Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.592 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.603 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.58 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToSb7Mo3 + Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 1> | 261.6 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 251.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 213.6 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 251.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 251.7 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 142.4 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 201.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 213.6 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 261.6 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 87.2 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 213.6 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 201.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 251.7 |
ZnSe (mp-1190) | <1 1 1> | <1 1 0> | 284.8 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 251.7 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 151.0 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 142.4 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 284.8 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 50.3 |
YVO4 (mp-19133) | <1 1 1> | <1 0 0> | 251.7 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 213.6 |
BN (mp-984) | <0 0 1> | <1 1 1> | 87.2 |
BN (mp-984) | <1 0 0> | <1 0 0> | 151.0 |
BN (mp-984) | <1 1 0> | <1 1 1> | 261.6 |
Al (mp-134) | <1 1 1> | <1 1 1> | 87.2 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 251.7 |
Fe3O4 (mp-19306) | <1 1 0> | <1 1 0> | 213.6 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 284.8 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 201.4 |
C (mp-66) | <1 0 0> | <1 0 0> | 50.3 |
C (mp-66) | <1 1 1> | <1 1 1> | 87.2 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 284.8 |
GdScO3 (mp-5690) | <0 1 1> | <1 1 0> | 284.8 |
GdScO3 (mp-5690) | <1 0 1> | <1 1 1> | 174.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 251.7 |
Mg (mp-153) | <1 1 1> | <1 0 0> | 251.7 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 151.0 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 151.0 |
KP(HO2)2 (mp-23959) | <0 1 1> | <1 1 0> | 213.6 |
LaF3 (mp-905) | <1 0 0> | <1 1 0> | 213.6 |
PbS (mp-21276) | <1 1 0> | <1 1 0> | 213.6 |
PbS (mp-21276) | <1 1 1> | <1 1 1> | 261.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 251.7 |
InP (mp-20351) | <1 1 0> | <1 1 0> | 142.4 |
InP (mp-20351) | <1 1 1> | <1 0 0> | 302.0 |
TbScO3 (mp-31119) | <0 0 1> | <1 1 0> | 284.8 |
TbScO3 (mp-31119) | <0 1 1> | <1 1 0> | 213.6 |
TbScO3 (mp-31119) | <1 1 0> | <1 0 0> | 251.7 |
Ni (mp-23) | <1 1 1> | <1 0 0> | 251.7 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 201.4 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbPrRh2 (mp-980069) | 0.0000 | 0.009 | 3 |
Er2NiIr (mp-862992) | 0.0000 | 0.011 | 3 |
Mn2AlRe (mp-864989) | 0.0000 | 0.000 | 3 |
GdCdAu2 (mp-866167) | 0.0000 | 0.000 | 3 |
ScCdHg2 (mp-867263) | 0.0000 | 0.000 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
MnFeCoGe (mp-1018024) | 0.0000 | 0.344 | 4 |
VGaFeCo (mp-1066581) | 0.0000 | 0.029 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
K3Zr (mp-973265) | 0.0000 | 0.980 | 2 |
RePb3 (mp-974611) | 0.0000 | 1.029 | 2 |
Li3Tc (mp-976334) | 0.0000 | 0.614 | 2 |
Tc3H (mp-972237) | 0.0000 | 0.676 | 2 |
PrW3 (mp-975787) | 0.0000 | 0.765 | 2 |
Xe (mp-979285) | 0.0000 | 0.002 | 1 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.340 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Sb Mo_pv |
Final Energy/Atom-5.2165 eV |
Corrected Energy-20.8660 eV
-20.8660 eV = -20.8660 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)