material

Zn3B

ID:

mp-971859

DOI:

10.17188/1313653


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
0.617 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.617 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
6.71 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
B + Zn
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
I4/mmm [139]
Hall
-I 4 2
Point Group
4/mmm
Crystal System
tetragonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

X-Ray Absorption Spectra

FEFF XANES

Select an element to display a spectrum averaged over all sites of that element in the structure.

Apply Gaussian smoothing:

0 eV
3 eV
FWHM: 0 eV

Download spectra for every symmetrically equivalent absorption site in the structure.

Download FEFF Input parameters.

Warning: These results are intended to be semi-quantitative in that corrections, such as edge shifts and Debye-Waller damping, have not been included.

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
Ag (mp-124) <1 1 0> <1 0 0> -0.385 220.5
TiO2 (mp-2657) <1 1 1> <1 1 0> -0.198 117.0
Ga2O3 (mp-886) <1 0 0> <1 1 0> -0.107 272.9
NdGaO3 (mp-3196) <0 1 0> <1 0 1> -0.107 339.2
CdS (mp-672) <1 0 1> <1 1 0> -0.106 194.9
Fe2O3 (mp-24972) <0 0 1> <0 0 1> -0.095 69.1
C (mp-48) <1 0 0> <1 0 1> -0.090 154.2
CdS (mp-672) <1 1 1> <0 0 1> -0.089 262.7
BaTiO3 (mp-5986) <1 0 1> <0 0 1> -0.082 373.2
Si (mp-149) <1 1 0> <1 0 1> -0.064 339.2
CeO2 (mp-20194) <1 1 0> <1 0 1> -0.064 339.2
NdGaO3 (mp-3196) <1 0 0> <1 0 1> -0.062 308.4
CdWO4 (mp-19387) <0 1 0> <0 0 1> -0.060 290.3
YVO4 (mp-19133) <1 1 0> <1 0 0> -0.059 330.8
ZnSe (mp-1190) <1 1 1> <0 0 1> -0.052 345.6
LiF (mp-1138) <1 1 1> <0 0 1> -0.045 345.6
NdGaO3 (mp-3196) <0 0 1> <1 1 1> -0.037 124.1
BaF2 (mp-1029) <1 0 0> <1 0 1> -0.035 277.6
WS2 (mp-224) <1 0 0> <0 0 1> -0.024 317.9
TiO2 (mp-2657) <1 0 0> <1 0 1> -0.024 123.4
AlN (mp-661) <0 0 1> <0 0 1> -0.019 152.1
ZnO (mp-2133) <0 0 1> <0 0 1> -0.016 179.7
LiNbO3 (mp-3731) <1 0 0> <0 0 1> -0.016 221.2
MgF2 (mp-1249) <1 1 1> <1 0 0> -0.011 358.4
TeO2 (mp-2125) <0 1 0> <1 0 1> -0.009 277.6
Mg (mp-153) <1 0 1> <0 0 1> -0.007 207.4
ZrO2 (mp-2858) <0 0 1> <0 0 1> -0.000 27.6
SrTiO3 (mp-4651) <0 0 1> <1 1 1> 0.001 124.1
Ag (mp-124) <1 0 0> <0 0 1> 0.001 69.1
MgF2 (mp-1249) <0 0 1> <1 0 0> 0.002 110.3
LiGaO2 (mp-5854) <1 1 1> <1 1 0> 0.002 272.9
Ag (mp-124) <1 1 1> <1 0 0> 0.003 275.7
Cu (mp-30) <1 1 1> <0 0 1> 0.003 69.1
SrTiO3 (mp-4651) <1 1 0> <1 1 1> 0.004 124.1
GaN (mp-804) <1 1 0> <1 1 0> 0.004 117.0
LiGaO2 (mp-5854) <0 1 0> <0 0 1> 0.005 359.4
ZnTe (mp-2176) <1 0 0> <0 0 1> 0.007 345.6
CsI (mp-614603) <1 0 0> <1 1 1> 0.007 124.1
DyScO3 (mp-31120) <1 0 1> <1 0 1> 0.007 277.6
Ni (mp-23) <1 1 0> <1 1 0> 0.011 155.9
Ni (mp-23) <1 0 0> <1 0 0> 0.011 110.3
InAs (mp-20305) <1 0 0> <0 0 1> 0.011 345.6
LiAlO2 (mp-3427) <1 0 0> <1 1 1> 0.012 165.5
CdSe (mp-2691) <1 0 0> <0 0 1> 0.013 345.6
Ga2O3 (mp-886) <0 1 0> <1 1 1> 0.014 289.6
SrTiO3 (mp-4651) <1 0 0> <1 1 0> 0.015 350.9
AlN (mp-661) <1 1 1> <1 1 0> 0.016 311.9
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.019 39.0
Bi2Te3 (mp-34202) <0 0 1> <1 0 1> 0.022 277.6
TbScO3 (mp-31119) <1 0 1> <1 0 1> 0.022 277.6
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
114 118 54 0 0 0
118 114 54 0 0 0
54 54 176 0 0 0
0 0 0 -28 0 0
0 0 0 0 -28 0
0 0 0 0 0 -20
Compliance Tensor Sij (10-12Pa-1)
-140.5 145.5 -1.5 0 0 0
145.5 -140.5 -1.5 0 0 0
-1.5 -1.5 6.6 0 0 0
0 0 0 -35.8 0 0
0 0 0 0 -35.8 0
0 0 0 0 0 -49
Shear Modulus GV
-3 GPa
Bulk Modulus KV
95 GPa
Shear Modulus GR
-7 GPa
Bulk Modulus KR
95 GPa
Shear Modulus GVRH
-5 GPa
Bulk Modulus KVRH
95 GPa
Elastic Anisotropy
-2.76
Poisson's Ratio
0.53

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
ZnCu2Ni (mp-30593) 0.1104 0.005 3
CrCoPt2 (mp-570863) 0.0452 0.034 3
LiCa6Ge (mp-12609) 0.0043 0.183 3
GaFeNi2 (mp-1065359) 0.0371 0.065 3
GaCo2Ni (mp-1018060) 0.0115 0.075 3
Cr8Ni50Mo15W2 (mp-767372) 0.2132 0.028 4
CrFeCoNi (mp-1012640) 0.3586 0.065 4
CrFeCoNi (mp-1096923) 0.4000 0.193 4
Ho3Zr (mp-976029) 0.0000 0.086 2
PrY3 (mp-975784) 0.0006 0.024 2
PuPd3 (mp-861601) 0.0000 0.531 2
Cu3Pd (mp-580357) 0.0000 0.000 2
PtRh3 (mp-974376) 0.0001 0.000 2
As (mp-1096826) 0.0032 0.559 1
Sc (mp-36) 0.0034 0.048 1
Eu (mp-623532) 0.0043 0.035 1
Au (mp-81) 0.0043 0.000 1
Dy (mp-10750) 0.0041 0.021 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Zn B
Final Energy/Atom
-1.9980 eV
Corrected Energy
-7.9920 eV
Uncorrected energy = -7.9920 eV Corrected energy = -7.9920 eV

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)