.0 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 134.7 |
Ag (mp-124) | <1 1 0> | <1 0 1> | 222.7 |
GaSe (mp-1943) | <1 1 0> | <1 1 0> | 116.6 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 134.7 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 1> | 111.3 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 67.3 |
LiGaO2 (mp-5854) | <1 1 0> | <1 0 0> | 202.0 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 116.6 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 116.6 |
C (mp-66) | <1 0 0> | <1 0 0> | 202.0 |
GdScO3 (mp-5690) | <1 1 1> | <1 0 1> | 222.7 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 146.5 |
TeO2 (mp-2125) | <1 0 1> | <1 1 0> | 233.3 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 269.4 |
LaF3 (mp-905) | <1 0 0> | <0 0 1> | 266.0 |
C (mp-66) | <1 1 1> | <0 0 1> | 88.7 |
TbScO3 (mp-31119) | <0 1 1> | <1 0 0> | 269.4 |
TbScO3 (mp-31119) | <1 1 1> | <1 0 1> | 222.7 |
InSb (mp-20012) | <1 0 0> | <1 0 0> | 134.7 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 266.0 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 266.0 |
SiC (mp-11714) | <1 0 0> | <1 0 1> | 222.7 |
SiC (mp-11714) | <1 1 0> | <1 0 0> | 269.4 |
SiC (mp-11714) | <1 1 1> | <1 0 0> | 269.4 |
MoSe2 (mp-1634) | <1 0 0> | <1 0 0> | 202.0 |
Au (mp-81) | <1 1 0> | <1 0 1> | 222.7 |
C (mp-48) | <1 0 1> | <1 0 1> | 222.7 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 202.0 |
WSe2 (mp-1821) | <1 0 1> | <1 0 0> | 202.0 |
Au (mp-81) | <1 1 1> | <0 0 1> | 88.7 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 266.0 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 266.0 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 88.7 |
ZrO2 (mp-2858) | <1 1 -1> | <1 1 0> | 233.3 |
MgF2 (mp-1249) | <1 1 0> | <1 0 0> | 202.0 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
-0.02275 | 0.02274 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.02274 |
0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.03217 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
3.26 | -0.00 | 0.00 |
-0.00 | 3.26 | 0.00 |
0.00 | 0.00 | 6.22 |
Dielectric Tensor εij (total) |
||
---|---|---|
5.46 | -0.00 | 0.00 |
-0.00 | 5.46 | 0.00 |
0.00 | 0.00 | 9.81 |
Polycrystalline dielectric constant
εpoly∞
4.25
|
Polycrystalline dielectric constant
εpoly
6.91
|
Refractive Index n2.06 |
Potentially ferroelectric?Unknown |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Rb_sv Te |
Final Energy/Atom-2.8992 eV |
Corrected Energy-34.7906 eV
-34.7906 eV = -34.7906 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)