material

LiBeSb

ID:

mp-9575

DOI:

10.17188/1313345


Tags: Lithium beryllium antimony (1/1/1) Beryllium lithium antimonide

Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.244 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.039 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
4.47 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Li3Sb + Sb + Be
Band Gap
0.908 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63mc [186]
Hall
P 6c 2c
Point Group
6mm
Crystal System
hexagonal

Electronic Structure

Topological data for ICSD ID 100114 from Topological Materials Database
Topological Classification
trivial*
Subclassification
LCEBR
* trivial insulator or metal
Linear Combination of Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

Vibrational Properties

Reference for phonon calculations and visualization: Visualize with phononwebsite

Phonon dispersion

Density of States
Warning! These calculations were performed using a PBEsol exchange correlation functional in the framework of DFPT using the Abinit code. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
SiO2 (mp-6930) <0 0 1> <0 0 1> 0.002 196.0
Mg (mp-153) <1 0 1> <1 1 0> 0.002 245.0
Ge3(BiO3)4 (mp-23560) <1 1 1> <0 0 1> 0.010 196.0
WSe2 (mp-1821) <1 0 1> <1 0 1> 0.010 256.5
KTaO3 (mp-3614) <1 1 1> <0 0 1> 0.011 196.0
SiC (mp-11714) <1 0 1> <0 0 1> 0.012 226.2
Al2O3 (mp-1143) <0 0 1> <0 0 1> 0.012 60.3
ZnO (mp-2133) <1 1 1> <1 0 0> 0.012 254.6
LaF3 (mp-905) <0 0 1> <0 0 1> 0.012 45.2
DyScO3 (mp-31120) <0 0 1> <1 0 0> 0.015 282.9
Fe2O3 (mp-24972) <1 0 1> <1 0 1> 0.017 224.4
TbScO3 (mp-31119) <0 0 1> <1 0 0> 0.018 282.9
MoSe2 (mp-1634) <0 0 1> <0 0 1> 0.019 180.9
WSe2 (mp-1821) <0 0 1> <0 0 1> 0.019 180.9
Ga2O3 (mp-886) <1 0 -1> <1 0 1> 0.022 192.4
GaTe (mp-542812) <1 0 1> <1 0 0> 0.023 198.0
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.023 226.2
GaTe (mp-542812) <1 0 0> <1 0 0> 0.025 226.3
TeO2 (mp-2125) <0 1 1> <1 0 0> 0.028 226.3
KTaO3 (mp-3614) <1 1 0> <1 0 1> 0.035 160.3
Bi2Se3 (mp-541837) <0 0 1> <0 0 1> 0.035 15.1
Al (mp-134) <1 1 1> <0 0 1> 0.035 196.0
GdScO3 (mp-5690) <1 1 1> <1 0 1> 0.038 288.5
AlN (mp-661) <1 1 1> <0 0 1> 0.039 226.2
LaAlO3 (mp-2920) <1 0 0> <1 0 0> 0.040 141.5
Te2W (mp-22693) <1 1 1> <0 0 1> 0.041 226.2
LiNbO3 (mp-3731) <0 0 1> <0 0 1> 0.045 286.5
BaTiO3 (mp-5986) <1 1 1> <1 1 0> 0.049 343.0
KCl (mp-23193) <1 1 1> <0 0 1> 0.049 286.5
TiO2 (mp-390) <1 0 1> <1 0 1> 0.051 160.3
GaTe (mp-542812) <0 0 1> <1 0 0> 0.051 226.3
Al (mp-134) <1 1 0> <1 0 1> 0.052 160.3
NdGaO3 (mp-3196) <0 1 1> <0 0 1> 0.056 105.5
KP(HO2)2 (mp-23959) <0 1 0> <1 1 1> 0.057 153.8
ZrO2 (mp-2858) <1 0 0> <0 0 1> 0.069 226.2
InAs (mp-20305) <1 1 1> <0 0 1> 0.071 196.0
GdScO3 (mp-5690) <1 1 0> <1 1 1> 0.074 256.4
CsI (mp-614603) <1 1 1> <0 0 1> 0.079 105.5
MgO (mp-1265) <1 1 1> <0 0 1> 0.083 286.5
MoSe2 (mp-1634) <1 0 0> <1 0 1> 0.083 256.5
ZnTe (mp-2176) <1 1 1> <0 0 1> 0.083 196.0
TbScO3 (mp-31119) <1 1 0> <1 1 1> 0.089 256.4
LiGaO2 (mp-5854) <1 1 1> <0 0 1> 0.093 226.2
Bi2Se3 (mp-541837) <1 0 1> <1 0 0> 0.094 254.6
CaCO3 (mp-3953) <0 0 1> <0 0 1> 0.096 196.0
KCl (mp-23193) <1 0 0> <1 1 1> 0.097 205.1
ZrO2 (mp-2858) <0 1 0> <0 0 1> 0.097 226.2
C (mp-66) <1 0 0> <1 1 1> 0.097 51.3
Ge(Bi3O5)4 (mp-23352) <1 1 1> <0 0 1> 0.098 180.9
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.100 196.0
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
127 31 19 0 0 0
31 127 19 0 0 0
19 19 120 0 0 0
0 0 0 44 0 0
0 0 0 0 44 0
0 0 0 0 0 48
Compliance Tensor Sij (10-12Pa-1)
8.5 -1.9 -1 0 0 0
-1.9 8.5 -1 0 0 0
-1 -1 8.7 0 0 0
0 0 0 22.9 0 0
0 0 0 0 22.9 0
0 0 0 0 0 20.9
Shear Modulus GV
47 GPa
Bulk Modulus KV
57 GPa
Shear Modulus GR
47 GPa
Bulk Modulus KR
57 GPa
Shear Modulus GVRH
47 GPa
Bulk Modulus KVRH
57 GPa
Elastic Anisotropy
0.04
Poisson's Ratio
0.17

