Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.774 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.67 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinI4/mmm [139] |
Hall-I 4 2 |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | elastic energy [meV] | MCIA† [Å2] |
---|---|---|---|---|
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 0.002 | 234.9 |
C (mp-66) | <1 1 0> | <1 1 0> | 0.007 | 199.3 |
SrTiO3 (mp-4651) | <1 1 0> | <0 0 1> | 0.008 | 62.3 |
PbSe (mp-2201) | <1 0 0> | <0 0 1> | 0.010 | 77.9 |
SrTiO3 (mp-4651) | <0 0 1> | <0 0 1> | 0.013 | 31.2 |
SrTiO3 (mp-4651) | <1 0 0> | <1 1 0> | 0.018 | 132.9 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 0.024 | 171.4 |
GaSb (mp-1156) | <1 0 0> | <0 0 1> | 0.025 | 77.9 |
Au (mp-81) | <1 0 0> | <0 0 1> | 0.027 | 140.2 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 0.027 | 233.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 0.028 | 199.3 |
CsI (mp-614603) | <1 0 0> | <0 0 1> | 0.040 | 62.3 |
CdSe (mp-2691) | <1 0 0> | <0 0 1> | 0.041 | 77.9 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 0.059 | 280.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 0.069 | 202.6 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 0.070 | 171.4 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 0.071 | 171.4 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 0.071 | 132.9 |
InP (mp-20351) | <1 0 0> | <0 0 1> | 0.072 | 140.2 |
Au (mp-81) | <1 1 0> | <1 1 0> | 0.075 | 199.3 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 1> | 0.075 | 273.0 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <0 0 1> | 0.077 | 155.8 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 0.077 | 140.2 |
MgF2 (mp-1249) | <1 0 1> | <1 1 0> | 0.080 | 132.9 |
Ni (mp-23) | <1 0 0> | <0 0 1> | 0.080 | 62.3 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 0.089 | 77.9 |
CdWO4 (mp-19387) | <0 0 1> | <1 1 0> | 0.090 | 332.2 |
CsI (mp-614603) | <1 1 0> | <1 1 0> | 0.095 | 265.8 |
MgF2 (mp-1249) | <1 0 0> | <0 0 1> | 0.096 | 187.0 |
CdWO4 (mp-19387) | <0 1 0> | <1 1 0> | 0.096 | 132.9 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 0.108 | 346.5 |
SiC (mp-8062) | <1 0 0> | <0 0 1> | 0.114 | 77.9 |
NdGaO3 (mp-3196) | <1 0 0> | <1 1 0> | 0.118 | 132.9 |
SrTiO3 (mp-4651) | <1 0 1> | <1 1 0> | 0.122 | 265.8 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 0.142 | 280.5 |
ZnO (mp-2133) | <1 0 1> | <1 1 0> | 0.142 | 199.3 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 0.146 | 199.3 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 0.147 | 62.3 |
ZrO2 (mp-2858) | <0 0 1> | <0 0 1> | 0.150 | 140.2 |
Mg (mp-153) | <1 1 1> | <1 1 1> | 0.151 | 273.0 |
ZnTe (mp-2176) | <1 0 0> | <0 0 1> | 0.160 | 77.9 |
TbScO3 (mp-31119) | <0 1 0> | <1 1 0> | 0.170 | 132.9 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 1> | 0.171 | 273.0 |
Mg (mp-153) | <1 0 1> | <1 0 1> | 0.171 | 148.5 |
BN (mp-984) | <1 1 1> | <0 0 1> | 0.174 | 311.6 |
NdGaO3 (mp-3196) | <1 1 0> | <0 0 1> | 0.179 | 62.3 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 0.179 | 77.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 0.185 | 249.3 |
NdGaO3 (mp-3196) | <0 0 1> | <0 0 1> | 0.186 | 31.2 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 0.187 | 171.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
154 | 16 | 58 | 0 | 0 | 0 |
16 | 154 | 58 | 0 | 0 | 0 |
58 | 58 | 102 | 0 | 0 | 0 |
0 | 0 | 0 | 42 | 0 | 0 |
0 | 0 | 0 | 0 | 42 | 0 |
0 | 0 | 0 | 0 | 0 | 24 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
8.5 | 1.2 | -5.5 | 0 | 0 | 0 |
1.2 | 8.5 | -5.5 | 0 | 0 | 0 |
-5.5 | -5.5 | 16.2 | 0 | 0 | 0 |
0 | 0 | 0 | 24 | 0 | 0 |
0 | 0 | 0 | 0 | 24 | 0 |
0 | 0 | 0 | 0 | 0 | 41 |
Shear Modulus GV40 GPa |
Bulk Modulus KV75 GPa |
Shear Modulus GR34 GPa |
Bulk Modulus KR75 GPa |
Shear Modulus GVRH37 GPa |
Bulk Modulus KVRH75 GPa |
Elastic Anisotropy0.86 |
Poisson's Ratio0.29 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Y2TeO2 (mp-755756) | 0.1975 | 0.000 | 3 |
Ba(PRu)2 (mp-4484) | 0.0535 | 0.000 | 3 |
Ba(CoGe)2 (mp-1070253) | 0.1976 | 0.000 | 3 |
Ba(POs)2 (mp-12056) | 0.0860 | 0.000 | 3 |
Sr(FeP)2 (mp-3299) | 0.1391 | 0.000 | 3 |
KLiZnS2 (mp-774907) | 0.4752 | 0.000 | 4 |
SrBiClO2 (mp-547244) | 0.4016 | 0.000 | 4 |
SrBiBrO2 (mp-552234) | 0.4032 | 0.000 | 4 |
KLiMnS2 (mp-753940) | 0.4309 | 0.000 | 4 |
BiPbClO2 (mp-23084) | 0.3267 | 0.000 | 4 |
Bi3O2 (mp-1022722) | 0.6993 | 0.125 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Ni_pv P |
Final Energy/Atom-5.6347 eV |
Corrected Energy-28.1736 eV
Uncorrected energy = -28.1736 eV
Corrected energy = -28.1736 eV
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)