material

TlTe3Pt2

ID:

mp-9251

DOI:

10.17188/1313093


Tags: Thallium platinum telluride (2/4/6)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.433 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
9.50 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 78787 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations
Band Structure
Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BN (mp-984) <0 0 1> <0 0 1> 0.002 169.1
Cu (mp-30) <1 0 0> <1 0 0> 0.004 195.6
NaCl (mp-22862) <1 1 1> <0 0 1> 0.011 56.4
C (mp-48) <0 0 1> <0 0 1> 0.013 225.5
LiTaO3 (mp-3666) <1 1 0> <1 1 0> 0.017 254.1
GaN (mp-804) <0 0 1> <0 0 1> 0.019 169.1
TePb (mp-19717) <1 1 1> <0 0 1> 0.021 225.5
SiC (mp-7631) <0 0 1> <0 0 1> 0.023 225.5
SiC (mp-11714) <0 0 1> <0 0 1> 0.026 225.5
LaAlO3 (mp-2920) <1 0 1> <0 0 1> 0.032 225.5
MgO (mp-1265) <1 0 0> <1 0 0> 0.033 146.7
TeO2 (mp-2125) <1 1 0> <1 0 0> 0.033 97.8
InP (mp-20351) <1 1 0> <1 1 0> 0.040 254.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.044 169.1
AlN (mp-661) <0 0 1> <1 0 0> 0.044 342.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.044 169.1
BaTiO3 (mp-5986) <0 0 1> <1 0 1> 0.047 223.9
C (mp-48) <1 0 0> <1 0 0> 0.048 342.3
BaTiO3 (mp-5986) <1 0 0> <0 0 1> 0.051 169.1
BaTiO3 (mp-5986) <1 0 1> <0 0 1> 0.055 281.9
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.055 342.3
SiC (mp-11714) <1 0 1> <1 1 0> 0.058 254.1
ZnO (mp-2133) <0 0 1> <1 0 0> 0.058 244.5
AlN (mp-661) <1 0 0> <0 0 1> 0.063 281.9
LiGaO2 (mp-5854) <0 1 1> <1 0 0> 0.063 342.3
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.064 225.5
CdWO4 (mp-19387) <0 0 1> <1 0 0> 0.067 244.5
NaCl (mp-22862) <1 0 0> <1 0 1> 0.068 223.9
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.069 225.5
PbS (mp-21276) <1 0 0> <1 0 0> 0.072 146.7
CdTe (mp-406) <1 1 1> <0 0 1> 0.074 225.5
GaSe (mp-1943) <0 0 1> <1 0 0> 0.075 244.5
Ni (mp-23) <1 1 1> <1 0 0> 0.075 342.3
GdScO3 (mp-5690) <1 1 0> <1 0 0> 0.076 195.6
YAlO3 (mp-3792) <0 1 1> <0 0 1> 0.078 338.3
TiO2 (mp-2657) <1 0 0> <1 0 1> 0.078 223.9
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.080 56.4
ZnO (mp-2133) <1 0 1> <0 0 1> 0.081 338.3
LiNbO3 (mp-3731) <1 1 0> <1 1 0> 0.084 254.1
BN (mp-984) <1 0 1> <1 0 1> 0.085 223.9
SiC (mp-11714) <1 0 0> <1 0 0> 0.088 244.5
InSb (mp-20012) <1 1 1> <0 0 1> 0.090 225.5
KTaO3 (mp-3614) <1 0 0> <1 0 1> 0.090 223.9
Mg (mp-153) <0 0 1> <0 0 1> 0.092 169.1
C (mp-66) <1 0 0> <1 0 0> 0.097 195.6
PbS (mp-21276) <1 1 0> <1 1 0> 0.107 254.1
GaAs (mp-2534) <1 1 1> <0 0 1> 0.118 56.4
LiF (mp-1138) <1 1 0> <0 0 1> 0.118 281.9
MgF2 (mp-1249) <1 1 0> <1 0 0> 0.129 244.5
Ag (mp-124) <1 1 1> <1 0 0> 0.135 244.5
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
83 24 10 5 0 0
24 83 10 -5 0 0
10 10 15 0 0 0
5 -5 0 9 0 0
0 0 0 0 9 5
0 0 0 0 5 30
Compliance Tensor Sij (10-12Pa-1)
14.8 -4 -7.5 -10.6 0 0
-4 14.8 -7.5 10.6 0 0
-7.5 -7.5 78 0 0 0
-10.6 10.6 0 123.7 0 0
0 0 0 0 123.7 -21.3
0 0 0 0 -21.3 37.4
Shear Modulus GV
19 GPa
Bulk Modulus KV
30 GPa
Shear Modulus GR
11 GPa
Bulk Modulus KR
14 GPa
Shear Modulus GVRH
15 GPa
Bulk Modulus KVRH
22 GPa
Elastic Anisotropy
4.52
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
TlPd2Se3 (mp-7038) 0.4256 0.000 3
CrTe4Au (mp-12743) 0.4926 0.000 3
Ba2CaI6 (mp-753345) 0.5056 0.062 3
AgBiI4 (mp-35909) 0.4597 0.040 3
TlPt2Se3 (mp-541487) 0.3600 0.000 3
LiGaPdF6 (mp-9245) 0.6638 0.007 4
SrLa6OsI12 (mp-567419) 0.6022 0.000 4
LiV2OF5 (mp-765917) 0.6332 0.084 4
NaLa6OsI12 (mp-569905) 0.6351 0.000 4
Na2GeTeO6 (mp-10340) 0.6347 0.000 4
VO2 (mvc-11573) 0.5459 0.151 2
FeO2 (mvc-11541) 0.5404 0.352 2
Nb2C (mp-569989) 0.4537 0.000 2
CrS2 (mvc-15) 0.4303 0.058 2
CoO2 (mp-1062939) 0.5333 0.024 2
Li4ZrNb(TeO6)2 (mp-756177) 0.7120 0.060 5
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Te Pt Tl_d
Final Energy/Atom
-4.4175 eV
Corrected Energy
-53.0100 eV
-53.0100 eV = -53.0100 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 78787
Submitted by
User remarks:
  • Thallium platinum telluride (2/4/6)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)