Final Magnetic Moment0.003 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.187 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.019 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density4.62 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToLaAl + Li + La |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 248.5 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 58.6 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 292.8 |
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 101.4 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 292.8 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 101.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 234.3 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 82.8 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 165.7 |
GaN (mp-804) | <0 0 1> | <1 1 0> | 248.5 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 248.5 |
SiO2 (mp-6930) | <1 1 1> | <1 1 0> | 165.7 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 165.7 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 248.5 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 175.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 292.8 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 165.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 292.8 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 292.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 248.5 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 292.8 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 248.5 |
Te2Mo (mp-602) | <0 0 1> | <1 0 0> | 292.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 0> | 165.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 292.8 |
BN (mp-984) | <0 0 1> | <1 0 0> | 234.3 |
BN (mp-984) | <1 0 0> | <1 0 0> | 58.6 |
BN (mp-984) | <1 1 0> | <1 1 0> | 165.7 |
BN (mp-984) | <1 1 1> | <1 0 0> | 234.3 |
MoS2 (mp-1434) | <0 0 1> | <1 0 0> | 175.7 |
Al (mp-134) | <1 0 0> | <1 0 0> | 292.8 |
Al (mp-134) | <1 1 0> | <1 1 0> | 248.5 |
LiGaO2 (mp-5854) | <1 0 1> | <1 0 0> | 175.7 |
LiGaO2 (mp-5854) | <1 1 0> | <1 1 0> | 248.5 |
CdTe (mp-406) | <1 1 0> | <1 1 0> | 248.5 |
TeO2 (mp-2125) | <0 0 1> | <1 0 0> | 292.8 |
SiC (mp-7631) | <1 0 0> | <1 0 0> | 234.3 |
SiC (mp-7631) | <1 0 1> | <1 0 0> | 234.3 |
Fe3O4 (mp-19306) | <1 0 0> | <1 0 0> | 292.8 |
MgO (mp-1265) | <1 0 0> | <1 0 0> | 234.3 |
Ge3(BiO3)4 (mp-23560) | <1 0 0> | <1 0 0> | 117.1 |
Ge3(BiO3)4 (mp-23560) | <1 1 0> | <1 1 0> | 165.7 |
C (mp-66) | <1 0 0> | <1 0 0> | 117.1 |
C (mp-66) | <1 1 0> | <1 1 0> | 165.7 |
GdScO3 (mp-5690) | <0 0 1> | <1 1 0> | 248.5 |
GdScO3 (mp-5690) | <0 1 0> | <1 0 0> | 175.7 |
YAlO3 (mp-3792) | <0 1 0> | <1 0 0> | 117.1 |
YAlO3 (mp-3792) | <1 1 0> | <1 0 0> | 58.6 |
TiO2 (mp-390) | <0 0 1> | <1 0 0> | 58.6 |
Mg (mp-153) | <0 0 1> | <1 0 0> | 175.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
56 | 34 | 34 | 0 | 0 | 0 |
34 | 56 | 34 | 0 | 0 | 0 |
34 | 34 | 56 | 0 | 0 | 0 |
0 | 0 | 0 | 34 | 0 | 0 |
0 | 0 | 0 | 0 | 34 | 0 |
0 | 0 | 0 | 0 | 0 | 34 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
33.1 | -12.5 | -12.5 | 0 | 0 | 0 |
-12.5 | 33.1 | -12.5 | 0 | 0 | 0 |
-12.5 | -12.5 | 33.1 | 0 | 0 | 0 |
0 | 0 | 0 | 29.2 | 0 | 0 |
0 | 0 | 0 | 0 | 29.2 | 0 |
0 | 0 | 0 | 0 | 0 | 29.2 |
Shear Modulus GV25 GPa |
Bulk Modulus KV41 GPa |
Shear Modulus GR19 GPa |
Bulk Modulus KR41 GPa |
Shear Modulus GVRH22 GPa |
Bulk Modulus KVRH41 GPa |
Elastic Anisotropy1.72 |
Poisson's Ratio0.28 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
BaSrYb2 (mp-980191) | 0.0000 | 0.034 | 3 |
AcYbCd2 (mp-979962) | 0.0000 | 0.000 | 3 |
SmErHg2 (mp-972635) | 0.0000 | 0.000 | 3 |
SmAg2Sn (mp-862735) | 0.0000 | 0.044 | 3 |
LiDy2Ru (mp-867111) | 0.0000 | 0.000 | 3 |
VFeCoGe (mp-1063914) | 0.0000 | 0.000 | 4 |
TiFeCoSb (mp-998973) | 0.0000 | 0.186 | 4 |
TiAlFeCo (mp-998980) | 0.0000 | 0.000 | 4 |
TiFeCoGe (mp-1018012) | 0.0000 | 0.028 | 4 |
VFeCoSi (mp-1066609) | 0.0000 | 0.002 | 4 |
Y3Sn (mp-1094256) | 0.0000 | 0.278 | 2 |
Rb3V (mp-974743) | 0.0000 | 0.925 | 2 |
Rb3Hg (mp-974990) | 0.0000 | 0.069 | 2 |
Mg3Sb (mp-1094520) | 0.0000 | 0.197 | 2 |
Mg3Cd (mp-1038832) | 0.0000 | 0.056 | 2 |
Cu (mp-998890) | 0.0000 | 0.037 | 1 |
Kr (mp-974400) | 0.0000 | 0.002 | 1 |
H2 (mp-632250) | 0.0000 | 0.000 | 1 |
Ge (mp-998883) | 0.0000 | 0.339 | 1 |
U (mp-108) | 0.0000 | 0.269 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Li_sv La Al |
Final Energy/Atom-4.0683 eV |
Corrected Energy-16.2733 eV
-16.2733 eV = -16.2733 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)