material

Ca(MgSb)2

ID:

mp-9565

DOI:

10.17188/1313335


Tags: Calcium magnesium antimony (1/2/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.713 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.81 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.792 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 100045 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
GaAs (mp-2534) <1 1 1> <0 0 1> 0.000 57.2
InSb (mp-20012) <1 1 1> <0 0 1> 0.001 76.3
ZnSe (mp-1190) <1 1 1> <0 0 1> 0.002 57.2
Au (mp-81) <1 1 1> <0 0 1> 0.002 362.4
CdTe (mp-406) <1 1 1> <0 0 1> 0.003 76.3
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.004 76.3
SiC (mp-8062) <1 1 1> <0 0 1> 0.010 133.5
Ge (mp-32) <1 1 1> <0 0 1> 0.013 57.2
ZrO2 (mp-2858) <1 0 0> <1 1 1> 0.014 258.2
CdWO4 (mp-19387) <0 1 1> <1 0 0> 0.015 284.8
Te2Mo (mp-602) <0 0 1> <0 0 1> 0.018 76.3
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.020 129.1
PbS (mp-21276) <1 1 1> <0 0 1> 0.023 248.0
AlN (mp-661) <1 0 1> <1 0 1> 0.024 161.6
Ag (mp-124) <1 1 1> <0 0 1> 0.025 362.4
LiF (mp-1138) <1 0 0> <0 0 1> 0.025 133.5
AlN (mp-661) <1 1 1> <1 1 1> 0.028 258.2
SiC (mp-11714) <1 0 0> <1 0 0> 0.030 249.2
ZnO (mp-2133) <1 0 1> <1 0 0> 0.030 178.0
GaN (mp-804) <0 0 1> <0 0 1> 0.034 171.7
CdWO4 (mp-19387) <1 0 1> <1 0 0> 0.035 178.0
InP (mp-20351) <1 1 1> <0 0 1> 0.035 248.0
AlN (mp-661) <1 1 0> <1 1 0> 0.038 246.7
AlN (mp-661) <1 0 0> <1 0 0> 0.038 142.4
ZrO2 (mp-2858) <1 0 -1> <1 0 1> 0.039 323.1
WSe2 (mp-1821) <0 0 1> <1 0 1> 0.040 202.0
MoSe2 (mp-1634) <0 0 1> <1 0 1> 0.040 202.0
TiO2 (mp-2657) <1 1 1> <1 0 0> 0.047 320.4
GdScO3 (mp-5690) <0 0 1> <1 0 0> 0.048 320.4
ZnSe (mp-1190) <1 1 0> <1 1 0> 0.049 185.0
Ni (mp-23) <1 0 0> <1 0 1> 0.049 282.7
ZnO (mp-2133) <1 0 0> <1 0 1> 0.059 121.2
YVO4 (mp-19133) <1 0 0> <1 1 1> 0.060 322.7
NaCl (mp-22862) <1 1 0> <1 1 0> 0.065 185.0
ZrO2 (mp-2858) <1 1 -1> <1 0 0> 0.069 320.4
GaAs (mp-2534) <1 1 0> <1 1 0> 0.069 185.0
SiC (mp-8062) <1 1 0> <1 1 0> 0.072 246.7
C (mp-48) <0 0 1> <0 0 1> 0.078 133.5
SiC (mp-7631) <1 0 0> <1 0 0> 0.078 142.4
SiC (mp-7631) <1 1 0> <1 1 0> 0.078 246.7
SiC (mp-7631) <1 1 1> <1 1 0> 0.079 246.7
MgF2 (mp-1249) <0 0 1> <0 0 1> 0.079 152.6
BaF2 (mp-1029) <1 1 0> <1 0 1> 0.088 282.7
SrTiO3 (mp-4651) <0 0 1> <0 0 1> 0.091 343.3
SiC (mp-11714) <0 0 1> <0 0 1> 0.094 57.2
TePb (mp-19717) <1 1 0> <0 0 1> 0.095 305.2
YVO4 (mp-19133) <1 1 1> <1 1 0> 0.099 246.7
SiC (mp-7631) <0 0 1> <0 0 1> 0.102 57.2
DyScO3 (mp-31120) <0 1 1> <1 1 1> 0.105 322.7
Mg (mp-153) <1 0 1> <1 0 1> 0.106 282.7
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
77 27 20 -3 0 0
27 77 20 3 0 0
20 20 66 0 0 0
-3 3 0 27 0 0
0 0 0 0 27 -3
0 0 0 0 -3 25
Compliance Tensor Sij (10-12Pa-1)
15.5 -4.6 -3.3 2.2 0 0
-4.6 15.5 -3.3 -2.2 0 0
-3.3 -3.3 17.2 0 0 0
2.2 -2.2 0 38.2 0 0
0 0 0 0 38.2 4.4
0 0 0 0 4.4 40.1
Shear Modulus GV
26 GPa
Bulk Modulus KV
39 GPa
Shear Modulus GR
26 GPa
Bulk Modulus KR
39 GPa
Shear Modulus GVRH
26 GPa
Bulk Modulus KVRH
39 GPa
Elastic Anisotropy
0.08
Poisson's Ratio
0.23

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
10.48 -0.00 0.00
-0.00 10.48 0.00
0.00 0.00 10.92
Dielectric Tensor εij (total)
16.80 -0.00 0.00
-0.00 16.80 0.00
0.00 0.00 18.91
Polycrystalline dielectric constant εpoly
(electronic contribution)
10.63
Polycrystalline dielectric constant εpoly
(total)
17.51
Refractive Index n
3.26
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr(CdAs)2 (mp-7771) 0.0815 0.000 3
Sr(CdSb)2 (mp-7432) 0.0661 0.000 3
Eu(CdAs)2 (mp-1070314) 0.0693 0.000 3
Yb(MgSb)2 (mp-10996) 0.0327 0.000 3
Eu(CdSb)2 (mp-19774) 0.0492 0.000 3
Li6Mn(FeO3)2 (mp-764386) 0.2613 0.040 4
LiFeCuS2 (mp-755288) 0.2801 0.262 4
Pu2O3 (mp-908430) 0.2596 0.073 2
Mg3As2 (mp-7891) 0.2218 0.018 2
Bi2O3 (mp-1017552) 0.2003 0.071 2
Pu2O3 (mp-21423) 0.2098 0.073 2
Mg3Sb2 (mp-2646) 0.2502 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Mg_pv Sb
Final Energy/Atom
-3.4036 eV
Corrected Energy
-17.4020 eV
Uncorrected energy = -17.0180 eV Composition-based energy adjustment (-0.192 eV/atom x 2.0 atoms) = -0.3840 eV Corrected energy = -17.4020 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 100045
Submitted by
User remarks:
  • Calcium magnesium antimony (1/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)