Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.718 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.20 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap5.121 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Topological Classificationtrivial*
|
SubclassificationLCEBR†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 297.7 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 160.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 205.7 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 366.4 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 137.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 366.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 343.5 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 160.3 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 120.9 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 274.8 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 274.8 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 183.2 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 320.6 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 144.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 343.5 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 22.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 320.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 251.9 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 241.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 160.3 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 120.9 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 114.5 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 274.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.7 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 241.8 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 206.1 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 206.1 |
LiF (mp-1138) | <1 0 0> | <0 0 1> | 366.4 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 366.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 91.6 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 274.8 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 297.7 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 206.1 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 274.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 274.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 366.4 |
Ag (mp-124) | <1 1 0> | <0 0 1> | 366.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 91.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 68.7 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 91.6 |
GaP (mp-2490) | <1 1 0> | <0 0 1> | 343.5 |
GaP (mp-2490) | <1 1 1> | <0 0 1> | 160.3 |
TbScO3 (mp-31119) | <0 1 0> | <0 0 1> | 343.5 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 183.2 |
Ni (mp-23) | <1 1 0> | <0 0 1> | 366.4 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 274.8 |
InSb (mp-20012) | <1 1 1> | <0 0 1> | 297.7 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 114.5 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
2.00 | -0.00 | 0.00 |
-0.00 | 2.00 | -0.00 |
0.00 | -0.00 | 2.01 |
Dielectric Tensor εij (total) |
||
---|---|---|
5.13 | -0.00 | 0.00 |
-0.00 | 5.13 | -0.00 |
0.00 | -0.00 | 5.72 |
Polycrystalline dielectric constant
εpoly∞
2.00
|
Polycrystalline dielectric constant
εpoly
5.33
|
Refractive Index n1.42 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaMoF6 (mvc-11084) | 0.1400 | 0.000 | 3 |
CaVF6 (mvc-15849) | 0.1431 | 0.001 | 3 |
CaFeF6 (mvc-15840) | 0.1370 | 0.170 | 3 |
CaCoF6 (mvc-15833) | 0.1617 | 0.000 | 3 |
CaTiF6 (mvc-14834) | 0.1073 | 0.009 | 3 |
Cs2LiAl3F12 (mp-13634) | 0.5302 | 0.000 | 4 |
NiF3 (mp-614777) | 0.3755 | 0.082 | 2 |
CrF3 (mp-560338) | 0.4303 | 0.000 | 2 |
CrF3 (mp-608175) | 0.4317 | 0.000 | 2 |
CoF3 (mp-561038) | 0.4037 | 0.052 | 2 |
PdF3 (mp-14112) | 0.3915 | 0.028 | 2 |
TiTlWO5F (mp-690560) | 0.6902 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv As F |
Final Energy/Atom-4.6042 eV |
Corrected Energy-36.8339 eV
-36.8339 eV = -36.8339 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)