Final Magnetic Moment0.000 μBCalculated total magnetic moment for the unit cell within the magnetic ordering provided (see below). Typically accurate to the second digit. |
Magnetic OrderingNM |
Formation Energy / Atom-0.128 eVCalculated formation energy from the elements normalized to per atom in the unit cell. |
Energy Above Hull / Atom0.000 eVThe energy of decomposition of this material into the set of most stable materials at this chemical composition, in eV/atom. Stability is tested against all potential chemical combinations that result in the material's composition. For example, a Co2O3 structure would be tested for decomposition against other Co2O3 structures, against Co and O2 mixtures, and against CoO and O2 mixtures. |
Density18.95 g/cm3The calculated bulk crystalline density, typically underestimated due calculated cell volumes overestimated on average by 3% (+/- 6%) |
Decomposes ToStable |
Band Gap0.000 eVIn general, band gaps computed with common exchange-correlation functionals such as the LDA and GGA are severely underestimated. Typically the disagreement is reported to be ~50% in the literature. Some internal testing by the Materials Project supports these statements; typically, we find that band gaps are underestimated by ~40%. We additionally find that several known insulators are predicted to be metallic. |
Hermann MauguinP6m2 [187] |
HallP 6 2 |
Point Group6m2 |
Crystal Systemhexagonal |
Topological ClassificationSM*
|
SubclassificationES†
|
Crossing TypeLine
|
Calculated powder diffraction pattern; note that peak spacings may be affected due to inaccuracies in calculated cell volume, which is typically overestimated on average by 3% (+/- 6%)
Select an element to display a spectrum averaged over all sites of that element in the structure.
Apply Gaussian smoothing:
Download spectra for every symmetrically equivalent absorption site in the structure.
Download FEFF Input parameters.
substrate material | substrate orientation | film orientation | MCIA† [Å2] |
---|---|---|---|
LaAlO3 (mp-2920) | <0 0 1> | <0 0 1> | 174.3 |
LaAlO3 (mp-2920) | <1 0 1> | <0 0 1> | 216.1 |
AlN (mp-661) | <1 0 0> | <1 1 0> | 106.1 |
AlN (mp-661) | <1 0 1> | <0 0 1> | 90.6 |
AlN (mp-661) | <0 0 1> | <0 0 1> | 62.7 |
AlN (mp-661) | <1 1 0> | <1 1 0> | 106.1 |
AlN (mp-661) | <1 1 1> | <1 1 0> | 176.8 |
CeO2 (mp-20194) | <1 1 0> | <1 0 0> | 306.3 |
CeO2 (mp-20194) | <1 0 0> | <1 0 1> | 151.0 |
CeO2 (mp-20194) | <1 1 1> | <0 0 1> | 216.1 |
GaAs (mp-2534) | <1 0 0> | <1 0 0> | 163.4 |
GaAs (mp-2534) | <1 1 0> | <0 0 1> | 139.4 |
GaAs (mp-2534) | <1 1 1> | <0 0 1> | 174.3 |
GaN (mp-804) | <0 0 1> | <0 0 1> | 27.9 |
BaF2 (mp-1029) | <1 0 0> | <1 0 1> | 237.4 |
BaF2 (mp-1029) | <1 1 1> | <0 0 1> | 195.2 |
SiO2 (mp-6930) | <0 0 1> | <0 0 1> | 20.9 |
SiO2 (mp-6930) | <1 0 0> | <0 0 1> | 27.9 |
GaN (mp-804) | <1 0 0> | <1 0 1> | 237.4 |
GaN (mp-804) | <1 0 1> | <0 0 1> | 76.7 |
KCl (mp-23193) | <1 0 0> | <1 0 1> | 237.4 |
