material

TiPt3

ID:

mp-972220

DOI:

10.17188/1313782


Material Details

Final Magnetic Moment
0.000 μB

Calculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit.

Magnetic Ordering
NM
Formation Energy / Atom
-0.838 eV

Calculated formation energy from the elements normalized to per atom in the unit cell.

Energy Above Hull / Atom
0.011 eV

The energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures.

Density
17.05 g/cm3

The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%)

Decomposes To
TiPt3
Band Gap
0.000 eV

In general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic.

Space Group

Hermann Mauguin
P63/mmc [194]
Hall
-P 6c 2c
Point Group
6/mmm
Crystal System
hexagonal

Electronic Structure

Band Structure and Density of States

Warning! Semi-local DFT tends to severely underestimate bandgaps. Please see the wiki for more info.

X-Ray Diffraction

    Select radiation source:
  • Cu
  • Ag
  • Mo
  • Fe

Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)

Substrates

Reference for minimal coincident interface area (MCIA) and elastic energy:
substrate orientation:
substrate material substrate orientation film orientation elastic energy [meV] MCIA [Å2]
BaTiO3 (mp-5986) <1 0 0> <1 0 1> 0.052 335.3
Te2W (mp-22693) <1 1 1> <1 0 0> 0.058 228.4
LaAlO3 (mp-2920) <0 0 1> <0 0 1> 0.067 327.3
ZnO (mp-2133) <1 0 0> <1 0 0> 0.073 279.1
SiC (mp-7631) <1 0 1> <1 0 1> 0.078 335.3
LiAlO2 (mp-3427) <1 1 0> <0 0 1> 0.082 327.3
Au (mp-81) <1 0 0> <1 0 1> 0.092 260.8
KCl (mp-23193) <1 0 0> <1 0 0> 0.095 203.0
Ag (mp-124) <1 0 0> <1 0 1> 0.107 260.8
BaTiO3 (mp-5986) <1 1 1> <1 0 0> 0.112 228.4
TiO2 (mp-390) <1 1 0> <1 1 0> 0.118 263.7
SrTiO3 (mp-4651) <1 0 0> <1 0 0> 0.122 177.6
AlN (mp-661) <0 0 1> <0 0 1> 0.129 109.1
WS2 (mp-224) <1 0 1> <1 0 0> 0.135 279.1
LiGaO2 (mp-5854) <1 1 0> <0 0 1> 0.153 190.9
TePb (mp-19717) <1 0 0> <1 0 1> 0.158 260.8
ZrO2 (mp-2858) <1 0 1> <1 1 1> 0.165 258.7
YAlO3 (mp-3792) <0 1 0> <1 1 0> 0.176 351.6
SiC (mp-7631) <0 0 1> <0 0 1> 0.179 109.1
BN (mp-984) <1 0 1> <1 0 0> 0.190 279.1
SiC (mp-11714) <0 0 1> <0 0 1> 0.196 109.1
BN (mp-984) <1 1 1> <1 1 0> 0.214 307.7
AlN (mp-661) <1 1 1> <1 1 1> 0.220 258.7
NdGaO3 (mp-3196) <1 1 1> <1 0 0> 0.220 203.0
SrTiO3 (mp-4651) <1 0 1> <0 0 1> 0.228 54.6
Te2Mo (mp-602) <0 0 1> <1 1 1> 0.236 155.2
MgF2 (mp-1249) <1 1 0> <1 1 0> 0.242 263.7
Ga2O3 (mp-886) <1 0 0> <1 1 0> 0.247 219.8
CdTe (mp-406) <1 0 0> <1 0 1> 0.258 260.8
MgF2 (mp-1249) <1 0 0> <1 1 1> 0.260 258.7
YVO4 (mp-19133) <1 1 0> <1 0 0> 0.262 329.9
C (mp-48) <0 0 1> <0 0 1> 0.280 109.1
GaN (mp-804) <0 0 1> <0 0 1> 0.284 27.3
InSb (mp-20012) <1 0 0> <1 0 1> 0.296 260.8
LiAlO2 (mp-3427) <1 0 0> <1 0 0> 0.306 228.4
KCl (mp-23193) <1 1 0> <1 1 0> 0.312 175.8
GaP (mp-2490) <1 1 1> <1 0 1> 0.343 260.8
MgF2 (mp-1249) <0 0 1> <1 0 1> 0.349 260.8
Si (mp-149) <1 1 1> <1 0 1> 0.354 260.8
CeO2 (mp-20194) <1 1 1> <1 0 1> 0.362 260.8
NdGaO3 (mp-3196) <1 0 0> <1 0 0> 0.365 177.6
ZrO2 (mp-2858) <0 0 1> <1 0 0> 0.366 279.1
MgF2 (mp-1249) <1 0 1> <1 0 1> 0.366 260.8
CdS (mp-672) <0 0 1> <0 0 1> 0.372 109.1
MoS2 (mp-1434) <1 0 0> <1 1 1> 0.395 206.9
ZnO (mp-2133) <1 1 0> <1 0 1> 0.399 149.0
Au (mp-81) <1 1 1> <1 0 1> 0.400 335.3
CaF2 (mp-2741) <1 1 1> <1 0 1> 0.416 260.8
GaTe (mp-542812) <1 0 0> <1 1 1> 0.429 310.4
LiAlO2 (mp-3427) <1 1 1> <1 1 0> 0.431 219.8
Up to 50 entries displayed.
minimal coincident interface area.

