Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.859 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.64 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap2.207 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinR3 [148] |
Hall-R 3 |
Point Group3 |
Crystal Systemtrigonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 0 1> | 261.1 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 261.1 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 87.0 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 148.3 |
BN (mp-984) | <1 1 0> | <0 0 1> | 261.1 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 1> | 171.9 |
C (mp-66) | <1 1 1> | <0 0 1> | 87.0 |
PbS (mp-21276) | <1 1 1> | <0 0 1> | 261.1 |
InP (mp-20351) | <1 1 0> | <1 0 0> | 148.3 |
Ni (mp-23) | <1 0 0> | <1 0 0> | 148.3 |
PbSe (mp-2201) | <1 1 1> | <0 0 1> | 261.1 |
MoSe2 (mp-1634) | <0 0 1> | <0 0 1> | 87.0 |
Au (mp-81) | <1 1 0> | <1 0 0> | 148.3 |
CdSe (mp-2691) | <1 1 1> | <0 0 1> | 261.1 |
WSe2 (mp-1821) | <0 0 1> | <0 0 1> | 87.0 |
ZnO (mp-2133) | <0 0 1> | <0 0 1> | 261.1 |
Cu (mp-30) | <1 1 0> | <1 0 0> | 148.3 |
Al2O3 (mp-1143) | <0 0 1> | <0 0 1> | 261.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 261.1 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 87.0 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 261.1 |
BN (mp-984) | <0 0 1> | <0 0 1> | 87.0 |
Al (mp-134) | <1 1 1> | <0 0 1> | 87.0 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 261.1 |
GdScO3 (mp-5690) | <1 0 1> | <0 0 1> | 174.1 |
InP (mp-20351) | <1 1 1> | <0 0 1> | 261.1 |
Ni (mp-23) | <1 1 1> | <0 0 1> | 87.0 |
WSe2 (mp-1821) | <1 0 0> | <1 0 0> | 148.3 |
Ge(Bi3O5)4 (mp-23352) | <1 1 0> | <1 0 0> | 148.3 |
CaCO3 (mp-3953) | <0 0 1> | <0 0 1> | 87.0 |
CaCO3 (mp-3953) | <1 0 0> | <1 0 1> | 171.9 |
TiO2 (mp-390) | <1 0 0> | <1 0 0> | 148.3 |
GaSb (mp-1156) | <1 1 1> | <0 0 1> | 261.1 |
Cu (mp-30) | <1 0 0> | <0 0 1> | 261.1 |
ZnTe (mp-2176) | <1 1 1> | <0 0 1> | 261.1 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sc(IO3)3 (mp-30002) | 0.4756 | 0.000 | 3 |
In(IO3)3 (mp-23400) | 0.5069 | 0.000 | 3 |
Sr(IO3)2 (mp-754869) | 0.4748 | 0.026 | 3 |
In(IO3)3 (mp-23559) | 0.2693 | 0.005 | 3 |
Co(IO3)2 (mp-774233) | 0.5480 | 0.145 | 3 |
NaGa(TeO3)2 (mp-554193) | 0.6184 | 0.002 | 4 |
LiVWO6 (mp-768026) | 0.6196 | 0.054 | 4 |
YCo(WO4)2 (mvc-587) | 0.6576 | 0.173 | 4 |
YFe(WO4)2 (mvc-620) | 0.6652 | 0.054 | 4 |
YMn(WO4)2 (mvc-622) | 0.6492 | 0.049 | 4 |
WF4 (mvc-14582) | 0.7447 | 0.060 | 2 |
Ge5F12 (mp-27342) | 0.7254 | 0.000 | 2 |
Sn3F8 (mp-1443) | 0.7478 | 0.000 | 2 |
TiZnH12(OF)6 (mp-866807) | 0.7112 | 0.020 | 5 |
Sr2NiSe2(ClO3)2 (mp-566796) | 0.7160 | 0.000 | 5 |
AlH2PbO2F3 (mp-643387) | 0.7345 | 0.000 | 5 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tl_d I O |
Final Energy/Atom-4.3315 eV |
Corrected Energy-125.2613 eV
-125.2613 eV = -112.6201 eV (uncorrected energy) - 12.6412 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)