Ca(ZnAs)2

ID:

mp-9571

DOI:

10.17188/1313342


Tags: Calcium dizinc arsenide Calcium zinc arsenide (1/2/2)

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.662 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.96 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.391 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P3m1 [164]
Hall
-P 3 2"
Point Group
3m
Crystal System
trigonal

Electronic Structure

Topological data for ICSD ID 100064 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
InAs (mp-20305) <1 1 1> <0 0 1> 0.001 198.3
CsI (mp-614603) <1 1 1> <0 0 1> 0.002 106.8
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.003 198.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.003 15.3
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.006 198.3
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.006 183.0
C (mp-66) <1 1 1> <0 0 1> 0.010 198.3
CdS (mp-672) <0 0 1> <0 0 1> 0.011 15.3
Ni (mp-23) <1 0 0> <1 0 0> 0.011 147.7
InP (mp-20351) <1 0 0> <1 0 0> 0.012 177.3
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.012 183.0
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.013 183.0
CdS (mp-672) <1 1 1> <0 0 1> 0.017 259.3
SiO2 (mp-6930) <1 0 1> <1 0 0> 0.019 177.3
LaF3 (mp-905) <0 0 1> <0 0 1> 0.020 45.8
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.024 198.3
BaTiO3 (mp-5986) <1 0 0> <1 0 0> 0.025 118.2
Mg (mp-153) <0 0 1> <0 0 1> 0.026 61.0
Te2W (mp-22693) <0 1 0> <1 0 0> 0.026 325.0
AlN (mp-661) <1 1 1> <0 0 1> 0.027 228.8
InP (mp-20351) <1 1 1> <0 0 1> 0.027 61.0
GdScO3 (mp-5690) <0 0 1> <0 0 1> 0.027 320.3
MgAl2O4 (mp-3536) <1 0 0> <1 1 1> 0.030 267.0
Te2W (mp-22693) <1 1 1> <0 0 1> 0.031 228.8
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.033 228.8
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.040 106.8
BaTiO3 (mp-5986) <1 1 0> <1 0 0> 0.041 118.2
SiC (mp-11714) <1 0 1> <0 0 1> 0.043 228.8
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.046 198.3
Al (mp-134) <1 0 0> <1 1 1> 0.048 213.6
Te2W (mp-22693) <0 0 1> <1 0 0> 0.048 88.6
GaAs (mp-2534) <1 0 0> <1 1 1> 0.062 267.0
CdSe (mp-2691) <1 1 1> <0 0 1> 0.067 198.3
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.067 61.0
WS2 (mp-224) <0 0 1> <0 0 1> 0.068 61.0
GaN (mp-804) <1 1 0> <1 0 1> 0.069 266.0
BN (mp-984) <1 0 1> <1 0 1> 0.073 99.8
KTaO3 (mp-3614) <1 0 0> <1 1 1> 0.078 213.6
TePb (mp-19717) <1 0 0> <1 1 1> 0.079 213.6
ZnSe (mp-1190) <1 0 0> <1 1 1> 0.086 267.0
GaSb (mp-1156) <1 1 1> <0 0 1> 0.093 198.3
ZnO (mp-2133) <1 0 1> <1 1 0> 0.093 255.9
Ga2O3 (mp-886) <1 1 0> <0 0 1> 0.097 289.8
CdWO4 (mp-19387) <0 0 1> <1 0 1> 0.102 332.5
TiO2 (mp-2657) <1 0 1> <1 0 0> 0.109 206.8
Mg (mp-153) <1 1 0> <0 0 1> 0.111 228.8
TiO2 (mp-2657) <1 1 1> <0 0 1> 0.118 289.8
GaTe (mp-542812) <1 0 1> <1 0 0> 0.121 295.4
BN (mp-984) <1 1 1> <1 0 0> 0.121 206.8
LiNbO3 (mp-3731) <1 0 1> <1 0 1> 0.123 232.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
120 32 28 -4 0 0
32 120 28 4 0 0
28 28 102 0 0 0
-4 4 0 28 0 0
0 0 0 0 28 -4
0 0 0 0 -4 44
Compliance Tensor Sij (10-12Pa-1)
9.4 -2.1 -2 1.6 0 0
-2.1 9.4 -2 -1.6 0 0
-2 -2 11 0 0 0
1.6 -1.6 0 36.4 0 0
0 0 0 0 36.4 3.2
0 0 0 0 3.2 23
Shear Modulus GV
37 GPa
Bulk Modulus KV
58 GPa
Shear Modulus GR
35 GPa
Bulk Modulus KR
57 GPa
Shear Modulus GVRH
36 GPa
Bulk Modulus KVRH
57 GPa
Elastic Anisotropy
0.29
Poisson's Ratio
0.24

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
15.25 0.00 0.00
0.00 15.25 0.00
0.00 0.00 12.69
Dielectric Tensor εij (total)
23.30 0.00 -0.00
0.00 23.30 0.00
-0.00 0.00 26.21
Polycrystalline dielectric constant εpoly
(electronic contribution)
14.40
Polycrystalline dielectric constant εpoly
(total)
24.27
Refractive Index n
3.79
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Sr(MgSb)2 (mp-9566) 0.0756 0.000 3
Ca(ZnSb)2 (mp-7429) 0.0666 0.000 3
Yb(CuS)2 (mp-1080149) 0.0666 0.000 3
Yb(ZnAs)2 (mp-10314) 0.0526 0.000 3
Yb(AlSi)2 (mp-10405) 0.0673 0.000 3
Li6Mn(FeO3)2 (mp-764386) 0.2776 0.040 4
LiFeCuS2 (mp-755288) 0.2695 0.262 4
Pu2O3 (mp-908430) 0.2618 0.073 2
Bi2O3 (mp-1017552) 0.2329 0.071 2
Pu2O3 (mp-21423) 0.2204 0.073 2
Ce2O3 (mp-2721) 0.2495 0.044 2
Ce2O3 (mp-906096) 0.2637 0.044 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ca_sv Zn As
Final Energy/Atom
-3.4286 eV
Corrected Energy
-17.1431 eV
-17.1431 eV = -17.1431 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 100064
  • 609920
Submitted by
User remarks:
  • Calcium dizinc arsenide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)