Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.201 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.004 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.57 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToInP |
Band Gap0.514 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
KP(HO2)2 (mp-23959) | <0 0 1> | <1 1 0> | 151.0 |
GaTe (mp-542812) | <0 0 1> | <1 0 0> | 232.5 |
Mg (mp-153) | <0 0 1> | <0 0 1> | 61.4 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 61.4 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 15.4 |
C (mp-66) | <1 1 1> | <0 0 1> | 199.6 |
SrTiO3 (mp-4651) | <1 0 1> | <0 0 1> | 107.5 |
SiC (mp-11714) | <0 0 1> | <0 0 1> | 107.5 |
Ge(Bi3O5)4 (mp-23352) | <1 1 1> | <0 0 1> | 184.2 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 199.6 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 107.5 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 199.6 |
CsI (mp-614603) | <1 1 1> | <0 0 1> | 107.5 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 199.6 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 61.4 |
WS2 (mp-224) | <0 0 1> | <0 0 1> | 61.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 199.6 |
C (mp-48) | <1 0 0> | <1 0 1> | 230.1 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 199.6 |
LiTaO3 (mp-3666) | <1 0 1> | <1 0 1> | 230.1 |
Ga2O3 (mp-886) | <1 1 0> | <0 0 1> | 291.7 |
TeO2 (mp-2125) | <0 0 1> | <0 0 1> | 322.4 |
ZnSe (mp-1190) | <1 0 0> | <1 1 1> | 263.1 |
KTaO3 (mp-3614) | <1 0 0> | <1 1 1> | 210.5 |
CdS (mp-672) | <1 0 1> | <1 0 1> | 32.9 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 15.4 |
BN (mp-984) | <1 1 1> | <1 0 0> | 203.4 |
Mg (mp-153) | <1 1 0> | <0 0 1> | 230.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 199.6 |
Cu (mp-30) | <1 0 0> | <1 1 1> | 52.6 |
Mg (mp-153) | <1 1 1> | <1 0 1> | 361.5 |
GaAs (mp-2534) | <1 0 0> | <1 1 1> | 263.1 |
GaP (mp-2490) | <1 0 0> | <1 0 1> | 361.5 |
YVO4 (mp-19133) | <1 0 1> | <1 1 1> | 210.5 |
LiNbO3 (mp-3731) | <1 0 1> | <1 0 1> | 230.1 |
CdS (mp-672) | <1 1 1> | <1 1 1> | 52.6 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 262.9 |
ZrO2 (mp-2858) | <1 0 -1> | <1 0 0> | 145.3 |
ZrO2 (mp-2858) | <1 0 0> | <0 0 1> | 230.3 |
Si (mp-149) | <1 0 0> | <1 0 1> | 361.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 138.2 |
NaCl (mp-22862) | <1 1 0> | <1 0 1> | 230.1 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 164.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 361.5 |
Al (mp-134) | <1 0 0> | <1 1 1> | 210.5 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 184.2 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 184.2 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 50.3 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 29.1 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 230.3 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
102 | 40 | 29 | 0 | 0 | 0 |
40 | 102 | 29 | 0 | 0 | 0 |
29 | 29 | 120 | 0 | 0 | 0 |
0 | 0 | 0 | 26 | 0 | 0 |
0 | 0 | 0 | 0 | 26 | 0 |
0 | 0 | 0 | 0 | 0 | 31 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
12 | -4.1 | -1.9 | 0 | 0 | 0 |
-4.1 | 12 | -1.9 | 0 | 0 | 0 |
-1.9 | -1.9 | 9.2 | 0 | 0 | 0 |
0 | 0 | 0 | 38.8 | 0 | 0 |
0 | 0 | 0 | 0 | 38.8 | 0 |
0 | 0 | 0 | 0 | 0 | 32.1 |
Shear Modulus GV32 GPa |
Bulk Modulus KV58 GPa |
Shear Modulus GR30 GPa |
Bulk Modulus KR58 GPa |
Shear Modulus GVRH31 GPa |
Bulk Modulus KVRH58 GPa |
Elastic Anisotropy0.20 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BeSiN2 (mp-7913) | 0.0620 | 0.000 | 3 |
LiInSe2 (mp-20310) | 0.1013 | 0.001 | 3 |
MgSnN2 (mp-1029791) | 0.1548 | 0.000 | 3 |
ZnSnN2 (mp-1029469) | 0.0648 | 0.000 | 3 |
Zn2SbN3 (mp-1029334) | 0.1456 | 0.004 | 3 |
Li2ZnSnS4 (mp-555186) | 0.1904 | 0.000 | 4 |
ZnGaNO (mp-558481) | 0.2875 | 0.058 | 4 |
ZnCu2GeS4 (mp-6408) | 0.3044 | 0.000 | 4 |
CoCu2SiS4 (mp-11769) | 0.3070 | 0.065 | 4 |
ZnCu2SnS4 (mp-1079541) | 0.3106 | 0.000 | 4 |
AlP (mp-8880) | 0.0076 | 0.004 | 2 |
MgGa (mp-1094992) | 0.0038 | 0.664 | 2 |
HgS (mp-973676) | 0.0083 | 0.002 | 2 |
CdTe (mp-12779) | 0.0025 | 0.003 | 2 |
ZnS (mp-560588) | 0.0052 | 0.003 | 2 |
Ge (mp-1007760) | 0.0267 | 0.121 | 1 |
Si (mp-165) | 0.0368 | 0.011 | 1 |
C (mp-611426) | 0.2259 | 0.146 | 1 |
C (mp-47) | 0.0450 | 0.162 | 1 |
Ge (mp-1091415) | 0.2389 | 0.008 | 1 |
Explore more synthesis descriptions for materials of composition InP.
Text computed by synthesisproject.org.
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: In_d P |
Final Energy/Atom-4.2840 eV |
Corrected Energy-17.1359 eV
-17.1359 eV = -17.1359 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)