Final Magnetic Moment1.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom-1.600 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.032 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.75 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCuO + GeO2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPmma [51] |
Hall-P 2a 2a |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 207.6 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 0> | 256.1 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 213.3 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 46.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 103.8 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 131.8 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 256.1 |
GaAs (mp-2534) | <1 0 0> | <1 1 0> | 102.5 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 192.8 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 79.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 0> | 219.6 |
BaF2 (mp-1029) | <1 1 1> | <0 1 1> | 272.2 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 158.2 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 252.1 |
GaN (mp-804) | <0 0 1> | <0 1 1> | 242.0 |
GaN (mp-804) | <1 0 0> | <1 1 1> | 266.7 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 175.7 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 263.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 281.8 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 43.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 133.5 |
SiO2 (mp-6930) | <1 0 1> | <1 0 1> | 139.1 |
SiO2 (mp-6930) | <1 1 0> | <0 1 0> | 237.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 0> | 219.6 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 79.1 |
KCl (mp-23193) | <1 1 0> | <1 0 0> | 219.6 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 153.7 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 252.1 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 263.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 281.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 175.7 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 252.1 |
DyScO3 (mp-31120) | <1 1 1> | <0 1 0> | 210.9 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 79.1 |
InAs (mp-20305) | <1 1 0> | <1 0 0> | 219.6 |
InAs (mp-20305) | <1 1 1> | <1 0 0> | 131.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 341.1 |
ZnSe (mp-1190) | <1 0 0> | <1 1 0> | 102.5 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 192.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 79.1 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 204.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 222.5 |
Ag (mp-124) | <1 0 0> | <0 1 0> | 52.7 |
Ag (mp-124) | <1 1 0> | <0 1 1> | 121.0 |
Ag (mp-124) | <1 1 1> | <0 1 0> | 210.9 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 272.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 311.5 |
CdS (mp-672) | <1 0 0> | <1 1 1> | 320.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 222.5 |
CdS (mp-672) | <1 1 0> | <0 0 1> | 252.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CuSiO3 (mp-16053) | 0.4887 | 0.088 | 3 |
AgGeO3 (mp-779664) | 0.4045 | 0.086 | 3 |
CuGeO3 (mp-561216) | 0.1576 | 0.021 | 3 |
CuGeO3 (mp-917381) | 0.0770 | 0.032 | 3 |
AgGeO3 (mp-779706) | 0.4106 | 0.091 | 3 |
MgTiAsO5 (mvc-5438) | 0.6584 | 0.269 | 4 |
MgAgAsO5 (mvc-5377) | 0.5679 | 0.137 | 4 |
Cr3B7ClO13 (mp-579770) | 0.6604 | 0.000 | 4 |
Fe3B7IO13 (mp-566623) | 0.6613 | 0.138 | 4 |
MgCu(GeO3)2 (mvc-8050) | 0.6277 | 0.066 | 4 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Cu_pv Ge_d O |
Final Energy/Atom-5.8920 eV |
Corrected Energy-63.1336 eV
-63.1336 eV = -58.9199 eV (uncorrected energy) - 4.2137 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)