material

Sr3MnN3

ID:

mp-9325

DOI:

10.17188/1313136


Tags: High pressure experimental phase Strontium trinitridomanganate(III)

Material Details

Final Magnetic Moment
0.004 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
Non-magnetic
Formation Energy / Atom
-0.904 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.38 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/m [176]
Hall
-P 6c
Point Group
6/m
Crystal System
hexagonal

Band Structure

Density of States
Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

sign indicates spin ↑ ↓

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Si (mp-149) <1 1 1> <0 0 1> 0.000 51.8
CeO2 (mp-20194) <1 1 1> <0 0 1> 0.000 51.8
C (mp-66) <1 1 1> <0 0 1> 0.003 155.4
CdS (mp-672) <1 0 1> <1 0 0> 0.003 163.0
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.005 155.4
SiO2 (mp-6930) <1 1 1> <1 0 1> 0.015 263.6
Bi2Te3 (mp-34202) <0 0 1> <0 0 1> 0.015 51.8
C (mp-48) <0 0 1> <0 0 1> 0.018 207.2
Te2W (mp-22693) <0 1 0> <1 0 0> 0.020 163.0
SiC (mp-11714) <1 0 1> <1 0 0> 0.024 163.0
BaF2 (mp-1029) <1 1 1> <0 0 1> 0.031 207.2
GaN (mp-804) <1 1 0> <1 0 0> 0.035 203.7
NdGaO3 (mp-3196) <1 1 0> <1 0 0> 0.050 122.2
Ag (mp-124) <1 1 1> <0 0 1> 0.053 207.2
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.053 155.4
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.053 155.4
MgF2 (mp-1249) <1 0 0> <1 0 1> 0.056 131.8
AlN (mp-661) <1 1 1> <1 1 0> 0.056 141.2
SiC (mp-11714) <0 0 1> <0 0 1> 0.059 155.4
GaP (mp-2490) <1 1 1> <0 0 1> 0.060 51.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.064 155.4
GaSe (mp-1943) <0 0 1> <1 0 0> 0.067 203.7
YAlO3 (mp-3792) <1 1 0> <1 1 0> 0.080 282.3
ZnO (mp-2133) <1 0 1> <0 0 1> 0.081 259.0
NdGaO3 (mp-3196) <1 0 0> <1 0 1> 0.084 131.8
BN (mp-984) <0 0 1> <1 0 0> 0.087 285.2
AlN (mp-661) <1 0 1> <1 0 1> 0.088 263.6
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.090 155.4
Ni (mp-23) <1 0 0> <1 0 0> 0.091 122.2
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.092 81.5
Ga2O3 (mp-886) <1 0 0> <1 0 1> 0.094 329.5
CaF2 (mp-2741) <1 1 1> <0 0 1> 0.095 51.8
TiO2 (mp-390) <1 0 1> <1 1 0> 0.100 282.3
Au (mp-81) <1 1 1> <0 0 1> 0.104 207.2
CaF2 (mp-2741) <1 0 0> <1 0 0> 0.104 122.2
Te2Mo (mp-602) <1 0 0> <1 0 0> 0.108 163.0
Te2Mo (mp-602) <0 0 1> <1 0 0> 0.112 163.0
CsI (mp-614603) <1 0 0> <1 0 0> 0.112 122.2
MoSe2 (mp-1634) <1 1 0> <1 0 1> 0.122 263.6
ZrO2 (mp-2858) <1 0 1> <1 1 0> 0.129 211.7
LiGaO2 (mp-5854) <0 1 0> <1 1 1> 0.129 262.6
GaP (mp-2490) <1 0 0> <1 0 0> 0.130 122.2
Cu (mp-30) <1 1 1> <0 0 1> 0.131 155.4
LiTaO3 (mp-3666) <0 0 1> <0 0 1> 0.131 207.2
ZnO (mp-2133) <1 1 0> <1 0 0> 0.132 122.2
ZnO (mp-2133) <1 0 0> <1 1 0> 0.134 70.6
SrTiO3 (mp-4651) <0 0 1> <1 0 0> 0.145 122.2
CdWO4 (mp-19387) <0 1 1> <1 0 1> 0.149 329.5
AlN (mp-661) <1 0 0> <1 0 0> 0.156 285.2
SiC (mp-8062) <1 0 0> <1 1 1> 0.161 175.1
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
83 20 41 0 -0 -0
20 83 41 -0 0 -0
41 41 121 0 -0 -0
0 -0 0 33 -0 0
0 -0 -0 -0 33 -0
-0 -0 -0 -0 0 31
Compliance Tensor Sij (10-12Pa-1)
14.6 -1.3 -4.5 0 0 0
-1.3 14.6 -4.5 0 0 0
-4.5 -4.5 11.3 0 0 0
0 0 0 29.9 0 0
0 0 0 0 29.9 0
0 0 0 0 0 31.8
Shear Modulus GV
32 GPa
Bulk Modulus KV
55 GPa
Shear Modulus GR
31 GPa
Bulk Modulus KR
50 GPa
Shear Modulus GVRH
32 GPa
Bulk Modulus KVRH
53 GPa
Elastic Anisotropy
0.19
Poisson's Ratio
0.25

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
RbMgBO3 (mp-1020633) 0.6617 0.000 4
Li4V(BO3)2 (mp-778789) 0.7299 0.033 4
Li4Fe(BO3)2 (mp-769681) 0.7263 0.021 4
Li4Mn(BO3)2 (mp-769946) 0.7284 0.011 4
NaMnBO3 (mp-776039) 0.7196 0.024 4
Ba3MnN3 (mp-9324) 0.2339 0.000 3
Ba3FeN3 (mp-8306) 0.2280 0.000 3
Sr3GaN3 (mp-7191) 0.3368 0.000 3
Sr3CrN3 (mp-12906) 0.1673 0.000 3
Sr3FeN3 (mp-706272) 0.1148 0.000 3
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: N Mn_pv Sr_sv
Final Energy/Atom
-6.3429 eV
Corrected Energy
-88.8006 eV
-88.8006 eV = -88.8006 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 80772
Submitted by
User remarks:
  • High pressure experimental phase
  • Strontium trinitridomanganate(III)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)