Final Magnetic Moment0.336 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.531 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.012 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density10.08 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToHfAl2 + Al2Os + HfOs |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Topological ClassificationSM*
|
SubclassificationESFD†
|
Crossing TypePoint
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 151.6 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 151.6 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 151.6 |
GaP (mp-2490) | <1 0 0> | <1 0 0> | 151.6 |
PbSe (mp-2201) | <1 0 0> | <1 0 0> | 151.6 |
BaTiO3 (mp-5986) | <1 0 0> | <1 0 0> | 151.6 |
Ga2O3 (mp-886) | <1 0 -1> | <1 0 0> | 151.6 |
Si (mp-149) | <1 0 0> | <1 0 0> | 151.6 |
CdSe (mp-2691) | <1 0 0> | <1 0 0> | 151.6 |
Y3Fe5O12 (mp-19648) | <1 0 0> | <1 0 0> | 151.6 |
GaSb (mp-1156) | <1 0 0> | <1 0 0> | 151.6 |
CaF2 (mp-2741) | <1 0 0> | <1 0 0> | 151.6 |
ZnTe (mp-2176) | <1 0 0> | <1 0 0> | 151.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Na6Cd16Au7 (mp-982883) | 0.1228 | 0.000 | 3 |
Sc6Al16Ir7 (mp-978662) | 0.1005 | 0.000 | 3 |
Ta6Co16Ge7 (mp-672652) | 0.1900 | 0.000 | 3 |
Zr6Al16Ru7 (mp-866136) | 0.0491 | 0.000 | 3 |
Nb6Co16Ge7 (mp-580140) | 0.1913 | 0.000 | 3 |
Yb6Fe23 (mp-669649) | 0.3628 | 0.074 | 2 |
Zr6Co23 (mp-30569) | 0.3459 | 0.000 | 2 |
Sr6Mg23 (mp-30782) | 0.3712 | 0.000 | 2 |
Er6Fe23 (mp-2162) | 0.3626 | 0.139 | 2 |
Ho6Fe23 (mp-2759) | 0.3713 | 0.011 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Hf_pv Al Os_pv |
Final Energy/Atom-7.3679 eV |
Corrected Energy-213.6677 eV
-213.6677 eV = -213.6677 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)