Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.285 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.285 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density3.51 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToN2 + C |
Band Gap3.809 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP31c [159] |
HallP 3 2c |
Point Group3m |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 0 0> | 185.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 0 0> | 123.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 110.1 |
AlN (mp-661) | <1 0 0> | <1 1 1> | 324.5 |
AlN (mp-661) | <1 0 1> | <1 1 1> | 194.7 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 335.9 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 278.0 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 123.6 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 146.9 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 257.0 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 183.6 |
BaF2 (mp-1029) | <1 0 0> | <1 1 1> | 324.5 |
BaF2 (mp-1029) | <1 1 0> | <1 0 1> | 335.9 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 144.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 185.4 |
GaN (mp-804) | <1 0 1> | <1 0 0> | 154.5 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 239.9 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 146.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 335.9 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 278.0 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 194.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 123.6 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 287.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 183.6 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 183.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 324.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 144.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 257.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 247.2 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 110.1 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 259.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 183.6 |
Te2W (mp-22693) | <1 0 0> | <0 0 1> | 293.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 92.7 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 144.0 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 214.0 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 257.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 1> | 239.9 |
GaSe (mp-1943) | <1 0 0> | <1 0 0> | 278.0 |
BN (mp-984) | <1 1 1> | <1 0 0> | 278.0 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 216.3 |
MoS2 (mp-1434) | <1 0 0> | <1 0 0> | 278.0 |
MoS2 (mp-1434) | <1 0 1> | <1 0 0> | 278.0 |
InAs (mp-20305) | <1 1 0> | <1 1 1> | 324.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 257.0 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 183.6 |
KTaO3 (mp-3614) | <1 1 0> | <0 0 1> | 183.6 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 110.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 247.2 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 110.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
Piezoelectric Tensor eij (C/m2) |
|||||
---|---|---|---|---|---|
0.21466 | -0.21466 | 0.00000 | 0.00000 | 0.02744 | 0.00000 |
0.00000 | 0.00000 | 0.00000 | 0.02744 | 0.00000 | -0.21466 |
0.06549 | 0.06549 | -0.15345 | 0.00000 | 0.00000 | 0.00000 |
Piezoelectric Modulus ‖eij‖max0.30481 C/m2 |
Crystallographic Direction vmax |
---|
-1.00000 |
0.00000 |
0.00000 |
Dielectric Tensor εij∞ (electronic contribution) |
||
---|---|---|
5.09 | 0.00 | 0.00 |
0.00 | 5.09 | 0.00 |
0.00 | 0.00 | 5.11 |
Dielectric Tensor εij (total) |
||
---|---|---|
7.24 | 0.00 | -0.00 |
0.00 | 7.24 | -0.00 |
-0.00 | -0.00 | 7.28 |
Polycrystalline dielectric constant
εpoly∞
5.10
|
Polycrystalline dielectric constant
εpoly
7.26
|
Refractive Index n2.26 |
Potentially ferroelectric?Unknown |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Ga3NO3 (mp-778698) | 0.3847 | 0.060 | 3 |
Be2GeO4 (mp-768285) | 0.3715 | 0.000 | 3 |
Ga3NO3 (mp-778065) | 0.3410 | 0.052 | 3 |
Be2SiO4 (mp-3347) | 0.3842 | 0.000 | 3 |
Be(PN2)2 (mp-1019545) | 0.3551 | 0.000 | 3 |
LiGaGeO4 (mp-8702) | 0.4161 | 0.000 | 4 |
LiCoGeO4 (mp-763507) | 0.4261 | 0.199 | 4 |
LiAlVO4 (mp-770509) | 0.4355 | 0.061 | 4 |
LiAlVO4 (mp-770365) | 0.4441 | 0.066 | 4 |
LiAlGeO4 (mp-16947) | 0.4053 | 0.015 | 4 |
Ge3N4 (mp-672289) | 0.2168 | 0.000 | 2 |
Cr3N4 (mp-1014369) | 0.1351 | 0.164 | 2 |
Si3N4 (mp-2245) | 0.2075 | 0.000 | 2 |
C3N4 (mp-1985) | 0.3682 | 0.322 | 2 |
Ti3N4 (mp-1080190) | 0.2265 | 0.118 | 2 |
YAl6Si18(N15O)2 (mp-677127) | 0.5986 | 0.092 | 5 |
NdAl6Si30(N15O)3 (mp-532626) | 0.5800 | 0.067 | 5 |
Li4Al3Ge3IO12 (mp-557456) | 0.7040 | 0.000 | 5 |
YAl6Si30(N15O)3 (mp-686618) | 0.5877 | 0.066 | 5 |
YAl6Si30(N15O)3 (mp-677140) | 0.5665 | 0.084 | 5 |
C (mp-1008374) | 0.5174 | 0.437 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: C N |
Final Energy/Atom-8.2139 eV |
Corrected Energy-229.9893 eV
-229.9893 eV = -229.9893 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)