Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.882 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density7.42 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 200.0 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 221.4 |
AlN (mp-661) | <1 0 0> | <1 0 1> | 327.4 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 204.3 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 255.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 221.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 153.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 221.4 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 128.9 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 51.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 297.8 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 340.6 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 272.5 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 68.1 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 163.7 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 260.5 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 255.4 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 119.2 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 148.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 68.1 |
SiO2 (mp-6930) | <1 0 1> | <1 1 0> | 322.3 |
SiO2 (mp-6930) | <1 1 1> | <1 0 1> | 163.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 257.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 148.9 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 204.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 68.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 255.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 297.8 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 68.1 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 297.8 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 374.6 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 272.5 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 163.7 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 340.6 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 221.4 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 245.6 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 186.1 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 111.7 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 260.5 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 335.0 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 119.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 335.0 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 193.4 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 119.2 |
Te2W (mp-22693) | <0 0 1> | <1 0 1> | 204.7 |
Te2W (mp-22693) | <0 1 0> | <1 1 1> | 266.7 |
Te2W (mp-22693) | <0 1 1> | <1 0 0> | 297.8 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 335.0 |
TePb (mp-19717) | <1 0 0> | <0 0 1> | 357.6 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 221.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
CaCuAs (mp-4120) | 0.0109 | 0.000 | 3 |
SrZnPb (mp-1019280) | 0.0002 | 0.016 | 3 |
YPPt (mp-16304) | 0.0041 | 0.000 | 3 |
UCuGe (mp-11833) | 0.0104 | 0.188 | 3 |
SrAgP (mp-10667) | 0.0001 | 0.000 | 3 |
ThAl2 (mp-669) | 0.0080 | 0.000 | 2 |
TmSi2 (mp-772) | 0.0081 | 0.074 | 2 |
UGa2 (mp-20632) | 0.0036 | 0.246 | 2 |
PuSi2 (mp-10186) | 0.0115 | 0.000 | 2 |
ErSi2 (mp-2145) | 0.0140 | 0.058 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Ni_pv Sb |
Final Energy/Atom-5.8306 eV |
Corrected Energy-35.3677 eV
Uncorrected energy = -34.9837 eV
Composition-based energy adjustment (-0.192 eV/atom x 2.0 atoms) = -0.3840 eV
Corrected energy = -35.3677 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)