material

Ba3(AlSi)2

ID:

mp-9578

DOI:

10.17188/1313348


Tags: Barium aluminium silicide (3/2/2)

Material Details

Final Magnetic Moment
0.001 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.357 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.000 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
3.90 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
Stable
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
Immm [71]
Hall
-I 2 2
Point Group
mmm
Crystal System
orthorhombic

Electronic Structure

Topological data for ICSD ID 100128 from Topological Materials Database
Topological Classification
TI*
Subclassification
SEBR
* Topological insulator
Split Elementary Band Representations

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
CdWO4 (mp-19387) <1 1 0> <0 0 1> 0.009 287.8
GdScO3 (mp-5690) <1 1 1> <0 0 1> 0.020 287.8
Cu (mp-30) <1 0 0> <1 0 1> 0.026 105.5
Ni (mp-23) <1 1 0> <0 0 1> 0.032 332.1
Cu (mp-30) <1 1 0> <0 0 1> 0.035 110.7
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.044 66.4
Fe2O3 (mp-24972) <1 0 0> <1 0 1> 0.063 210.9
CdWO4 (mp-19387) <0 0 1> <0 0 1> 0.068 155.0
MgF2 (mp-1249) <1 0 0> <0 0 1> 0.071 287.8
BN (mp-984) <1 1 0> <0 0 1> 0.072 66.4
MgF2 (mp-1249) <1 1 1> <0 0 1> 0.077 332.1
CdS (mp-672) <1 1 1> <0 1 0> 0.082 259.9
TeO2 (mp-2125) <0 0 1> <0 0 1> 0.084 354.3
SiC (mp-11714) <0 0 1> <0 0 1> 0.102 221.4
TbScO3 (mp-31119) <1 1 1> <0 0 1> 0.105 287.8
SiC (mp-7631) <0 0 1> <0 0 1> 0.108 221.4
SiC (mp-11714) <1 0 0> <0 0 1> 0.111 221.4
CdWO4 (mp-19387) <1 0 0> <0 0 1> 0.111 155.0
Fe3O4 (mp-19306) <1 0 0> <0 0 1> 0.112 221.4
SiC (mp-7631) <1 0 0> <0 0 1> 0.119 332.1
C (mp-66) <1 0 0> <1 0 0> 0.119 103.1
KCl (mp-23193) <1 0 0> <0 0 1> 0.132 332.1
LiF (mp-1138) <1 0 0> <0 0 1> 0.145 354.3
SiO2 (mp-6930) <1 1 0> <0 0 1> 0.147 287.8
C (mp-48) <1 1 0> <0 0 1> 0.148 66.4
CaCO3 (mp-3953) <1 0 0> <0 0 1> 0.150 88.6
InAs (mp-20305) <1 0 0> <0 0 1> 0.158 265.7
YVO4 (mp-19133) <0 0 1> <0 0 1> 0.161 265.7
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.169 265.7
InSb (mp-20012) <1 0 0> <1 1 0> 0.172 134.7
DyScO3 (mp-31120) <1 1 1> <0 0 1> 0.175 287.8
LiGaO2 (mp-5854) <0 0 1> <0 0 1> 0.175 110.7
Te2W (mp-22693) <0 1 0> <0 0 1> 0.176 265.7
InAs (mp-20305) <1 1 0> <0 0 1> 0.178 265.7
C (mp-66) <1 1 0> <0 0 1> 0.191 110.7
CdTe (mp-406) <1 0 0> <1 1 0> 0.194 134.7
SiO2 (mp-6930) <1 1 1> <0 0 1> 0.196 265.7
ZnTe (mp-2176) <1 1 0> <0 0 1> 0.196 265.7
YAlO3 (mp-3792) <0 0 1> <0 0 1> 0.201 110.7
CeO2 (mp-20194) <1 1 0> <0 0 1> 0.202 332.1
WS2 (mp-224) <0 0 1> <0 0 1> 0.203 287.8
MoS2 (mp-1434) <0 0 1> <0 0 1> 0.204 287.8
Si (mp-149) <1 1 0> <0 0 1> 0.210 332.1
LiAlO2 (mp-3427) <1 0 1> <1 0 1> 0.212 210.9
BN (mp-984) <1 1 1> <0 0 1> 0.230 66.4
LiGaO2 (mp-5854) <1 0 0> <0 0 1> 0.232 287.8
CdTe (mp-406) <1 1 0> <0 0 1> 0.236 310.0
InSb (mp-20012) <1 1 0> <0 0 1> 0.236 310.0
YAlO3 (mp-3792) <1 0 1> <0 0 1> 0.248 287.8
SiC (mp-8062) <1 1 0> <0 0 1> 0.250 132.9
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
62 23 15 0 0 0
23 57 18 0 0 0
15 18 87 0 0 0
0 0 0 13 0 0
0 0 0 0 30 0
0 0 0 0 0 21
Compliance Tensor Sij (10-12Pa-1)
19.4 -7.4 -1.7 0 0 0
-7.4 21.4 -3.2 0 0 0
-1.7 -3.2 12.4 0 0 0
0 0 0 74.5 0 0
0 0 0 0 33.1 0
0 0 0 0 0 46.7
Shear Modulus GV
23 GPa
Bulk Modulus KV
35 GPa
Shear Modulus GR
21 GPa
Bulk Modulus KR
35 GPa
Shear Modulus GVRH
22 GPa
Bulk Modulus KVRH
35 GPa
Elastic Anisotropy
0.58
Poisson's Ratio
0.24

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
Ba3(AlSn)2 (mp-7377) 0.3178 0.006 3
Sr3(AlSn)2 (mp-7376) 0.5354 0.004 3
Sr3(AlSi)2 (mp-7068) 0.2971 0.000 3
Ba3(AlGe)2 (mp-10669) 0.1108 0.000 3
Sr3(AlGe)2 (mp-10671) 0.3842 0.000 3
Ti3B4 (mp-1025170) 0.6913 0.000 2
Nb2B3 (mp-1080021) 0.7438 0.000 2
Ta3B4 (mp-10142) 0.7306 0.000 2
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ba_sv Al Si
Final Energy/Atom
-3.7990 eV
Corrected Energy
-26.5929 eV
-26.5929 eV = -26.5929 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
ICSD IDs
  • 100128
Submitted by
User remarks:
  • Barium aluminium silicide (3/2/2)

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)