Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-2.441 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.033 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density6.93 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToTm2S3 |
Band Gap0.656 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPnma [62] |
Hall-P 2ac 2n |
Point Groupmmm |
Crystal Systemorthorhombic |
Topological ClassificationTI*
|
SubclassificationNLC†
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <0 0 1> | <0 1 1> | 281.5 |
AlN (mp-661) | <1 0 0> | <0 1 1> | 281.5 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 197.9 |
AlN (mp-661) | <1 1 0> | <1 1 1> | 245.6 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 116.2 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 316.7 |
GaAs (mp-2534) | <1 1 0> | <0 1 1> | 281.5 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 197.9 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 316.7 |
GaN (mp-804) | <1 1 0> | <1 0 1> | 116.1 |
SiO2 (mp-6930) | <0 0 1> | <0 1 0> | 320.2 |
SiO2 (mp-6930) | <1 0 0> | <1 1 1> | 245.6 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 316.7 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 158.3 |
InAs (mp-20305) | <1 1 0> | <0 1 0> | 160.1 |
ZnSe (mp-1190) | <1 1 0> | <0 1 1> | 281.5 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 232.5 |
CdS (mp-672) | <1 0 0> | <0 1 0> | 320.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 158.3 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 218.3 |
LiF (mp-1138) | <1 1 0> | <0 1 1> | 281.5 |
Te2W (mp-22693) | <0 0 1> | <0 0 1> | 197.9 |
Te2W (mp-22693) | <0 1 0> | <0 0 1> | 158.3 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 109.1 |
YVO4 (mp-19133) | <1 0 0> | <0 1 1> | 281.5 |
YVO4 (mp-19133) | <1 0 1> | <0 1 1> | 281.5 |
YVO4 (mp-19133) | <1 1 0> | <0 0 1> | 197.9 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 218.3 |
TePb (mp-19717) | <1 1 0> | <0 0 1> | 118.8 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 197.9 |
Te2Mo (mp-602) | <1 0 0> | <0 0 1> | 158.3 |
Ag (mp-124) | <1 0 0> | <0 1 1> | 225.2 |
Ag (mp-124) | <1 1 0> | <1 0 0> | 218.3 |
Ag (mp-124) | <1 1 1> | <0 0 1> | 118.8 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 1 1> | 225.2 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 197.9 |
GaSe (mp-1943) | <1 0 0> | <0 0 1> | 197.9 |
GaSe (mp-1943) | <1 0 1> | <0 0 1> | 277.1 |
BN (mp-984) | <0 0 1> | <1 1 1> | 245.6 |
BN (mp-984) | <1 0 0> | <0 0 1> | 316.7 |
BN (mp-984) | <1 1 0> | <0 0 1> | 237.5 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 277.1 |
LiNbO3 (mp-3731) | <1 0 1> | <0 1 1> | 225.2 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 277.1 |
Al (mp-134) | <1 1 0> | <0 1 1> | 281.5 |
LiGaO2 (mp-5854) | <0 0 1> | <0 0 1> | 277.1 |
LiGaO2 (mp-5854) | <0 1 0> | <0 0 1> | 197.9 |
LiGaO2 (mp-5854) | <0 1 1> | <0 0 1> | 356.3 |
LiGaO2 (mp-5854) | <1 1 0> | <0 1 0> | 240.2 |
CdTe (mp-406) | <1 0 0> | <1 0 0> | 218.3 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Hf2N2O (mp-755911) | 0.3889 | 0.108 | 3 |
Zr2N2O (mp-755576) | 0.3622 | 0.087 | 3 |
Zr2N2O (mp-756054) | 0.3274 | 0.112 | 3 |
Zr2N2O (mp-776235) | 0.6085 | 0.090 | 3 |
Y2HfS5 (mp-16919) | 0.5837 | 0.014 | 3 |
Tb2S3 (mp-9323) | 0.0713 | 0.000 | 2 |
Dy2Se3 (mp-7368) | 0.0824 | 0.000 | 2 |
Ho2S3 (mp-8956) | 0.0415 | 0.008 | 2 |
Dy2S3 (mp-1270) | 0.0563 | 0.000 | 2 |
Tb2Se3 (mp-15257) | 0.0927 | 0.000 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Tm_3 S |
Final Energy/Atom-6.3152 eV |
Corrected Energy-134.2647 eV
-134.2647 eV = -126.3031 eV (uncorrected energy) - 7.9615 eV (MP Anion Correction)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)