Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.637 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.119 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.35 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNa3Sb + Ba5Sb3 + Ba5Sb4 |
Band Gap0.546 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 242.0 |
CeO2 (mp-20194) | <1 0 0> | <1 1 1> | 296.4 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 285.2 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 285.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 1> | 296.4 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 171.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 285.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 161.3 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 242.0 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 171.1 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 296.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 285.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 242.0 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 296.4 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 171.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 285.2 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 342.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 285.2 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 228.2 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 296.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 98.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 228.2 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 171.1 |
BN (mp-984) | <1 0 0> | <1 0 0> | 57.0 |
LiNbO3 (mp-3731) | <1 0 0> | <1 1 1> | 296.4 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 242.0 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 228.2 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 285.2 |
SiC (mp-7631) | <0 0 1> | <1 1 1> | 98.8 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 161.3 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 161.3 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 285.2 |
LiTaO3 (mp-3666) | <0 0 1> | <1 0 0> | 285.2 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 285.2 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 114.1 |
Te2W (mp-22693) | <0 0 1> | <1 1 1> | 197.6 |
Te2W (mp-22693) | <0 1 0> | <1 1 0> | 161.3 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 242.0 |
C (mp-66) | <1 0 0> | <1 0 0> | 114.1 |
C (mp-66) | <1 1 0> | <1 1 0> | 161.3 |
Mg (mp-153) | <1 1 0> | <1 1 1> | 296.4 |
Mg (mp-153) | <1 1 1> | <1 1 0> | 242.0 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 114.1 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 161.3 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 161.3 |
BN (mp-984) | <0 0 1> | <1 0 0> | 285.2 |
BN (mp-984) | <1 1 0> | <1 0 0> | 228.2 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 285.2 |
TbScO3 (mp-31119) | <0 0 1> | <1 0 0> | 285.2 |
InSb (mp-20012) | <1 1 1> | <1 1 1> | 296.4 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
36 | 18 | 18 | 0 | 0 | 0 |
18 | 36 | 18 | 0 | 0 | 0 |
18 | 18 | 36 | 0 | 0 | 0 |
0 | 0 | 0 | 13 | 0 | 0 |
0 | 0 | 0 | 0 | 13 | 0 |
0 | 0 | 0 | 0 | 0 | 13 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
41.4 | -13.9 | -13.9 | 0 | 0 | 0 |
-13.9 | 41.4 | -13.9 | 0 | 0 | 0 |
-13.9 | -13.9 | 41.4 | 0 | 0 | 0 |
0 | 0 | 0 | 78.7 | 0 | 0 |
0 | 0 | 0 | 0 | 78.7 | 0 |
0 | 0 | 0 | 0 | 0 | 78.7 |
Shear Modulus GV11 GPa |
Bulk Modulus KV24 GPa |
Shear Modulus GR11 GPa |
Bulk Modulus KR24 GPa |
Shear Modulus GVRH11 GPa |
Bulk Modulus KVRH24 GPa |
Elastic Anisotropy0.14 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
LiAgTe (mp-962069) | 0.0000 | 0.126 | 3 |
LiAlGe (mp-961645) | 0.0000 | 0.340 | 3 |
TiNiSb (mp-581712) | 0.0000 | 0.456 | 3 |
ZrFeTe (mp-961649) | 0.0000 | 0.067 | 3 |
ZrAsRh (mp-961720) | 0.0000 | 0.522 | 3 |
BaCl2 (mp-568662) | 0.0000 | 0.000 | 2 |
BiO2 (mp-32548) | 0.0000 | 0.102 | 2 |
CeH2 (mp-505569) | 0.0000 | 0.000 | 2 |
EuF2 (mp-504731) | 0.0000 | 0.000 | 2 |
Cu2S (mp-12087) | 0.0000 | 0.094 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ba_sv Na_pv Sb |
Final Energy/Atom-3.0935 eV |
Corrected Energy-9.2804 eV
-9.2804 eV = -9.2804 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)