material

ZrSnTe

ID:

mp-9289

DOI:

10.17188/1313113


Tags: Zirconium tin telluride (1/1/1)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.821 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
7.54 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P4/nmm [129]
Hall
P 4ab 2ab 1ab
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Topological data for ICSD ID 80190 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CaF2 (mp-2741) <1 0 0> <0 0 1> 0.000 152.0
LiGaO2 (mp-5854) <1 0 1> <0 0 1> 0.005 135.1
GaP (mp-2490) <1 0 0> <0 0 1> 0.006 152.0
InAs (mp-20305) <1 0 0> <0 0 1> 0.023 152.0
LiGaO2 (mp-5854) <1 0 0> <1 0 1> 0.027 319.6
GdScO3 (mp-5690) <0 0 1> <1 1 0> 0.030 255.9
C (mp-66) <1 1 0> <0 0 1> 0.032 253.4
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.033 152.0
NdGaO3 (mp-3196) <1 1 0> <0 0 1> 0.037 304.1
SiC (mp-8062) <1 1 0> <1 0 0> 0.044 108.6
Cu (mp-30) <1 1 1> <1 0 0> 0.048 181.0
Mg (mp-153) <1 1 1> <0 0 1> 0.050 270.3
ZnTe (mp-2176) <1 1 0> <1 0 0> 0.056 108.6
GdScO3 (mp-5690) <1 0 1> <0 0 1> 0.060 168.9
CdSe (mp-2691) <1 1 0> <1 0 0> 0.061 108.6
InAs (mp-20305) <1 1 0> <1 0 0> 0.063 108.6
SiC (mp-8062) <1 0 0> <0 0 1> 0.068 152.0
ZrO2 (mp-2858) <1 0 1> <1 0 0> 0.074 217.2
GaSb (mp-1156) <1 1 0> <1 0 0> 0.079 108.6
YAlO3 (mp-3792) <0 0 1> <1 0 0> 0.082 253.4
YAlO3 (mp-3792) <1 0 0> <0 0 1> 0.084 320.9
GaTe (mp-542812) <1 0 -1> <0 0 1> 0.089 152.0
YVO4 (mp-19133) <1 0 1> <1 0 1> 0.090 279.6
TbScO3 (mp-31119) <1 0 1> <0 0 1> 0.095 168.9
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.099 323.4
Ga2O3 (mp-886) <1 0 -1> <0 0 1> 0.103 152.0
MoSe2 (mp-1634) <1 1 1> <1 1 1> 0.108 269.5
PbSe (mp-2201) <1 1 0> <1 0 0> 0.109 108.6
MgAl2O4 (mp-3536) <1 0 0> <0 0 1> 0.112 67.6
LiAlO2 (mp-3427) <0 0 1> <0 0 1> 0.115 135.1
SiC (mp-7631) <1 0 0> <1 0 0> 0.116 325.8
MoSe2 (mp-1634) <1 1 0> <0 0 1> 0.124 270.3
LiF (mp-1138) <1 0 0> <0 0 1> 0.130 16.9
Fe2O3 (mp-24972) <0 0 1> <1 0 0> 0.137 181.0
LiAlO2 (mp-3427) <1 0 1> <1 0 0> 0.142 217.2
GaTe (mp-542812) <1 0 0> <0 0 1> 0.150 135.1
NdGaO3 (mp-3196) <0 1 1> <1 0 1> 0.158 159.8
TiO2 (mp-2657) <1 0 0> <1 0 0> 0.158 181.0
TbScO3 (mp-31119) <0 0 1> <1 1 0> 0.167 255.9
LiAlO2 (mp-3427) <1 1 1> <0 0 1> 0.170 219.6
DyScO3 (mp-31120) <0 1 1> <1 0 1> 0.176 159.8
DyScO3 (mp-31120) <1 0 1> <0 0 1> 0.177 168.9
Ga2O3 (mp-886) <1 0 1> <1 0 0> 0.179 325.8
SiC (mp-11714) <1 0 0> <0 0 1> 0.182 253.4
Ag (mp-124) <1 1 0> <1 0 0> 0.189 72.4
SiO2 (mp-6930) <1 1 0> <1 0 0> 0.190 144.8
BN (mp-984) <1 0 0> <1 1 1> 0.191 215.6
GaTe (mp-542812) <0 0 1> <0 0 1> 0.191 152.0
CdSe (mp-2691) <1 0 0> <0 0 1> 0.191 152.0
BN (mp-984) <1 1 1> <1 0 1> 0.193 239.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
140 63 42 0 0 0
63 140 42 0 0 0
42 42 163 0 0 0
0 0 0 51 0 0
0 0 0 0 51 0
0 0 0 0 0 76
Compliance Tensor Sij (10-12Pa-1)
9.3 -3.8 -1.4 0 0 0
-3.8 9.3 -1.4 0 0 0
-1.4 -1.4 6.9 0 0 0
0 0 0 19.6 0 0
0 0 0 0 19.6 0
0 0 0 0 0 13.2
Shear Modulus GV
55 GPa
Bulk Modulus KV
82 GPa
Shear Modulus GR
53 GPa
Bulk Modulus KR
82 GPa
Shear Modulus GVRH
54 GPa
Bulk Modulus KVRH
82 GPa
Elastic Anisotropy
0.25
Poisson's Ratio
0.23

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ti2CuSb3 (mp-505804) 0.1311 0.057 3
Hf2CuSb3 (mp-19928) 0.1636 0.032 3
Hf2Sb3Pd (mp-1070907) 0.1352 0.038 3
Zr2Sb3Pd (mp-1071230) 0.1867 0.033 3
Zr2CuSb3 (mp-16421) 0.1820 0.049 3
LuSe2 (mp-1018793) 0.3965 0.002 2
LuS2 (mp-1018792) 0.3929 0.022 2
HfSb2 (mp-1018717) 0.1742 0.059 2
ErS2 (mp-1018687) 0.3942 0.053 2
TmS2 (mp-1071948) 0.3942 0.048 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Sn_d Te
Final Energy/Atom
-5.9138 eV
Corrected Energy
-36.3271 eV
Uncorrected energy = -35.4831 eV Composition-based energy adjustment (-0.422 eV/atom x 2.0 atoms) = -0.8440 eV Corrected energy = -36.3271 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 80190
Submitted by
User remarks:
  • Zirconium tin telluride (1/1/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)