Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.120 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.255 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.02 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToCaSi2 + CaCd6 + CaSi |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinF43m [216] |
HallF 4 2 3 |
Point Group43m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 77.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 126.4 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 316.0 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 126.4 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 252.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 232.2 |
LaAlO3 (mp-2920) | <1 0 1> | <1 1 0> | 316.0 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 252.8 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 189.6 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 189.6 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 252.8 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 252.8 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 316.0 |
DyScO3 (mp-31120) | <1 0 0> | <1 1 0> | 189.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 252.8 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 268.1 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 189.6 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 232.2 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 189.6 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 189.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 223.4 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 189.6 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 44.7 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 63.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 223.4 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 77.4 |
Te2Mo (mp-602) | <0 0 1> | <1 1 1> | 77.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 0> | 252.8 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 89.4 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 189.6 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 223.4 |
BN (mp-984) | <0 0 1> | <1 0 0> | 312.8 |
MoS2 (mp-1434) | <0 0 1> | <1 1 0> | 316.0 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 309.6 |
Al (mp-134) | <1 1 0> | <1 1 0> | 189.6 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 252.8 |
LiGaO2 (mp-5854) | <1 0 0> | <1 1 1> | 309.6 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 63.2 |
CdTe (mp-406) | <1 1 1> | <1 1 1> | 77.4 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 223.4 |
SiC (mp-7631) | <1 1 0> | <1 1 0> | 252.8 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 44.7 |
LiTaO3 (mp-3666) | <0 0 1> | <1 1 1> | 309.6 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 223.4 |
TiO2 (mp-2657) | <1 1 0> | <1 0 0> | 178.7 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 89.4 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 44.7 |
TiO2 (mp-2657) | <1 0 1> | <1 0 0> | 312.8 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 223.4 |
GdScO3 (mp-5690) | <1 0 0> | <1 1 0> | 189.6 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
68 | 33 | 33 | 0 | 0 | 0 |
33 | 68 | 33 | 0 | 0 | 0 |
33 | 33 | 68 | 0 | 0 | 0 |
0 | 0 | 0 | 22 | 0 | 0 |
0 | 0 | 0 | 0 | 22 | 0 |
0 | 0 | 0 | 0 | 0 | 22 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
21.6 | -7.1 | -7.1 | 0 | 0 | 0 |
-7.1 | 21.6 | -7.1 | 0 | 0 | 0 |
-7.1 | -7.1 | 21.6 | 0 | 0 | 0 |
0 | 0 | 0 | 46 | 0 | 0 |
0 | 0 | 0 | 0 | 46 | 0 |
0 | 0 | 0 | 0 | 0 | 46 |
Shear Modulus GV20 GPa |
Bulk Modulus KV45 GPa |
Shear Modulus GR20 GPa |
Bulk Modulus KR45 GPa |
Shear Modulus GVRH20 GPa |
Bulk Modulus KVRH45 GPa |
Elastic Anisotropy0.06 |
Poisson's Ratio0.31 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
TaAlPt (mp-961679) | 0.0000 | 0.677 | 3 |
TlCoBi (mp-631546) | 0.0000 | 0.860 | 3 |
BaHfMo (mp-631521) | 0.0000 | 1.273 | 3 |
ZrGePt (mp-961681) | 0.0000 | 0.607 | 3 |
TiSnPd (mp-961682) | 0.0000 | 0.000 | 3 |
BaCl2 (mp-568662) | 0.0000 | 0.000 | 2 |
BiO2 (mp-32548) | 0.0000 | 0.102 | 2 |
CeH2 (mp-505569) | 0.0000 | 0.000 | 2 |
EuF2 (mp-504731) | 0.0000 | 0.000 | 2 |
Cu2S (mp-12087) | 0.0000 | 0.094 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Ca_sv Cd Si |
Final Energy/Atom-2.9048 eV |
Corrected Energy-8.7145 eV
-8.7145 eV = -8.7145 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)