Piezoelectricity

Reference for tensor and properties: Methodology
Piezoelectric Tensor eij (C/m2)
0.00000 0.00000 0.00000 0.00000 -0.08086 0.00000
0.00000 0.00000 0.00000 -0.08086 0.00000 0.00000
0.23277 0.23277 -0.69881 0.00000 0.00000 0.00000
Piezoelectric Modulus ‖eijmax
0.77246 C/m2
Crystallographic Direction vmax
0.00000
-1.00000
0.00000

Dielectric Properties

Reference for tensor and properties: Methodology
Dielectric Tensor εij (electronic contribution)
12.97 0.00 0.00
0.00 12.97 0.00
0.00 0.00 13.81
Dielectric Tensor εij (total)
17.68 0.00 -0.00
0.00 17.68 0.00
-0.00 0.00 18.98
Polycrystalline dielectric constant εpoly
(electronic contribution)
13.25
Polycrystalline dielectric constant εpoly
(total)
18.12
Refractive Index n
3.64
Potentially ferroelectric?
Unknown

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ScSnAu (mp-6919) 0.2274 0.069 3
DySbPd (mp-12041) 0.2935 0.048 3
TmSnAu (mp-16741) 0.2753 0.054 3
LuCuPb (mp-16753) 0.2882 0.000 3
LuSnAu (mp-13302) 0.2300 0.063 3
Na2O (mp-755413) 0.6702 0.079 2
CaIn2 (mp-21068) 0.7139 0.000 2
Cs2Se (mp-1080258) 0.4885 0.063 2
H2W (mp-1095432) 0.6783 0.193 2
Ag2S (mp-1095694) 0.7070 0.049 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Li_sv Be_sv Sb
Final Energy/Atom
-3.5033 eV
Corrected Energy
-21.0196 eV
-21.0196 eV = -21.0196 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 616318
  • 100114
Submitted by
User remarks:
  • Beryllium lithium antimonide

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)