KCl (mp-23193) | <1 1 1> | <0 0 1> | 216.1 |
GaN (mp-804) | <1 1 0> | <1 0 0> | 204.2 |
GaN (mp-804) | <1 1 1> | <1 1 0> | 176.8 |
SiO2 (mp-6930) | <1 0 1> | <0 0 1> | 34.9 |
SiO2 (mp-6930) | <1 1 0> | <1 0 0> | 183.8 |
SiO2 (mp-6930) | <1 1 1> | <0 0 1> | 104.6 |
KCl (mp-23193) | <1 1 0> | <1 0 1> | 172.6 |
DyScO3 (mp-31120) | <1 1 1> | <1 0 1> | 280.5 |
KTaO3 (mp-3614) | <1 1 0> | <1 1 0> | 70.7 |
CdS (mp-672) | <1 1 0> | <1 0 0> | 245.0 |
DyScO3 (mp-31120) | <0 0 1> | <0 0 1> | 209.2 |
DyScO3 (mp-31120) | <0 1 0> | <1 0 0> | 265.5 |
DyScO3 (mp-31120) | <1 0 0> | <0 0 1> | 139.4 |
DyScO3 (mp-31120) | <1 0 1> | <0 0 1> | 55.8 |
DyScO3 (mp-31120) | <1 1 0> | <1 1 1> | 180.2 |
InAs (mp-20305) | <1 0 0> | <0 0 1> | 188.2 |
InAs (mp-20305) | <1 1 0> | <1 0 1> | 258.9 |
InAs (mp-20305) | <1 1 1> | <0 0 1> | 62.7 |
ZnSe (mp-1190) | <1 0 0> | <1 0 0> | 163.4 |
ZnSe (mp-1190) | <1 1 0> | <0 0 1> | 139.4 |
ZnSe (mp-1190) | <1 1 1> | <0 0 1> | 174.3 |
KTaO3 (mp-3614) | <1 0 0> | <1 0 0> | 81.7 |
KTaO3 (mp-3614) | <1 1 1> | <0 0 1> | 27.9 |
CdS (mp-672) | <0 0 1> | <0 0 1> | 48.8 |
CdS (mp-672) | <1 0 0> | <1 0 0> | 204.2 |
CdS (mp-672) | <1 0 1> | <0 0 1> | 230.1 |
CdS (mp-672) | <1 1 1> | <1 0 0> | 102.1 |
LiF (mp-1138) | <1 0 0> | <1 0 0> | 81.7 |
LiF (mp-1138) | <1 1 0> | <1 1 0> | 70.7 |
Stiffness Tensor Cij (GPa) |
|||||
---|---|---|---|---|---|
611 | 171 | 247 | 0 | 0 | 0 |
171 | 611 | 247 | 0 | 0 | 0 |
247 | 247 | 727 | 0 | 0 | 0 |
0 | 0 | 0 | 174 | 0 | 0 |
0 | 0 | 0 | 0 | 174 | 0 |
0 | 0 | 0 | 0 | 0 | 220 |
Compliance Tensor Sij (10-12Pa-1) |
|||||
---|---|---|---|---|---|
2 | -0.3 | -0.6 | 0 | 0 | 0 |
-0.3 | 2 | -0.6 | 0 | 0 | 0 |
-0.6 | -0.6 | 1.8 | 0 | 0 | 0 |
0 | 0 | 0 | 5.7 | 0 | 0 |
0 | 0 | 0 | 0 | 5.7 | 0 |
0 | 0 | 0 | 0 | 0 | 4.6 |
Shear Modulus GV199 GPa |
Bulk Modulus KV364 GPa |
Shear Modulus GR196 GPa |
Bulk Modulus KR358 GPa |
Shear Modulus GVRH198 GPa |
Bulk Modulus KVRH361 GPa |
Elastic Anisotropy0.09 |
Poisson's Ratio0.27 |
material | dissimilarity | Ehull | # of elements |
---|---|---|---|
KNbSe2 (mp-7940) | 0.7339 | 0.029 | 3 |
LiNb2O (mp-1025455) | 0.4889 | 0.686 | 3 |
NbInSe2 (mp-1018116) | 0.2099 | 0.004 | 3 |
InMoS2 (mp-1087488) | 0.5002 | 0.091 | 3 |
NbInS2 (mp-20621) | 0.2928 | 0.016 | 3 |
SrMg (mp-1094327) | 0.5344 | 0.205 | 2 |
Tc3N (mp-1017987) | 0.0627 | 0.000 | 2 |
SrMg2 (mp-1094282) | 0.3972 | 0.275 | 2 |
SrMg2 (mp-1094323) | 0.5385 | 0.272 | 2 |
Sr2Mg (mp-1094355) | 0.4581 | 0.152 | 2 |
Run TypeGGA |
Energy Cutoff520 eV |
# of K-pointsNone |
U Values-- |
PseudopotentialsVASP PAW: Re_pv N |
Final Energy/Atom-11.4491 eV |
Corrected Energy-45.7964 eV
-45.7964 eV = -45.7964 eV (uncorrected energy)
|
Displaying lattice parameters for primitive cell; note that calculated cell volumes are typically overestimated on average by 3% (+/- 6%). Note the primitive cell may appear less symmetric than the conventional cell representation (see "Structure Type" selector below the 3d structure)