@article{Zelinska2008, author = "Zelinska, O.Ya. and Tkachuk, A.V. and Grosvenor, A.P. and Mar, A.", title = "Structure and physical properties of Yb Zn2 Sb2 and Yb Cd2 Sb2", journal = "Chemistry of Metals and Alloys", year = "2008", volume = "1", pages = "204-209", ASTM_id = "CMEAL3" } @article{Artmann1996, author = "Artmann, A. and Mewis, A. and Roepke, M. and Michels, G.", title = "A M2 X2-Verbindungen mit Ca Al2 Si2-Struktur. XI: Struktur und Eigenschaften der Verbindungen A Cd2 X2 (A: Eu, Yb; X: P, As Sb)", journal = "Zeitschrift fuer Anorganische und Allgemeine Chemie (1950) (DE)", year = "1996", volume = "622", pages = "679-682", ASTM_id = "ZAACAB" }