Final Magnetic Moment0.005 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom0.633 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.633 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density17.30 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToRe + Sb |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinFm3m [225] |
Hall-F 4 2 3 |
Point Groupm3m |
Crystal Systemcubic |
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
AlN (mp-661) | <1 0 1> | <1 0 0> | 286.1 |
CeO2 (mp-20194) | <1 1 1> | <1 1 1> | 212.4 |
BaF2 (mp-1029) | <1 1 0> | <1 1 0> | 57.8 |
GaN (mp-804) | <0 0 1> | <1 0 0> | 286.1 |
KCl (mp-23193) | <1 0 0> | <1 0 0> | 40.9 |
KCl (mp-23193) | <1 1 1> | <1 1 1> | 70.8 |
InAs (mp-20305) | <1 0 0> | <1 0 0> | 327.0 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 163.5 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 81.7 |
CdS (mp-672) | <0 0 1> | <1 1 0> | 231.2 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 81.7 |
Te2W (mp-22693) | <0 0 1> | <1 0 0> | 204.4 |
Te2W (mp-22693) | <1 0 0> | <1 1 0> | 289.0 |
YVO4 (mp-19133) | <0 0 1> | <1 0 0> | 204.4 |
TePb (mp-19717) | <1 0 0> | <1 0 0> | 40.9 |
Te2Mo (mp-602) | <1 1 0> | <1 1 1> | 283.2 |
Ag (mp-124) | <1 1 1> | <1 1 1> | 212.4 |
LiNbO3 (mp-3731) | <0 0 1> | <1 1 1> | 70.8 |
AlN (mp-661) | <0 0 1> | <1 0 0> | 204.4 |
AlN (mp-661) | <1 0 0> | <1 0 0> | 286.1 |
CeO2 (mp-20194) | <1 1 0> | <1 1 0> | 173.4 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 163.5 |
BaF2 (mp-1029) | <1 0 0> | <1 0 0> | 40.9 |
BaF2 (mp-1029) | <1 1 1> | <1 1 1> | 70.8 |
LiGaO2 (mp-5854) | <0 1 0> | <1 0 0> | 163.5 |
GaN (mp-804) | <1 0 0> | <1 0 0> | 204.4 |
SiO2 (mp-6930) | <0 0 1> | <1 1 1> | 283.2 |
KCl (mp-23193) | <1 1 0> | <1 1 0> | 57.8 |
TiO2 (mp-2657) | <0 0 1> | <1 1 0> | 173.4 |
TiO2 (mp-2657) | <1 1 0> | <1 1 0> | 57.8 |
TiO2 (mp-2657) | <1 1 1> | <1 1 0> | 57.8 |
DyScO3 (mp-31120) | <0 1 0> | <1 1 0> | 173.4 |
DyScO3 (mp-31120) | <1 1 0> | <1 0 0> | 327.0 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 204.4 |
C (mp-66) | <1 1 1> | <1 1 1> | 283.2 |
GdScO3 (mp-5690) | <0 1 0> | <1 1 0> | 173.4 |
GdScO3 (mp-5690) | <1 1 0> | <1 0 0> | 327.0 |
Te2W (mp-22693) | <1 0 1> | <1 0 0> | 204.4 |
YVO4 (mp-19133) | <1 0 0> | <1 1 0> | 231.2 |
YVO4 (mp-19133) | <1 1 0> | <1 0 0> | 327.0 |
TePb (mp-19717) | <1 1 0> | <1 1 0> | 57.8 |
TePb (mp-19717) | <1 1 1> | <1 1 1> | 70.8 |
Te2Mo (mp-602) | <1 0 0> | <1 1 1> | 283.2 |
Te2Mo (mp-602) | <1 0 1> | <1 1 1> | 283.2 |
Mg (mp-153) | <0 0 1> | <1 1 0> | 173.4 |
Mg (mp-153) | <1 0 0> | <1 0 0> | 204.4 |
Ag (mp-124) | <1 0 0> | <1 1 0> | 173.4 |
Bi2Te3 (mp-34202) | <0 0 1> | <1 0 0> | 204.4 |
BN (mp-984) | <0 0 1> | <1 1 1> | 70.8 |
LaF3 (mp-905) | <0 0 1> | <1 1 0> | 231.2 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
269 | 165 | 165 | 0 | 0 | 0 |
165 | 269 | 165 | 0 | 0 | 0 |
165 | 165 | 269 | 0 | 0 | 0 |
0 | 0 | 0 | 39 | 0 | 0 |
0 | 0 | 0 | 0 | 39 | 0 |
0 | 0 | 0 | 0 | 0 | 39 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
7 | -2.7 | -2.7 | 0 | 0 | 0 |
-2.7 | 7 | -2.7 | 0 | 0 | 0 |
-2.7 | -2.7 | 7 | 0 | 0 | 0 |
0 | 0 | 0 | 25.8 | 0 | 0 |
0 | 0 | 0 | 0 | 25.8 | 0 |
0 | 0 | 0 | 0 | 0 | 25.8 |
Shear Modulus GV44 GPa |
Bulk Modulus KV200 GPa |
Shear Modulus GR43 GPa |
Bulk Modulus KR200 GPa |
Shear Modulus GVRH44 GPa |
Bulk Modulus KVRH200 GPa |
Elastic Anisotropy0.10 |
Poisson's Ratio0.40 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
Zn2CuIr (mp-980665) | 0.0000 | 0.000 | 3 |
LiAcTe2 (mp-864755) | 0.0000 | 0.000 | 3 |
PrYMg2 (mp-861479) | 0.0000 | 0.000 | 3 |
NdMgCd2 (mp-866065) | 0.0000 | 0.000 | 3 |
Li2LaTl (mp-866195) | 0.0000 | 0.000 | 3 |
LiMgSnPd (mp-7555) | 0.0000 | 0.000 | 4 |
LiMgSnAu (mp-7554) | 0.0000 | 0.088 | 4 |
LiMgSbPt (mp-571584) | 0.0000 | 0.086 | 4 |
LiMgSbPd (mp-10179) | 0.0000 | 0.096 | 4 |
LiMgSnPt (mp-11806) | 0.0000 | 0.000 | 4 |
Ga3Au (mp-983412) | 0.0000 | 0.160 | 2 |
GaSi3 (mp-983359) | 0.0000 | 0.465 | 2 |
SmTa3 (mp-972514) | 0.0000 | 0.480 | 2 |
LiZn3 (mp-865907) | 0.0000 | 0.002 | 2 |
Mn3Ge (mp-865027) | 0.0000 | 0.000 | 2 |
Br (mp-673171) | 0.0000 | 0.630 | 1 |
Ti (mp-73) | 0.0000 | 0.112 | 1 |
I (mp-684663) | 0.0000 | 0.469 | 1 |
Cr (mp-90) | 0.0000 | 0.000 | 1 |
Bi (mp-568610) | 0.0000 | 0.136 | 1 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Re_pv Sb |
Final Energy/Atom-9.7331 eV |
Corrected Energy-38.9325 eV
-38.9325 eV = -38.9325 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)