material

Li6PS5I

ID:

mp-950995

DOI:

10.17188/1313292


Material Details

Final Magnetic Moment
0.003 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-1.291 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.006 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
2.22 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Li3PS4 + Li2S + LiI
Band Gap
2.274 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Cc [9]
Hall
C 2yc
Point Group
m
Crystal System
monoclinic

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Mg (mp-153) <0 0 1> <0 0 1> 0.000 184.2
InP (mp-20351) <1 1 1> <0 0 1> 0.000 184.2
SiC (mp-8062) <1 1 0> <1 0 0> 0.000 271.2
CdS (mp-672) <0 0 1> <0 0 1> 0.000 92.1
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.001 184.2
CdS (mp-672) <1 1 0> <1 0 1> 0.005 149.0
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.006 184.2
WS2 (mp-224) <0 0 1> <0 0 1> 0.006 184.2
KTaO3 (mp-3614) <1 0 0> <1 0 -1> 0.009 210.7
Al (mp-134) <1 0 0> <1 0 -1> 0.017 210.7
Cu (mp-30) <1 0 0> <1 0 -1> 0.018 105.3
Ni (mp-23) <1 0 0> <1 0 -1> 0.018 210.7
YVO4 (mp-19133) <0 0 1> <1 0 -1> 0.021 105.3
YVO4 (mp-19133) <1 0 1> <1 0 -1> 0.022 210.7
GaN (mp-804) <1 0 0> <1 0 0> 0.024 271.2
CdS (mp-672) <1 1 1> <1 0 -1> 0.025 105.3
AlN (mp-661) <0 0 1> <1 0 0> 0.032 271.2
Au (mp-81) <1 1 0> <0 1 0> 0.034 147.6
Cu (mp-30) <1 1 0> <0 1 0> 0.035 147.6
BaTiO3 (mp-5986) <0 0 1> <1 0 -1> 0.036 210.7
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.037 276.2
Ag (mp-124) <1 1 0> <0 1 0> 0.038 147.6
LaF3 (mp-905) <0 0 1> <1 0 0> 0.039 90.4
Ga2O3 (mp-886) <1 0 -1> <1 0 0> 0.047 271.2
Bi2Se3 (mp-541837) <0 0 1> <1 0 0> 0.050 90.4
LiAlO2 (mp-3427) <0 0 1> <1 0 0> 0.054 271.2
GaN (mp-804) <1 0 1> <1 0 0> 0.055 271.2
PbS (mp-21276) <1 1 1> <0 0 1> 0.059 184.2
ZnO (mp-2133) <1 0 1> <0 0 1> 0.072 276.2
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.101 271.2
SiC (mp-8062) <1 1 1> <1 0 0> 0.111 271.2
TePb (mp-19717) <1 0 0> <1 0 -1> 0.117 210.7
CdS (mp-672) <1 0 0> <1 1 0> 0.127 173.1
LaF3 (mp-905) <1 1 0> <1 0 0> 0.134 90.4
CdWO4 (mp-19387) <0 1 0> <1 0 0> 0.135 271.2
LaF3 (mp-905) <1 0 0> <1 0 -1> 0.139 105.3
YAlO3 (mp-3792) <0 1 0> <1 0 0> 0.146 271.2
TeO2 (mp-2125) <0 1 0> <1 0 0> 0.150 271.2
LaF3 (mp-905) <1 0 1> <0 0 1> 0.150 276.2
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.156 276.2
LiAlO2 (mp-3427) <1 1 1> <1 0 -1> 0.171 105.3
KCl (mp-23193) <1 0 0> <1 0 -1> 0.183 210.7
YVO4 (mp-19133) <1 0 0> <1 0 0> 0.184 90.4
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.193 271.2
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.195 180.8
Al2O3 (mp-1143) <1 0 1> <1 0 0> 0.213 271.2
YAlO3 (mp-3792) <1 1 0> <1 0 0> 0.214 271.2
LiAlO2 (mp-3427) <1 1 0> <1 0 0> 0.245 90.4
YAlO3 (mp-3792) <1 0 0> <1 0 0> 0.268 271.2
MoS2 (mp-1434) <1 0 0> <1 0 0> 0.280 271.2
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
47 18 18 0 -0 0
18 46 16 0 -1 0
18 16 43 0 1 0
0 0 0 14 0 -0
-0 -1 1 0 13 0
0 0 0 -0 0 12
Compliance Tensor Sij (10-12Pa-1)
27.8 -8 -8.4 0 0.7 0
-8 27.4 -6.9 0 1.4 0
-8.4 -6.9 29.2 0 -1.9 0
0 0 0 71.1 0 2.5
0.7 1.4 -1.9 0 76.5 0
0 0 0 2.5 0 81.9
Shear Modulus GV
13 GPa
Bulk Modulus KV
27 GPa
Shear Modulus GR
13 GPa
Bulk Modulus KR
27 GPa
Shear Modulus GVRH
13 GPa
Bulk Modulus KVRH
27 GPa
Elastic Anisotropy
0.03
Poisson's Ratio
0.28

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Co3(PO4)2 (mp-651271) 0.5409 0.016 3
Li3Fe5O9 (mp-770655) 0.5235 0.107 3
Li2FeF4 (mp-777588) 0.5738 0.103 3
Ni4P2O9 (mp-771899) 0.5611 0.037 3
Li14Fe4O13 (mp-781016) 0.5725 0.097 3
LiVNiO4 (mp-780215) 0.4801 0.008 4
LiVFeO4 (mp-775342) 0.4787 0.010 4
Cu6PS5Br (mp-554627) 0.4639 0.001 4
LiMgVO4 (mp-569876) 0.4813 0.000 4
LiFeSiO4 (mp-766664) 0.4824 0.045 4
Fe2O3 (mp-628327) 0.7251 0.116 2
Al2O3 (mp-7048) 0.6470 0.009 2
Al2O3 (mp-2254) 0.6779 0.017 2
Ga2O3 (mp-886) 0.6023 0.000 2
Fe2O3 (mp-715516) 0.6815 0.116 2
Li7V7P6(O8F)3 (mp-763895) 0.5383 0.022 5
Li7Fe7P6(O8F)3 (mp-997551) 0.5246 0.221 5
Li5Co2Cu2(PO4)4 (mp-766608) 0.5175 0.067 5
Na2TiZn2SiO7 (mp-13810) 0.4722 0.000 5
Na2TiZn2GeO7 (mp-14065) 0.5458 0.007 5
Li2Mg2MnFe(PO4)4 (mp-849669) 0.7312 0.008 6
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv P S I
Final Energy/Atom
-4.0744 eV
Corrected Energy
-111.7232 eV
Uncorrected energy = -105.9352 eV Composition-based energy adjustment (-0.503 eV/atom x 10.0 atoms) = -5.0300 eV Composition-based energy adjustment (-0.379 eV/atom x 2.0 atoms) = -0.7580 eV Corrected energy = -111.7232 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 421083

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)