Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.545 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density9.98 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP63/mmc [194] |
Hall-P 6c 2c |
Point Group6/mmm |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
TePb (mp-19717) | <1 1 0> | <0 0 1> | 300.4 |
TePb (mp-19717) | <1 1 1> | <0 0 1> | 75.1 |
Te2Mo (mp-602) | <0 0 1> | <0 0 1> | 75.1 |
Bi2Te3 (mp-34202) | <0 0 1> | <0 0 1> | 225.3 |
GaSe (mp-1943) | <0 0 1> | <0 0 1> | 325.5 |
BN (mp-984) | <0 0 1> | <0 0 1> | 300.4 |
BN (mp-984) | <1 0 0> | <0 0 1> | 325.5 |
BN (mp-984) | <1 0 1> | <0 0 1> | 225.3 |
LiNbO3 (mp-3731) | <0 0 1> | <0 0 1> | 25.0 |
Bi2Se3 (mp-541837) | <0 0 1> | <0 0 1> | 175.3 |
MoS2 (mp-1434) | <0 0 1> | <0 0 1> | 225.3 |
MoS2 (mp-1434) | <1 0 0> | <0 0 1> | 200.3 |
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 25.0 |
LaAlO3 (mp-2920) | <1 0 0> | <1 0 0> | 287.9 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 75.1 |
LaAlO3 (mp-2920) | <1 1 1> | <0 0 1> | 125.2 |
Al (mp-134) | <1 1 1> | <0 0 1> | 325.5 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 25.0 |
AlN (mp-661) | <1 1 0> | <1 0 0> | 191.9 |
AlN (mp-661) | <1 1 1> | <0 0 1> | 200.3 |
CeO2 (mp-20194) | <1 0 0> | <0 0 1> | 150.2 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 287.9 |
LiGaO2 (mp-5854) | <0 0 1> | <1 0 0> | 191.9 |
LiGaO2 (mp-5854) | <1 0 0> | <0 0 1> | 250.4 |
CdTe (mp-406) | <1 0 0> | <0 0 1> | 225.3 |
CdTe (mp-406) | <1 1 0> | <0 0 1> | 300.4 |
CdTe (mp-406) | <1 1 1> | <0 0 1> | 75.1 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 175.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 175.3 |
GaN (mp-804) | <1 0 0> | <0 0 1> | 225.3 |
GaN (mp-804) | <1 1 0> | <0 0 1> | 150.2 |
SiC (mp-7631) | <0 0 1> | <0 0 1> | 25.0 |
SiC (mp-7631) | <1 1 0> | <0 0 1> | 250.4 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 300.4 |
SiO2 (mp-6930) | <1 0 0> | <1 0 0> | 191.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 96.0 |
LiTaO3 (mp-3666) | <0 0 1> | <0 0 1> | 300.4 |
KCl (mp-23193) | <1 0 0> | <0 0 1> | 125.2 |
KCl (mp-23193) | <1 1 0> | <0 0 1> | 300.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 75.1 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 150.2 |
MgO (mp-1265) | <1 1 1> | <0 0 1> | 225.3 |
DyScO3 (mp-31120) | <0 1 0> | <0 0 1> | 300.4 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 325.5 |
TiO2 (mp-2657) | <0 0 1> | <0 0 1> | 175.3 |
TiO2 (mp-2657) | <1 0 0> | <1 0 0> | 96.0 |
TiO2 (mp-2657) | <1 1 1> | <0 0 1> | 200.3 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 175.3 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 325.5 |
C (mp-66) | <1 0 0> | <1 0 0> | 191.9 |
A full elastic tensor has not been calculated for this material. Registered users can view statistical-learning-based predictions of this material's bulk and shear moduli.
Once you have registered you can also "vote" for full calculation of this material's elastic properties.
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
YbAl2Cu (mp-977428) | 0.3717 | 0.000 | 3 |
GdMg2Ni9 (mp-567249) | 0.3889 | 0.451 | 3 |
SmMg2Ni9 (mp-569494) | 0.4014 | 0.000 | 3 |
CaMg2Ni9 (mp-12695) | 0.3647 | 0.013 | 3 |
Ca3Al7Ag2 (mp-11430) | 0.3587 | 0.000 | 3 |
CeIr3 (mp-31100) | 0.0481 | 0.008 | 2 |
CeNi3 (mp-580354) | 0.0598 | 0.000 | 2 |
NdRh3 (mp-864699) | 0.0251 | 0.000 | 2 |
NdNi3 (mp-1095561) | 0.0442 | 0.000 | 2 |
LaRh3 (mp-569100) | 0.0517 | 0.020 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: La Rh_pv |
Final Energy/Atom-7.2831 eV |
Corrected Energy-174.7938 eV
-174.7938 eV = -174.7938 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)