Elasticity

Reference for tensor and properties:
Stiffness Tensor Cij (GPa)
383 160 155 0 0 0
160 383 155 0 0 0
155 155 403 0 0 0
0 0 0 66 0 0
0 0 0 0 66 0
0 0 0 0 0 111
Compliance Tensor Sij (10-12Pa-1)
3.4 -1.1 -0.9 0 0 0
-1.1 3.4 -0.9 0 0 0
-0.9 -0.9 3.2 0 0 0
0 0 0 15.1 0 0
0 0 0 0 15.1 0
0 0 0 0 0 9
Shear Modulus GV
95 GPa
Bulk Modulus KV
234 GPa
Shear Modulus GR
89 GPa
Bulk Modulus KR
234 GPa
Shear Modulus GVRH
92 GPa
Bulk Modulus KVRH
234 GPa
Elastic Anisotropy
0.38
Poisson's Ratio
0.33

Similar Structures beta feature

Explanation of dissimilarity measure: Documentation.
material dissimilarity Ehull # of elements
NaCaMg6 (mp-1099110) 0.0259 0.111 3
Cr8Ni50Mo15W2 (mp-767372) 0.2592 0.028 4
CrFeCoNi (mp-1012640) 0.1816 0.065 4
CrFeCoNi (mp-1096923) 0.3950 0.193 4
Be3Ni (mp-984315) 0.0079 0.003 2
Pr3Y (mp-975586) 0.0055 0.025 2
LaPm3 (mp-976823) 0.0073 0.032 2
CoRe3 (mp-865960) 0.0112 0.000 2
MgGa2 (mp-1094644) 0.0109 0.055 2
Eu (mp-21462) 0.0185 0.046 1
Co (mp-987206) 0.0230 0.000 1
Co (mp-54) 0.0217 0.000 1
Na (mp-10172) 0.0223 0.010 1
Cs (mp-11832) 0.0223 0.035 1
Up to 5 similar elemental, binary, ternary, quaternary, etc. structures displayed (dissimilarity threshold 0.75). Ehull: energy above hull per atom [eV].

Calculation Summary

Elasticity

Methodology

Structure Optimization

Run Type
GGA
Energy Cutoff
520 eV
# of K-points
None
U Values
--
Pseudopotentials
VASP PAW: Ti_pv Pt
Final Energy/Atom
-7.3654 eV
Corrected Energy
-58.9233 eV
-58.9233 eV = -58.9233 eV (uncorrected energy)

Detailed input parameters and outputs for all calculations


Show JSON History Show BibTex Citation Download BibTex Citation
Submitted by

Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)