Final Magnetic Moment0.485 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingFM |
Formation Energy / Atom0.134 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.209 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToNi + NiI2 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63mc [186] |
HallP 6c 2c |
Point Group6mm |
Crystal Systemhexagonal |
sign indicates spin ↑ ↓
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 227.9 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 57.0 |
AlN (mp-661) | <1 1 0> | <1 0 1> | 250.4 |
CeO2 (mp-20194) | <1 1 0> | <0 0 1> | 284.9 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 57.0 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 213.7 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 213.7 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 241.4 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 195.1 |
KCl (mp-23193) | <1 0 0> | <1 1 1> | 201.3 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 270.6 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 223.0 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 185.2 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 144.8 |
CdS (mp-672) | <1 0 1> | <1 0 0> | 195.1 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 195.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 83.6 |
LiF (mp-1138) | <1 1 0> | <0 0 1> | 114.0 |
LiF (mp-1138) | <1 1 1> | <0 0 1> | 270.6 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 199.4 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 213.7 |
Te2W (mp-22693) | <0 1 1> | <1 1 0> | 241.4 |
YVO4 (mp-19133) | <0 0 1> | <0 0 1> | 256.4 |
YVO4 (mp-19133) | <1 0 0> | <0 0 1> | 185.2 |
YVO4 (mp-19133) | <1 0 1> | <0 0 1> | 199.4 |
YVO4 (mp-19133) | <1 1 1> | <1 0 1> | 250.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 227.9 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 42.7 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 213.7 |
Te2Mo (mp-602) | <1 0 1> | <0 0 1> | 213.7 |
Ag (mp-124) | <1 0 0> | <1 0 0> | 83.6 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 139.4 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 270.6 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 227.9 |
GaSe (mp-1943) | <0 0 1> | <1 0 0> | 167.2 |
GaSe (mp-1943) | <1 0 0> | <1 0 1> | 281.7 |
BN (mp-984) | <0 0 1> | <1 0 0> | 167.2 |
BN (mp-984) | <1 0 0> | <1 0 1> | 156.5 |
BN (mp-984) | <1 0 1> | <1 1 1> | 100.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 270.6 |
BN (mp-984) | <1 1 1> | <1 0 1> | 313.0 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 99.7 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 139.4 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 242.1 |
AlN (mp-661) | <1 1 1> | <1 0 1> | 250.4 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 299.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 167.2 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 227.9 |
BaF2 (mp-1029) | <1 0 0> | <1 1 0> | 193.1 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 270.6 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2GeSe4 (mvc-16079) | 0.1119 | 0.003 | 4 |
CoSi(CuS2)2 (mp-11769) | 0.0922 | 0.074 | 4 |
MnAg2GeTe4 (mp-1025568) | 0.1055 | 0.007 | 4 |
FeSi(CuSe2)2 (mp-1025510) | 0.1029 | 0.055 | 4 |
CoCu2GeS4 (mp-6498) | 0.1101 | 0.061 | 4 |
HgN (mp-973674) | 0.0624 | 1.404 | 2 |
ZnN (mp-971911) | 0.0318 | 0.473 | 2 |
PbN (mp-973785) | 0.0278 | 0.644 | 2 |
NiN (mp-973933) | 0.0767 | 0.307 | 2 |
ZnTe (mp-571195) | 0.0845 | 0.003 | 2 |
BC2N (mp-30148) | 0.0916 | 0.542 | 3 |
Si3NiP4 (mp-8311) | 0.0932 | 0.000 | 3 |
AlGaN2 (mp-1008556) | 0.1046 | 0.016 | 3 |
CrGaP2 (mp-1018079) | 0.1044 | 0.389 | 3 |
InAgSe2 (mp-20554) | 0.1005 | 0.000 | 3 |
Ge (mp-1007760) | 0.1158 | 0.020 | 1 |
C (mp-47) | 0.1078 | 0.160 | 1 |
C (mp-611426) | 0.1252 | 0.145 | 1 |
C (mp-66) | 0.1277 | 0.136 | 1 |
Si (mp-165) | 0.1112 | 0.011 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-points30 |
U Values-- |
PseudopotentialsVASP PAW: Ni_pv I |
Final Energy/Atom-3.5144 eV |
Corrected Energy-14.0575 eV
-14.0575 eV = -14.0575 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)