material

ZrCo2

ID:

mp-929

DOI:

10.17188/1313114


Tags: Zirconium cobalt hydride (1/2/0.17) Cobalt zirconium (2/1) Zirconium cobalt (1/2)

Material Details

Final Magnetic Moment
0.021 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.311 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
8.42 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Fd3m [227]
Hall
F 4d 2 3 1d
Point Group
m3m
Crystal System
cubic

Electronic Structure

Topological data for ICSD ID 96317 from Topological Materials Database
Topological Classification
SM*
Subclassification
ES
Crossing Type
Line
* Semimetal
Enforced Semimetal with Line or Plane degeneracy

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 0 0> <1 0 0> 0.000 190.9
ZnTe (mp-2176) <1 0 0> <1 0 0> 0.002 190.9
CeO2 (mp-20194) <1 0 0> <1 0 0> 0.003 238.7
Si (mp-149) <1 0 0> <1 0 0> 0.005 238.7
Ag (mp-124) <1 1 0> <1 1 0> 0.006 270.0
SiC (mp-8062) <1 0 0> <1 0 0> 0.017 95.5
Cu (mp-30) <1 1 0> <1 1 0> 0.017 202.5
PbS (mp-21276) <1 1 0> <1 1 0> 0.036 202.5
PbS (mp-21276) <1 1 1> <1 1 1> 0.036 248.0
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.050 190.9
InP (mp-20351) <1 1 0> <1 1 0> 0.064 202.5
InP (mp-20351) <1 1 1> <1 1 1> 0.064 248.0
CdSe (mp-2691) <1 0 0> <1 0 0> 0.094 190.9
ZnO (mp-2133) <1 1 0> <1 1 0> 0.099 270.0
CdS (mp-672) <0 0 1> <1 1 1> 0.108 248.0
C (mp-48) <0 0 1> <1 0 0> 0.115 334.1
MgO (mp-1265) <1 1 0> <1 1 0> 0.120 202.5
GaSb (mp-1156) <1 0 0> <1 0 0> 0.132 190.9
MgO (mp-1265) <1 0 0> <1 0 0> 0.139 238.7
Cu (mp-30) <1 0 0> <1 0 0> 0.149 238.7
TiO2 (mp-390) <0 0 1> <1 0 0> 0.150 190.9
DyScO3 (mp-31120) <0 1 1> <1 1 0> 0.155 270.0
Mg (mp-153) <1 1 1> <1 0 0> 0.165 238.7
PbSe (mp-2201) <1 0 0> <1 0 0> 0.189 190.9
CdS (mp-672) <1 1 0> <1 1 0> 0.192 202.5
CdS (mp-672) <1 0 0> <1 0 0> 0.199 143.2
MgF2 (mp-1249) <1 0 0> <1 0 0> 0.210 143.2
AlN (mp-661) <0 0 1> <1 0 0> 0.212 334.1
GaP (mp-2490) <1 0 0> <1 0 0> 0.213 238.7
Fe3O4 (mp-19306) <1 1 0> <1 1 0> 0.236 202.5
ZrO2 (mp-2858) <1 0 -1> <1 0 0> 0.249 143.2
NaCl (mp-22862) <1 1 0> <1 1 0> 0.264 135.0
C (mp-66) <1 1 0> <1 1 0> 0.278 202.5
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.317 238.7
TiO2 (mp-2657) <0 0 1> <1 0 0> 0.321 190.9
DyScO3 (mp-31120) <1 0 1> <1 1 1> 0.348 165.4
BN (mp-984) <0 0 1> <1 0 0> 0.360 334.1
KTaO3 (mp-3614) <1 1 0> <1 1 0> 0.365 67.5
KTaO3 (mp-3614) <1 1 1> <1 1 1> 0.367 82.7
Ni (mp-23) <1 1 1> <1 0 0> 0.383 334.1
Ni (mp-23) <1 1 0> <1 0 0> 0.383 238.7
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.390 135.0
GaAs (mp-2534) <1 1 1> <1 0 0> 0.438 286.4
ZnSe (mp-1190) <1 1 1> <1 0 0> 0.439 286.4
SrTiO3 (mp-4651) <1 0 1> <1 1 1> 0.440 165.4
GdScO3 (mp-5690) <0 1 1> <1 1 1> 0.448 165.4
TbScO3 (mp-31119) <1 0 1> <1 1 1> 0.454 165.4
Ge (mp-32) <1 1 1> <1 0 0> 0.462 286.4
WS2 (mp-224) <0 0 1> <1 0 0> 0.516 238.7
MoS2 (mp-1434) <0 0 1> <1 0 0> 0.516 238.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
256 118 118 0 0 0
118 256 118 0 0 0
118 118 256 0 0 0
0 0 0 81 0 0
0 0 0 0 81 0
0 0 0 0 0 81
Compliance Tensor Sij (10-12Pa-1)
5.5 -1.7 -1.7 0 0 0
-1.7 5.5 -1.7 0 0 0
-1.7 -1.7 5.5 0 0 0
0 0 0 12.3 0 0
0 0 0 0 12.3 0
0 0 0 0 0 12.3
Shear Modulus GV
76 GPa
Bulk Modulus KV
164 GPa
Shear Modulus GR
76 GPa
Bulk Modulus KR
164 GPa
Shear Modulus GVRH
76 GPa
Bulk Modulus KVRH
164 GPa
Elastic Anisotropy
0.03
Poisson's Ratio
0.30

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
YbNi4Au (mp-1024977) 0.0000 0.040 3
TmInCu4 (mp-1024957) 0.0028 0.000 3
GdNi4Au (mp-1077131) 0.0027 0.855 3
YbCu4Au (mp-1077165) 0.0028 0.000 3
GdInCu4 (mp-1077293) 0.0009 0.000 3
DyNi2 (mp-421) 0.0000 0.000 2
YZn2 (mp-1072382) 0.0000 0.022 2
Cr2Ni (mp-1077252) 0.0000 0.279 2
YCu2 (mp-1077241) 0.0000 0.106 2
NaAs2 (mp-1077399) 0.0000 0.227 2
Co (mp-1072089) 0.0000 0.199 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zr_sv Co
Final Energy/Atom
-7.8995 eV
Corrected Energy
-47.3970 eV
Uncorrected energy = -47.3970 eV Corrected energy = -47.3970 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 625679
  • 625689
  • 189945
  • 625668
  • 625709
  • 656651
  • 625696
  • 625693
  • 604257
  • 625691
  • 625692
  • 625694
  • 603796
  • 625697
  • 102743
  • 603222
  • 625678
  • 625705
  • 102742
  • 625700
  • 96317
Submitted by
User remarks:
  • Cobalt zirconium (2/1)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)