Final Magnetic Moment0.002 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.016 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.005 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density14.28 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToPtRh3 |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinPm3m [221] |
Hall-P 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <1 1 1> | 26.1 |
LaAlO3 (mp-2920) | <1 0 0> | <1 1 0> | 149.4 |
LaAlO3 (mp-2920) | <1 0 1> | <1 0 0> | 75.4 |
LaAlO3 (mp-2920) | <1 1 0> | <1 1 0> | 128.0 |
AlN (mp-661) | <0 0 1> | <1 1 1> | 26.1 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 192.0 |
LaAlO3 (mp-2920) | <1 1 1> | <1 1 1> | 130.7 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 234.7 |
AlN (mp-661) | <1 0 1> | <1 1 0> | 106.7 |
AlN (mp-661) | <1 1 1> | <1 0 0> | 226.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 0> | 30.2 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 42.7 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 135.8 |
GaAs (mp-2534) | <1 1 1> | <1 1 1> | 235.2 |
CeO2 (mp-20194) | <1 1 1> | <1 1 0> | 256.0 |
GaAs (mp-2534) | <1 1 0> | <1 1 0> | 192.0 |
GaN (mp-804) | <1 1 0> | <1 1 0> | 85.3 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 75.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 170.7 |
GaN (mp-804) | <0 0 1> | <1 1 1> | 26.1 |
GaN (mp-804) | <1 0 0> | <1 1 0> | 149.4 |
GaN (mp-804) | <1 0 1> | <1 1 0> | 192.0 |
GaN (mp-804) | <1 1 1> | <1 1 1> | 209.1 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 339.7 |
DyScO3 (mp-31120) | <1 0 1> | <1 0 0> | 226.3 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 0> | 286.7 |
SiO2 (mp-6930) | <1 0 0> | <1 1 0> | 192.0 |
SiO2 (mp-6930) | <1 0 1> | <1 0 0> | 241.4 |
SiO2 (mp-6930) | <1 1 0> | <1 1 0> | 192.0 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 196.1 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 170.7 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 75.4 |
InAs (mp-20305) | <1 1 0> | <1 1 0> | 170.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 135.8 |
ZnSe (mp-1190) | <1 1 1> | <1 1 1> | 235.2 |
DyScO3 (mp-31120) | <0 0 1> | <1 1 0> | 64.0 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 42.7 |
DyScO3 (mp-31120) | <0 1 1> | <1 1 0> | 106.7 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 60.4 |
InAs (mp-20305) | <1 1 1> | <1 1 0> | 341.4 |
ZnSe (mp-1190) | <1 1 0> | <1 1 0> | 192.0 |
CdS (mp-672) | <1 0 1> | <1 1 0> | 298.7 |
CdS (mp-672) | <1 1 0> | <1 1 0> | 192.0 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 135.8 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 192.0 |
KTaO3 (mp-3614) | <1 1 1> | <1 0 0> | 226.3 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 192.0 |
CdS (mp-672) | <0 0 1> | <1 1 1> | 104.5 |
CdS (mp-672) | <1 0 0> | <1 1 0> | 234.7 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 135.8 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
396 | 212 | 212 | 0 | 0 | 0 |
212 | 396 | 212 | 0 | 0 | 0 |
212 | 212 | 396 | 0 | 0 | 0 |
0 | 0 | 0 | 150 | 0 | 0 |
0 | 0 | 0 | 0 | 150 | 0 |
0 | 0 | 0 | 0 | 0 | 150 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
4 | -1.4 | -1.4 | 0 | 0 | 0 |
-1.4 | 4 | -1.4 | 0 | 0 | 0 |
-1.4 | -1.4 | 4 | 0 | 0 | 0 |
0 | 0 | 0 | 6.6 | 0 | 0 |
0 | 0 | 0 | 0 | 6.6 | 0 |
0 | 0 | 0 | 0 | 0 | 6.6 |
Shear Modulus GV127 GPa |
Bulk Modulus KV273 GPa |
Shear Modulus GR120 GPa |
Bulk Modulus KR273 GPa |
Shear Modulus GVRH124 GPa |
Bulk Modulus KVRH273 GPa |
Elastic Anisotropy0.29 |
Poisson's Ratio0.30 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
ZnCu2Ni (mp-30593) | 0.1125 | 0.005 | 3 |
CrCoPt2 (mp-570863) | 0.0492 | 0.000 | 3 |
LiCa6Ge (mp-12609) | 0.0000 | 0.180 | 3 |
GaFeNi2 (mp-1065359) | 0.0412 | 0.066 | 3 |
GaCo2Ni (mp-1018060) | 0.0157 | 0.075 | 3 |
Cr8Ni50Mo15W2 (mp-767372) | 0.2155 | 0.028 | 4 |
CrFeCoNi (mp-1012640) | 0.3608 | 0.118 | 4 |
CrFeCoNi (mp-1096923) | 0.4019 | 0.193 | 4 |
MnBe3 (mp-973292) | 0.0000 | 0.010 | 2 |
Ho3Hg (mp-975256) | 0.0000 | 0.094 | 2 |
Hf3Au (mp-976725) | 0.0000 | 0.142 | 2 |
LiIn3 (mp-863027) | 0.0000 | 0.000 | 2 |
TaRu3 (mp-867816) | 0.0000 | 0.000 | 2 |
P (mp-674158) | 0.0000 | 3.518 | 1 |
Xe (mp-611517) | 0.0000 | 0.006 | 1 |
Eu (mp-623532) | 0.0000 | 0.035 | 1 |
He (mp-614456) | 0.0000 | 0.008 | 1 |
Au (mp-81) | 0.0000 | 0.000 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Pt Rh_pv |
Final Energy/Atom-7.0375 eV |
Corrected Energy-28.1498 eV
-28.1498 eV = -28.1498 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)