Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.056 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.010 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.89 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSmMg + Sm |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinCmcm [63] |
Hall-C 2c 2 |
Point Groupmmm |
Crystal Systemorthorhombic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 0> | 274.0 |
AlN (mp-661) | <1 0 0> | <0 1 0> | 295.1 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 194.5 |
AlN (mp-661) | <1 1 0> | <0 1 0> | 337.3 |
CeO2 (mp-20194) | <1 0 0> | <0 1 0> | 210.8 |
CeO2 (mp-20194) | <1 1 0> | <0 1 0> | 42.2 |
CeO2 (mp-20194) | <1 1 1> | <0 1 0> | 252.9 |
GaAs (mp-2534) | <1 0 0> | <0 1 0> | 63.2 |
GaAs (mp-2534) | <1 1 0> | <0 1 0> | 231.9 |
BaF2 (mp-1029) | <1 0 0> | <0 1 0> | 316.2 |
BaF2 (mp-1029) | <1 1 0> | <0 1 0> | 168.6 |
GaN (mp-804) | <0 0 1> | <0 1 0> | 105.4 |
GaN (mp-804) | <1 0 1> | <0 1 0> | 210.8 |
GaN (mp-804) | <1 1 0> | <0 1 0> | 147.6 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 298.6 |
LiNbO3 (mp-3731) | <0 0 1> | <0 1 0> | 210.8 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 337.3 |
SiO2 (mp-6930) | <1 0 0> | <0 1 0> | 84.3 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 97.3 |
KCl (mp-23193) | <1 0 0> | <0 1 0> | 316.2 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 196.8 |
MoS2 (mp-1434) | <0 0 1> | <0 1 0> | 105.4 |
MoS2 (mp-1434) | <1 1 0> | <0 1 0> | 231.9 |
DyScO3 (mp-31120) | <0 0 1> | <0 1 0> | 63.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 1 0> | 274.0 |
DyScO3 (mp-31120) | <0 1 1> | <0 1 0> | 168.6 |
Al (mp-134) | <1 0 0> | <0 1 0> | 63.2 |
Al (mp-134) | <1 1 0> | <0 1 0> | 231.9 |
Al (mp-134) | <1 1 1> | <0 1 0> | 274.0 |
DyScO3 (mp-31120) | <1 0 0> | <0 1 0> | 274.0 |
DyScO3 (mp-31120) | <1 0 1> | <0 1 0> | 105.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 194.5 |
InAs (mp-20305) | <1 0 0> | <0 1 0> | 316.2 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 328.1 |
InAs (mp-20305) | <1 1 1> | <0 1 0> | 337.3 |
LiGaO2 (mp-5854) | <0 0 1> | <0 1 0> | 84.3 |
LiGaO2 (mp-5854) | <0 1 0> | <0 1 0> | 295.1 |
LiGaO2 (mp-5854) | <1 0 0> | <0 1 0> | 105.4 |
LiGaO2 (mp-5854) | <1 0 1> | <0 1 0> | 231.9 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 337.3 |
ZnSe (mp-1190) | <1 0 0> | <0 1 0> | 63.2 |
ZnSe (mp-1190) | <1 1 0> | <0 1 0> | 231.9 |
KTaO3 (mp-3614) | <1 0 0> | <0 1 0> | 63.2 |
KTaO3 (mp-3614) | <1 1 0> | <0 1 0> | 231.9 |
KTaO3 (mp-3614) | <1 1 1> | <0 1 0> | 274.0 |
CdTe (mp-406) | <1 0 0> | <0 1 0> | 274.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 196.8 |
CdS (mp-672) | <1 1 0> | <0 1 0> | 337.3 |
TeO2 (mp-2125) | <0 0 1> | <0 1 0> | 63.2 |
TeO2 (mp-2125) | <0 1 0> | <0 1 0> | 210.8 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KSrMg6 (mp-1099307) | 0.6303 | 0.237 | 3 |
Nd2Mg (mp-976425) | 0.1446 | 0.014 | 2 |
Gd2Mg (mp-865078) | 0.1333 | 0.016 | 2 |
Dy2Mg (mp-864888) | 0.2365 | 0.006 | 2 |
Y2Mg (mp-865583) | 0.1684 | 0.007 | 2 |
SrMg (mp-1094880) | 0.3407 | 0.038 | 2 |
Mn (mp-542909) | 0.7154 | 0.053 | 1 |
W (mp-1065340) | 0.6818 | 0.491 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sm_3 Mg_pv |
Final Energy/Atom-3.7354 eV |
Corrected Energy-22.4123 eV
-22.4123 eV = -22.4123 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)