Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.678 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.057 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density11.76 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNdIr2 + Nd5Ir3 + NdAu |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <1 1 0> | 298.3 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 158.2 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 223.7 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 274.0 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 263.6 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 223.7 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 210.9 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 149.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 210.9 |
LiF (mp-1138) | <1 1 1> | <1 0 0> | 263.6 |
Te2W (mp-22693) | <1 1 0> | <1 1 0> | 223.7 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 52.7 |
YVO4 (mp-19133) | <1 0 0> | <1 0 0> | 316.4 |
YVO4 (mp-19133) | <1 0 1> | <1 0 0> | 210.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 210.9 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 263.6 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 223.7 |
Te2Mo (mp-602) | <1 0 1> | <1 1 0> | 223.7 |
Ag (mp-124) | <1 1 0> | <1 1 0> | 74.6 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 91.3 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 1 1> | 274.0 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 263.6 |
BN (mp-984) | <0 0 1> | <1 0 0> | 263.6 |
BN (mp-984) | <1 0 0> | <1 0 0> | 158.2 |
BN (mp-984) | <1 1 0> | <1 1 1> | 274.0 |
MoS2 (mp-1434) | <0 0 1> | <1 1 1> | 274.0 |
Al (mp-134) | <1 0 0> | <1 0 0> | 210.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 1 0> | 223.7 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 263.6 |
LiGaO2 (mp-5854) | <0 1 1> | <1 0 0> | 263.6 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 263.6 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 210.9 |
MgO (mp-1265) | <1 1 0> | <1 1 0> | 74.6 |
MgO (mp-1265) | <1 1 1> | <1 1 1> | 91.3 |
TiO2 (mp-2657) | <0 0 1> | <1 0 0> | 105.5 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 316.4 |
C (mp-66) | <1 1 1> | <1 0 0> | 263.6 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 298.3 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 263.6 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 263.6 |
Mg (mp-153) | <0 0 1> | <1 1 1> | 274.0 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 263.6 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 223.7 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 223.7 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 263.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 263.6 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 316.4 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 263.6 |
KP(HO2)2 (mp-23959) | <0 0 1> | <1 0 0> | 158.2 |
KP(HO2)2 (mp-23959) | <0 1 0> | <1 0 0> | 158.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
128 | 64 | 64 | 0 | 0 | 0 |
64 | 128 | 64 | 0 | 0 | 0 |
64 | 64 | 128 | 0 | 0 | 0 |
0 | 0 | 0 | 22 | 0 | 0 |
0 | 0 | 0 | 0 | 22 | 0 |
0 | 0 | 0 | 0 | 0 | 22 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
11.8 | -4 | -4 | 0 | 0 | 0 |
-4 | 11.8 | -4 | 0 | 0 | 0 |
-4 | -4 | 11.8 | 0 | 0 | 0 |
0 | 0 | 0 | 45.3 | 0 | 0 |
0 | 0 | 0 | 0 | 45.3 | 0 |
0 | 0 | 0 | 0 | 0 | 45.3 |
Shear Modulus GV26 GPa |
Bulk Modulus KV86 GPa |
Shear Modulus GR25 GPa |
Bulk Modulus KR86 GPa |
Shear Modulus GVRH26 GPa |
Bulk Modulus KVRH86 GPa |
Elastic Anisotropy0.16 |
Poisson's Ratio0.36 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
HoTmZn2 (mp-983126) | 0.0000 | 0.000 | 3 |
Pm2PtAu (mp-982772) | 0.0000 | 0.000 | 3 |
YbPrPd2 (mp-981530) | 0.0000 | 0.011 | 3 |
YTmAl2 (mp-980662) | 0.0000 | 0.016 | 3 |
YbPbAu2 (mp-980054) | 0.0000 | 0.000 | 3 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
VFeCoSb (mp-1066862) | 0.0000 | 0.163 | 4 |
ErPd (mp-851) | 0.0000 | 0.000 | 2 |
YbRu (mp-567116) | 0.0000 | 0.294 | 2 |
PrIn (mp-20023) | 0.0000 | 0.000 | 2 |
ReC (mp-1009731) | 0.0000 | 1.115 | 2 |
ScCu (mp-1169) | 0.0000 | 0.000 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Nd_3 Ir Au |
Final Energy/Atom-6.0903 eV |
Corrected Energy-24.3613 eV
-24.3613 eV = -24.3613 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)