Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.743 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.076 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTmBiPd + BiPd + TmPd3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 0> | <1 1 1> | 247.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 238.3 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 269.6 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 134.8 |
GaAs (mp-2534) | <1 1 1> | <1 0 0> | 285.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 190.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 238.3 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 269.6 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 202.2 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 269.6 |
DyScO3 (mp-31120) | <1 0 1> | <1 1 1> | 165.1 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 190.6 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 134.8 |
ZnSe (mp-1190) | <1 1 1> | <1 0 0> | 285.9 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 67.4 |
KTaO3 (mp-3614) | <1 1 1> | <1 1 1> | 82.5 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 247.6 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 143.0 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 202.2 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 143.0 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 202.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 238.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 238.3 |
SiC (mp-7631) | <0 0 1> | <1 0 0> | 285.9 |
C (mp-66) | <1 1 0> | <1 1 0> | 202.2 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 1> | 165.1 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 165.1 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 238.3 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 238.3 |
KP(HO2)2 (mp-23959) | <1 0 0> | <1 0 0> | 238.3 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 202.2 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 247.6 |
GaP (mp-2490) | <1 1 0> | <1 1 0> | 134.8 |
GaP (mp-2490) | <1 1 1> | <1 1 0> | 269.6 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 202.2 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 1> | 165.1 |
Ni (mp-23) | <1 0 0> | <1 1 1> | 247.6 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 333.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 190.6 |
NdGaO3 (mp-3196) | <0 0 1> | <1 1 0> | 269.6 |
NdGaO3 (mp-3196) | <0 1 0> | <1 1 0> | 134.8 |
NdGaO3 (mp-3196) | <1 1 0> | <1 0 0> | 238.3 |
SiC (mp-11714) | <1 0 1> | <1 0 0> | 333.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 190.6 |
Si (mp-149) | <1 0 0> | <1 0 0> | 238.3 |
Si (mp-149) | <1 1 1> | <1 1 0> | 269.6 |
Au (mp-81) | <1 1 0> | <1 1 0> | 202.2 |
WS2 (mp-224) | <1 0 0> | <1 1 0> | 134.8 |
NaCl (mp-22862) | <1 1 0> | <1 1 0> | 134.8 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 190.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Sm2MgTl (mp-978625) | 0.0000 | 0.005 | 3 |
LiLu2Ru (mp-977393) | 0.0000 | 0.000 | 3 |
Tm2ZnAg (mp-971979) | 0.0000 | 0.011 | 3 |
MnGeRu2 (mp-864936) | 0.0000 | 0.000 | 3 |
Gd2IrPd (mp-866029) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.058 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.074 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
K3Hg (mp-983388) | 0.0000 | 0.063 | 2 |
SbPt3 (mp-973353) | 0.0000 | 0.123 | 2 |
ScZn3 (mp-973143) | 0.0000 | 0.018 | 2 |
Yb3Os (mp-980006) | 0.0000 | 0.236 | 2 |
SmCd3 (mp-867158) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.446 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.139 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 Bi Pd |
Final Energy/Atom-5.4240 eV |
Corrected Energy-21.6958 eV
-21.6958 eV = -21.6958 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)