Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingAFM |
Formation Energy / Atom-1.853 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.278 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density2.91 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToMn2H2SO6 + Li2SO4 |
Band Gap3.322 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP21/c [14] |
Hall-P 2ybc |
Point Group2/m |
Crystal Systemmonoclinic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 1 0> | <1 0 -1> | 341.6 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 214.7 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 300.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 343.5 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 171.7 |
AlN (mp-661) | <1 0 1> | <1 0 -1> | 227.7 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 42.9 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 214.6 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 128.8 |
GaAs (mp-2534) | <1 1 0> | <1 0 0> | 223.2 |
BaF2 (mp-1029) | <1 1 0> | <0 0 1> | 171.7 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 214.7 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 343.5 |
GaN (mp-804) | <1 1 0> | <1 0 -1> | 56.9 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 223.2 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 55.8 |
SiO2 (mp-6930) | <1 1 0> | <1 0 1> | 245.0 |
SiO2 (mp-6930) | <1 1 1> | <0 1 1> | 166.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 128.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 223.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 0> | 55.8 |
SiO2 (mp-6930) | <1 0 1> | <0 1 1> | 250.3 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 171.7 |
DyScO3 (mp-31120) | <1 0 0> | <1 0 0> | 223.2 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 163.4 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 343.5 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 343.5 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 128.8 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 128.8 |
ZnSe (mp-1190) | <1 1 0> | <1 0 0> | 223.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 111.6 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 55.8 |
LiF (mp-1138) | <1 1 0> | <1 0 0> | 279.0 |
CdS (mp-672) | <0 0 1> | <1 0 1> | 245.0 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 343.5 |
CdS (mp-672) | <1 1 0> | <0 1 1> | 250.3 |
Te2Mo (mp-602) | <0 0 1> | <1 1 0> | 272.2 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 334.8 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 334.8 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 167.4 |
GaSe (mp-1943) | <0 0 1> | <0 1 0> | 214.6 |
GaSe (mp-1943) | <1 0 1> | <1 0 0> | 279.0 |
BN (mp-984) | <0 0 1> | <0 1 1> | 250.3 |
BN (mp-984) | <1 0 0> | <0 0 1> | 171.7 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 300.5 |
BN (mp-984) | <1 1 1> | <1 1 0> | 272.2 |
LiNbO3 (mp-3731) | <0 0 1> | <1 0 -1> | 284.7 |
LiNbO3 (mp-3731) | <1 0 0> | <1 0 -1> | 284.7 |
BN (mp-984) | <1 0 1> | <1 1 -1> | 182.8 |
BN (mp-984) | <1 1 0> | <0 1 1> | 166.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnSO4 (mp-5126) | 0.5626 | 0.000 | 3 |
CdSeO4 (mp-779156) | 0.5719 | 0.001 | 3 |
CuSO4 (mp-20525) | 0.5522 | 0.000 | 3 |
ReHg2O5 (mp-667291) | 0.5770 | 0.000 | 3 |
CoSO4 (mp-554360) | 0.5696 | 0.000 | 3 |
Al2Si2H4O9 (mp-721216) | 0.5443 | 0.013 | 4 |
Al2Si2H4O9 (mp-541152) | 0.5304 | 0.013 | 4 |
Fe4P3(HO5)3 (mp-25756) | 0.5496 | 0.000 | 4 |
UCu2(PO5)2 (mp-558650) | 0.5547 | 0.000 | 4 |
MgAg2P2O9 (mvc-9823) | 0.5625 | 0.109 | 4 |
LiCoHSO5 (mp-942704) | 0.1934 | 0.088 | 5 |
LiV3P2(HO3)4 (mp-763813) | 0.4972 | 0.017 | 5 |
BeAlSiHO5 (mp-759686) | 0.5155 | 0.007 | 5 |
LiFeHSO5 (mp-943462) | 0.1192 | 0.164 | 5 |
ZnCoPHO5 (mp-603567) | 0.4754 | 0.000 | 5 |
LiMnVP2(HO5)2 (mp-765066) | 0.7047 | 0.143 | 6 |
LiVCrP2(HO5)2 (mp-765311) | 0.7039 | 0.013 | 6 |
Na3Zn4P4H4NO16 (mp-772852) | 0.6194 | 0.005 | 6 |
CuP2H8CN2O5 (mp-24145) | 0.7071 | 0.288 | 6 |
FePH4NO4F (mp-745119) | 0.7079 | 0.165 | 6 |
Run TypeGGA+U |
Energy Cutoff520 eV |
# of K-pointsNone |
U ValuesMn: 3.9 eV |
PseudopotentialsVASP PAW: Li_sv Mn_pv H S O |
Final Energy/Atom-6.0009 eV |
Corrected Energy-239.4565 eV
-239.4565 eV = -216.0334 eV (uncorrected energy) - 16.6996 eV (MP Anion Correction) - 6.7234 eV (MP Advanced Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)