Final Magnetic Moment0.071 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.381 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.021 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density5.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLuAl3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 0 0> | 199.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 170.9 |
AlN (mp-661) | <1 1 0> | <0 0 1> | 162.7 |
CeO2 (mp-20194) | <1 1 0> | <1 1 1> | 177.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 97.6 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 1> | 295.5 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 227.8 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 370.3 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 227.8 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 113.9 |
AlN (mp-661) | <1 0 1> | <1 0 0> | 142.4 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 227.8 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 370.3 |
CeO2 (mp-20194) | <1 1 1> | <1 0 0> | 313.3 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 216.2 |
GaN (mp-804) | <1 1 0> | <1 1 1> | 59.1 |
SiO2 (mp-6930) | <1 1 0> | <1 1 1> | 295.5 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 292.8 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 246.7 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 1> | 177.3 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 113.9 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 177.3 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 130.1 |
GaN (mp-804) | <1 1 1> | <1 0 0> | 284.9 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 370.3 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 284.9 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 260.3 |
KCl (mp-23193) | <1 0 0> | <1 1 0> | 296.0 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 296.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 0> | 313.3 |
CdS (mp-672) | <0 0 1> | <1 0 0> | 170.9 |
LiF (mp-1138) | <1 0 0> | <1 0 1> | 346.0 |
LiF (mp-1138) | <1 1 0> | <1 0 1> | 346.0 |
InAs (mp-20305) | <1 1 0> | <0 0 1> | 260.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 227.8 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 197.4 |
Te2W (mp-22693) | <0 1 0> | <1 0 1> | 216.2 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 1> | 346.0 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 345.4 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 256.4 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 313.3 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 162.7 |
Te2W (mp-22693) | <1 1 0> | <1 0 1> | 216.2 |
Ag (mp-124) | <1 0 0> | <0 0 1> | 260.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 1> | 302.7 |
TePb (mp-19717) | <1 0 0> | <1 1 0> | 296.0 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 227.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 142.4 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 32.5 |
Te2Mo (mp-602) | <1 0 0> | <1 0 1> | 216.2 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
RbMg6Zr (mp-1022554) | 0.2446 | 0.263 | 3 |
TmAl3 (mp-979040) | 0.1030 | 0.012 | 2 |
Li3Dy (mp-977188) | 0.1441 | 0.213 | 2 |
SmAg3 (mp-972557) | 0.1367 | 0.036 | 2 |
CeAg3 (mp-862709) | 0.0807 | 0.039 | 2 |
SrMg3 (mp-1094338) | 0.1265 | 0.061 | 2 |
Tl (mp-972351) | 0.7107 | 0.000 | 1 |
Mn (mp-542909) | 0.6261 | 0.053 | 1 |
Hg (mp-569360) | 0.6980 | 0.001 | 1 |
W (mp-1065340) | 0.5403 | 0.491 | 1 |
Cs (mp-1012110) | 0.6117 | 0.046 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Al |
Final Energy/Atom-4.3203 eV |
Corrected Energy-34.5628 eV
-34.5628 eV = -34.5628 eV (uncorrected energy)
|