Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.119 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.001 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCsPrS2 |
Band Gap2.259 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3m [166] |
Hall-R 3 2" |
Point Group3m |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 302.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 111.4 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 318.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 238.8 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 191.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 238.8 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 207.0 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 334.3 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 318.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 207.0 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 63.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 334.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 238.8 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 302.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 63.7 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 270.7 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 318.4 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 159.2 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 334.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 238.8 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 207.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 238.8 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 318.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 191.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 63.7 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 334.3 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 318.4 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 111.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 15.9 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 318.4 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 238.8 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 254.7 |
CdS (mp-672) | <1 1 1> | <0 0 1> | 270.7 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 334.3 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 111.4 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 382.1 |
Te2W (mp-22693) | <1 1 1> | <0 0 1> | 238.8 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 159.2 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 334.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 238.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 302.5 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 143.3 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 104.2 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 127.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 207.0 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 207.0 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 47.8 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 207.0 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 270.7 |
BN (mp-984) | <0 0 1> | <0 0 1> | 15.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbTmS2 (mp-9368) | 0.0521 | 0.000 | 3 |
RbErS2 (mp-9367) | 0.0583 | 0.000 | 3 |
CsNdS2 (mp-9081) | 0.0422 | 0.002 | 3 |
CsCeS2 (mp-7015) | 0.0515 | 0.000 | 3 |
Ba2BrN (mp-1018098) | 0.0598 | 0.000 | 3 |
Na3Mn2SbO6 (mp-985626) | 0.7253 | 0.361 | 4 |
Na3Ni2SbO6 (mp-971678) | 0.5939 | 0.000 | 4 |
Na2Li(NiO2)3 (mp-773956) | 0.6807 | 0.031 | 4 |
Na3Co2SbO6 (mp-561940) | 0.6997 | 0.015 | 4 |
Na3Co2SbO6 (mp-19087) | 0.6381 | 0.000 | 4 |
SbTe (mp-7716) | 0.5388 | 0.009 | 2 |
Bi8Se7 (mp-680214) | 0.5096 | 0.009 | 2 |
Ag2O (mp-7711) | 0.4370 | 0.120 | 2 |
TlS (mp-998912) | 0.5066 | 0.062 | 2 |
Sb2Te3 (mp-1201) | 0.5329 | 0.000 | 2 |
Na6MnNi3(SbO6)2 (mp-1094109) | 0.6323 | 0.139 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cs_sv Pr_3 S |
Final Energy/Atom-5.2750 eV |
Corrected Energy-22.1060 eV
Uncorrected energy = -21.1000 eV
Composition-based energy adjustment (-0.503 eV/atom x 2.0 atoms) = -1.0060 eV
Corrected energy = -22.1060 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)