material

Ba3Zr2S7

ID:

mp-9179

DOI:

10.17188/1313033


Tags: Tribarium dizirconium sulfide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-2.232 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.012 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.14 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Ba3Zr2S7
Band Gap
0.518 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 75241 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CaCO3 (mp-3953) <0 0 1> <1 0 1> 0.011 132.8
C (mp-66) <1 1 1> <1 0 1> 0.011 132.8
GaSe (mp-1943) <0 0 1> <1 0 1> 0.012 265.5
KP(HO2)2 (mp-23959) <1 0 0> <0 0 1> 0.014 228.7
TbScO3 (mp-31119) <1 1 0> <0 0 1> 0.015 127.1
Ge3(BiO3)4 (mp-23560) <1 0 0> <0 0 1> 0.020 228.7
C (mp-66) <1 0 0> <0 0 1> 0.021 25.4
KCl (mp-23193) <1 0 0> <0 0 1> 0.023 203.3
DyScO3 (mp-31120) <1 1 0> <0 0 1> 0.031 127.1
LiF (mp-1138) <1 1 0> <0 0 1> 0.043 355.7
BaTiO3 (mp-5986) <0 0 1> <0 0 1> 0.046 127.1
Te2Mo (mp-602) <1 0 0> <0 0 1> 0.046 330.3
C (mp-66) <1 1 0> <0 0 1> 0.054 127.1
LiF (mp-1138) <1 1 1> <0 0 1> 0.062 203.3
GdScO3 (mp-5690) <1 1 0> <0 0 1> 0.072 127.1
SiO2 (mp-6930) <0 0 1> <1 0 0> 0.074 130.3
Au (mp-81) <1 0 0> <0 0 1> 0.076 228.7
WS2 (mp-224) <1 0 1> <0 0 1> 0.076 228.7
AlN (mp-661) <1 0 0> <0 0 1> 0.089 127.1
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.102 203.3
CaCO3 (mp-3953) <1 0 1> <0 0 1> 0.103 177.9
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.103 203.3
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.109 260.6
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.125 152.5
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.135 330.3
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.137 177.9
SiO2 (mp-6930) <1 0 1> <0 0 1> 0.159 279.5
Ag (mp-124) <1 0 0> <0 0 1> 0.164 228.7
SiC (mp-11714) <0 0 1> <0 0 1> 0.181 330.3
SiC (mp-7631) <0 0 1> <0 0 1> 0.184 330.3
ZnO (mp-2133) <1 1 1> <0 0 1> 0.187 127.1
Mg (mp-153) <1 0 1> <0 0 1> 0.198 279.5
BaTiO3 (mp-5986) <1 1 0> <0 0 1> 0.201 304.9
LiGaO2 (mp-5854) <0 1 1> <0 0 1> 0.204 127.1
PbS (mp-21276) <1 0 0> <0 0 1> 0.210 330.3
BN (mp-984) <0 0 1> <0 0 1> 0.216 177.9
NaCl (mp-22862) <1 0 0> <0 0 1> 0.253 127.1
YVO4 (mp-19133) <1 0 0> <1 1 0> 0.254 184.3
SrTiO3 (mp-4651) <1 1 0> <0 0 1> 0.260 127.1
Te2W (mp-22693) <0 0 1> <0 0 1> 0.267 177.9
Cu (mp-30) <1 1 1> <0 0 1> 0.273 177.9
Cu (mp-30) <1 1 0> <0 0 1> 0.276 127.1
Te2W (mp-22693) <1 1 1> <0 0 1> 0.292 228.7
Te2W (mp-22693) <0 1 0> <0 0 1> 0.308 330.3
YAlO3 (mp-3792) <1 1 0> <0 0 1> 0.315 228.7
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.315 254.1
BaTiO3 (mp-5986) <1 1 1> <0 0 1> 0.317 203.3
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.320 127.1
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.324 76.2
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.334 330.3
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
123 27 32 0 0 0
27 123 32 0 0 0
32 32 108 0 0 0
0 0 0 23 0 0
0 0 0 0 23 0
0 0 0 0 0 26
Compliance Tensor Sij (10-12Pa-1)
9 -1.4 -2.3 0 0 0
-1.4 9 -2.3 0 0 0
-2.3 -2.3 10.6 0 0 0
0 0 0 44.1 0 0
0 0 0 0 44.1 0
0 0 0 0 0 39
Shear Modulus GV
32 GPa
Bulk Modulus KV
60 GPa
Shear Modulus GR
29 GPa
Bulk Modulus KR
60 GPa
Shear Modulus GVRH
30 GPa
Bulk Modulus KVRH
60 GPa
Elastic Anisotropy
0.50
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr3Ru2O7 (mp-5868) 0.1518 0.024 3
K3Mn2F7 (mp-554144) 0.1819 0.370 3
Ca3Mn2O7 (mp-19124) 0.0921 0.059 3
Rb3Mn2Br7 (mp-28002) 0.1571 0.023 3
K3Mn2Cl7 (mp-28076) 0.0698 0.001 3
SrEu2Al2O7 (mp-983228) 0.3779 0.047 4
Ba3SrTa2O9 (mp-7980) 0.5915 0.015 4
SrGd2Al2O7 (mp-545404) 0.6057 1.061 4
K2RbMn2F7 (mp-558227) 0.1689 0.000 4
K2RbMn2F7 (mp-613298) 0.1716 0.000 4
Ba10Mg3ZrTa6O30 (mp-686330) 0.7274 0.112 5
Ba3CaZrWO9 (mp-736122) 0.6630 0.175 5
Ba6Tb3Nb(SnO9)2 (mp-686370) 0.6407 0.083 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Zr_sv S
Final Energy/Atom
-6.1622 eV
Corrected Energy
-78.5906 eV
-78.5906 eV = -73.9464 eV (uncorrected energy) - 4.6442 eV (MP Anion Correction)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 75241
Submitted by
User remarks:
  • Tribarium dizirconium sulfide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)