Final Magnetic Moment0.001 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-1.017 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.100 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density8.41 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLu2Te3 + Te |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP4/nmm [129] |
HallP 4ab 2ab 1ab |
Point Group4/mmm |
Crystal Systemtetragonal |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 0> | <0 0 1> | 292.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 136.5 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 215.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 307.9 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 153.9 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 163.3 |
GaAs (mp-2534) | <1 0 0> | <0 0 1> | 156.0 |
GaN (mp-804) | <0 0 1> | <1 0 1> | 215.7 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 217.7 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 272.1 |
SiO2 (mp-6930) | <0 0 1> | <1 0 0> | 153.9 |
SiO2 (mp-6930) | <1 0 0> | <1 0 1> | 215.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 156.0 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 39.0 |
DyScO3 (mp-31120) | <0 0 1> | <1 0 1> | 345.2 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 253.5 |
DyScO3 (mp-31120) | <0 1 1> | <1 0 1> | 215.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 1> | 172.6 |
DyScO3 (mp-31120) | <1 1 0> | <0 0 1> | 253.5 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 215.7 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 39.0 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 54.4 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 195.0 |
ZnSe (mp-1190) | <1 0 0> | <0 0 1> | 156.0 |
KTaO3 (mp-3614) | <1 0 0> | <0 0 1> | 78.0 |
KTaO3 (mp-3614) | <1 1 0> | <1 0 1> | 345.2 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 231.3 |
CdS (mp-672) | <1 0 0> | <0 0 1> | 253.5 |
CdS (mp-672) | <1 0 1> | <1 1 1> | 289.1 |
CdS (mp-672) | <1 1 1> | <1 0 1> | 215.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 153.9 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 217.7 |
AlN (mp-661) | <1 0 0> | <0 0 1> | 214.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 214.5 |
Te2W (mp-22693) | <0 0 1> | <1 1 0> | 108.9 |
BaF2 (mp-1029) | <1 0 0> | <0 0 1> | 39.0 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 54.4 |
BaF2 (mp-1029) | <1 1 1> | <1 0 0> | 269.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 253.5 |
YVO4 (mp-19133) | <1 0 0> | <1 1 1> | 231.3 |
YVO4 (mp-19133) | <1 0 1> | <1 0 1> | 215.7 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 195.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 326.6 |
GaN (mp-804) | <1 1 1> | <0 0 1> | 156.0 |
TePb (mp-19717) | <1 0 0> | <1 1 1> | 173.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 192.4 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 172.6 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 97.5 |
Te2Mo (mp-602) | <1 1 1> | <0 0 1> | 97.5 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 153.9 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
90 | 64 | 30 | 0 | 0 | 0 |
64 | 90 | 30 | 0 | 0 | 0 |
30 | 30 | 118 | 0 | 0 | 0 |
0 | 0 | 0 | 24 | 0 | 0 |
0 | 0 | 0 | 0 | 24 | 0 |
0 | 0 | 0 | 0 | 0 | 12 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
23.4 | -16.2 | -1.8 | 0 | 0 | 0 |
-16.2 | 23.4 | -1.8 | 0 | 0 | 0 |
-1.8 | -1.8 | 9.4 | 0 | 0 | 0 |
0 | 0 | 0 | 42 | 0 | 0 |
0 | 0 | 0 | 0 | 42 | 0 |
0 | 0 | 0 | 0 | 0 | 85 |
Shear Modulus GV23 GPa |
Bulk Modulus KV61 GPa |
Shear Modulus GR19 GPa |
Bulk Modulus KR61 GPa |
Shear Modulus GVRH21 GPa |
Bulk Modulus KVRH61 GPa |
Elastic Anisotropy1.34 |
Poisson's Ratio0.34 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZrVSi (mp-5541) | 0.2380 | 0.000 | 3 |
ThAsSe (mp-1019357) | 0.1777 | 0.000 | 3 |
ThSbTe (mp-1019361) | 0.2141 | 0.000 | 3 |
HfVSi (mp-1018720) | 0.2387 | 0.000 | 3 |
ThPS (mp-12876) | 0.1951 | 0.000 | 3 |
HoTe2 (mp-1018732) | 0.0689 | 0.058 | 2 |
ErTe2 (mp-1018692) | 0.0657 | 0.068 | 2 |
DyTe2 (mp-1018679) | 0.0813 | 0.047 | 2 |
TmTe2 (mp-1072729) | 0.0300 | 0.078 | 2 |
YTe2 (mp-1077365) | 0.0894 | 0.050 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Lu_3 Te |
Final Energy/Atom-4.6198 eV |
Corrected Energy-27.7189 eV
-27.7189 eV = -27.7189 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)